← Back to Patent Explorer
US2952553A Expired / Lapsed US ⏱️ 0.0 years remaining

Method for forming a metal casting mold

Assignee: Diamond Shamrock Corp
•
Filing: 1959-01-12
•
Granted: 1960-09-13
•
Expires: 1979-01-12
📄 Original PDF 🌐 Google Patents

Abstract

No abstract record available.

Inventors

  • 👤 Frank P Ilenda
  • 👤 Jr Cletus E Peeler

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-04 03:22
CPC Classifications
B; B22; B22C; B22C1/00; B22C1/16; B22C1/162

Claims Analysis

Total Claims: 2
Claim 1
Independent Claim 124 words
THE METHOD OF FORMING A CASTING MOLD WHICH COMPRISES PLACING IN CONTACT WITH A CASTING-DEFINING SURFACE A COMPOSITION COMPRISING AN INTIMATE MIXTURE OF A MAJOR PORTION OF ABOUT 90 TO 97% BY WEIGHT OF A FINELYDIVIDED REFRACTORY MATERIAL AND A MINOR PROPORTION OF ABOUT 3 TO 10% BY WEIGHT OF A LIQUID BINDER COMPOSITION COMPRISING IN COMBINATION ABOUT 80 TO 99% BY WEIGHT OF AN AQUEOUS ALKALI METAL SILICATE HAVING A SOLIDS CONTENT OF ABOUT 30 TO 50% AND ABOUT 1 TO 20% BY WEIGHT OF A FINELY-DIVIDED WATER SOLUBLE, SOLID ALKALI METAL SILICATE HAVING AN ALKALI METAL OXIDE:SILICA RATIO WITHIN THE RANGE OF 2.0:1.0 TO 1.0:3.3, INCLUSIVE, AND SUBJECTING THE MIXTURE TO CONTACT WITH A GASEOUS MATERIAL CAPABLE OF RIGIDIFYING THE MOLD-FORMING MIXTURE.
Claim 2
Independent Claim 124 words
THE METHOD OF FORMING A CASTING MOLD WHICH COMPRISES PLACING IN CONTACT WITH A CASTING-DEFINING SURFACE A COMPOSITION COMPRISING AN INTIMATE MIXTURE OF A MAJOR PORTION OF ABOUT 90 TO 97% BY WEIGHT OF A FINELYDIVIDED REFRACTORY MATERIAL AND A MINOR PROPORTION OF ABOUT 3 TO 10% BY WEIGHT OF A LIQUID BINDER COMPOSITION COMPRISING IN COMBINATION ABOUT 80 TO 99% BY WEIGHT OF AN AQUEOUS ALKALI METAL SILICATE HAVING A SOLIDS CONTENT OF ABOUT 30 TO 50% AND ABOUT 1 TO 20% BY WEIGHT OF A FINELY-DIVIDED WATER SOLUBLE, SOLID ALKALI METAL SILICATE HAVING AN ALKALI METAL OXIDE:SILICA RATIO WITHIN THE RANGE OF 2.0:1.0 TO 1.0:3.3, INCLUSIVE, AND SUBJECTING THE MIXTURE TO CONTACT WITH A GASEOUS MATERIAL CAPABLE OF RIGIDIFYING THE MOLD-FORMING MIXTURE.

References Cited (Backward Citations)

FR976384A Cited
GB710099A Cited
GB745402A Cited
US2861893A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1963-09-13 1964-03-14 1964-09-13 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1967-09-13 1968-03-14 1968-09-13 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1971-09-13 1972-03-14 1972-09-13 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag