Claims Analysis
Total Claims: 20
Claim 1
Independent Claim
126 words
A method for press-bonding a laminated assembly of a sheet material and a plastic film, which comprises providing on at least the peripheral portion of the sheet material and/or the plastic film a printer layer capable of adhering the sheet material and the plastic film at room temperature, stacking the sheet material and the plastic film to form a laminated assembly, evacuating a first vacuum compartment defined by the sheet material and the plastic film to a vacuumed condition and at the same time, evacuating a second vacuum compartment enclosing at least the plastic film side of the first compartment, to a vacuumed condition, and then releasing the second vacuum compartment from the vacuumed condition and thereby to press-bond the plastic film to the sheet material.
Claim 2
Independent Claim
126 words
A method for press-bonding a laminated assembly of a sheet material and a plastic film, which comprises providing on at least the peripheral portion of the sheet material and/or the plastic film a printer layer capable of adhering the sheet material and the plastic film at room temperature, stacking the sheet material and the plastic film to form a laminated assembly, evacuating a first vacuum compartment defined by the sheet material and the plastic film to a vacuumed condition and at the same time, evacuating a second vacuum compartment enclosing at least the plastic film side of the first compartment, to a vacuumed condition, and then releasing the second vacuum compartment from the vacuumed condition and thereby to press-bond the plastic film to the sheet material.
Claim 3
Dependent Claim
14 words
The method according to Claim 1, wherein the plastic film has a self-healing property.
Claim 4
Dependent Claim
14 words
The method according to Claim 1, wherein the sheet material is a glass sheet.
Claim 5
Dependent Claim
29 words
The method according to Claim 1, wherein the plastic film has embosses with a depth of from 0.1 to 5 µ m on the side facing the sheet material.
Claim 6
Dependent Claim
26 words
The method according to Claim 1, wherein the primer layer is a primer capable of strengthening the adhesive force along the periphery of the plastic film.
Claim 7
Independent Claim
137 words
A method for press-bonding a laminated assembly of a sheet material and a plastic film, which comprises providing on at least the peripheral portion of the sheet material and/or the plastic film a primer layer capable of adhering the sheet material and the plastic film at room temperature, stacking the sheet material and the plastic film to form a laminated assembly, placing the laminated assembly in a first vacuum compartment defined by a cover film, evacuating the first vacuum compartment to a vacuumed condition and at the same time, evacuating a second vacuum compartment enclosing the first vacuum compartment, to a vacuumed condition, and then releasing the second vacuum compartment from the vacuumed condition and thereby to press the cover film to the laminated assembly surface so that the plastic film is press-bonded to the sheet material.
Claim 8
Independent Claim
137 words
A method for press-bonding a laminated assembly of a sheet material and a plastic film, which comprises providing on at least the peripheral portion of the sheet material and/or the plastic film a primer layer capable of adhering the sheet material and the plastic film at room temperature, stacking the sheet material and the plastic film to form a laminated assembly, placing the laminated assembly in a first vacuum compartment defined by a cover film, evacuating the first vacuum compartment to a vacuumed condition and at the same time, evacuating a second vacuum compartment enclosing the first vacuum compartment, to a vacuumed condition, and then releasing the second vacuum compartment from the vacuumed condition and thereby to press the cover film to the laminated assembly surface so that the plastic film is press-bonded to the sheet material.
Claim 9
Dependent Claim
14 words
The method according to Claim 6, wherein the plastic film has a self-healing property.
Claim 10
Dependent Claim
14 words
The method according to Claim 6, wherein the sheet material is a glass sheet.
Claim 11
Dependent Claim
29 words
The method according to Claim 6, wherein the plastic film has embosses with a depth of from 0.1 to 5 µ m on the side facing the sheet material.
Claim 12
Dependent Claim
26 words
The method according to Claim 6, wherein the primer layer is a primer capable of strengthening the adhesive force along the periphery of the plastic film.
Claim 13
Independent Claim
121 words
A method for press-bonding a laminated assembly of a sheet material and a plastic film, which comprises stacking a sheet material and a plastic film to form a laminated assembly, placing the laminated assembly in a first vacuum compartment defined by a cover film having a roughened surface on the side facing the plastic film of the laminated assembly, evacuating the first vacuum compartment to a vacuumed condition and at the same time, evacuating a second vacuum compartment enclosing the first vacuum compartment, to a vacuumed condition, and then releasing the second vacuum compartment from the vacuumed condition and thereby to press the cover film to the laminated assembly surface so that the plastic film is press-bonded to the sheet material.
Claim 14
Independent Claim
121 words
A method for press-bonding a laminated assembly of a sheet material and a plastic film, which comprises stacking a sheet material and a plastic film to form a laminated assembly, placing the laminated assembly in a first vacuum compartment defined by a cover film having a roughened surface on the side facing the plastic film of the laminated assembly, evacuating the first vacuum compartment to a vacuumed condition and at the same time, evacuating a second vacuum compartment enclosing the first vacuum compartment, to a vacuumed condition, and then releasing the second vacuum compartment from the vacuumed condition and thereby to press the cover film to the laminated assembly surface so that the plastic film is press-bonded to the sheet material.
Claim 15
Dependent Claim
14 words
The method according to Claim 11, wherein the plastic film has a self-healing property.
Claim 16
Dependent Claim
29 words
The method according to Claim 11, wherein the roughened surface of the cover film has a roughness of from 0.5 to 70 µm, preferably from 2 to 40 µm.
Claim 17
Dependent Claim
40 words
The method according to Claim 11, wherein a primer layer capable of adhering the plastic film and the sheet material at room temperature is present between the plastic film and the sheet material at least along the peripheral portion thereof.
Claim 18
Dependent Claim
14 words
The method according to Claim 11, wherein the sheet material is a glass sheet.
Claim 19
Dependent Claim
28 words
The method according to Claim 11, wherein the plastic film has embosses with a depth of from 0.1 to 5 µm on the side facing the sheet material.
Claim 20
Dependent Claim
16 words
A laminated product produced by the method claimed in any one of claims 1 to 16.