US3251708A
Expired / Lapsed
US
⏱️ 0.0 years remaining
Coating with a polyamide-epoxy resin
Assignee: Inland Steel Co
•
Filing: 1962-06-01
•
Granted: 1966-05-17
•
Expires: 1982-06-01
Abstract
No abstract record available.
Inventors
- 👤 Benjamin A Schmetterer
- 👤 Fred E Wills
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-11-06 18:28
CPC Classifications
B; B05; B05D; B05D7/00; B05D7/14; B05D7/16; Y; Y10; Y10T; Y10T428/00; Y10T428/31504; Y10T428/31511; Y10T428/31529
Claims Analysis
Total Claims: 2
Claim 1
Independent Claim
202 words
A PROCESS OF PROVIDING A STRIP OF METAL WITH A THIN CONTINUOUS COATING OF AN ORGANIC RESIN WHICH COMPRISES; CONTINUOUSLY APPLYING TO AT LEAST ONE SIDE OF A METAL STRIP MOVING IN A CONTINUOUS PROCESSING LINE AT A SUBSTANTIALLY CONSTANT SPEED A UNIFORM FLUID FILM OF A SOLUTION OF A POLYAMIDE RESINOUS MATERIAL CONTAINING TERMINAL AMINO GROUPS AND AN EPOXY RESINOUS MATERIAL CONTAINING TERMINAL EPOXY GROUPS DISSOLVED IN THE HALOGENATED HYDROCARBON SOLVENT HAVING A MAJOR PROPORTION THEREOF COMPOSED OF METHYLENE CHLORIDE AND SAID RESINOUS MATERIALS BEING PRESENT IN A PROPORTION OF ABOUT ONE TO FOUR PARTS BY WEIGHT OF SAID EPOXY RESINOUS MATERIAL TO ABOUT ONE PART BY WEIGHT OF SAID POLYAMIDE RESINOUS MATERIAL, SAID SOLUTION HAVING DISSOLVED THEREIN AS A BUFFERING AGENT AN AMINE HAVING A BOILING POINT HIGHER THAN SAID SOLVENT, EXPOSING SAID FLUID FILM ON SAID STRIP TO A TEMPERATURE BETWEEN ABOUT 1500*F. AND 1700*F. FOR A PERIOD ABOUT 3 TO 5 SECONDS TO EFFECT SUBSTANTIALLY IMMEDIATE AND COMPLETE CURING OF SAID FILM, AND RAPIDLY COOLING SAID FILM AND SAID STRIP TO ABOUT ROOM TEMPERATURE BY CONTACTING WITH A COOLING FLUID; WHEREBY A FULLY CURED POLYAMIDE-EPOXY RESIN COATING IS CONTINUOUSLY AND RAPIDLY FORMED IN-LINE ON SAID STRIP OF METAL.
Claim 2
Dependent Claim
202 words
A PROCESS OF PROVIDING A STRIP OF METAL WITH A THIN CONTINUOUS COATING OF AN ORGANIC RESIN WHICH COMPRISES; CONTINUOUSLY APPLYING TO AT LEAST ONE SIDE OF A METAL STRIP MOVING IN A CONTINUOUS PROCESSING LINE AT A SUBSTANTIALLY CONSTANT SPEED A UNIFORM FLUID FILM OF A SOLUTION OF A POLYAMIDE RESINOUS MATERIAL CONTAINING TERMINAL AMINO GROUPS AND AN EPOXY RESINOUS MATERIAL CONTAINING TERMINAL EPOXY GROUPS DISSOLVED IN THE HALOGENATED HYDROCARBON SOLVENT HAVING A MAJOR PROPORTION THEREOF COMPOSED OF METHYLENE CHLORIDE AND SAID RESINOUS MATERIALS BEING PRESENT IN A PROPORTION OF ABOUT ONE TO FOUR PARTS BY WEIGHT OF SAID EPOXY RESINOUS MATERIAL TO ABOUT ONE PART BY WEIGHT OF SAID POLYAMIDE RESINOUS MATERIAL, SAID SOLUTION HAVING DISSOLVED THEREIN AS A BUFFERING AGENT AN AMINE HAVING A BOILING POINT HIGHER THAN SAID SOLVENT, EXPOSING SAID FLUID FILM ON SAID STRIP TO A TEMPERATURE BETWEEN ABOUT 1500*F. AND 1700*F. FOR A PERIOD ABOUT 3 TO 5 SECONDS TO EFFECT SUBSTANTIALLY IMMEDIATE AND COMPLETE CURING OF SAID FILM, AND RAPIDLY COOLING SAID FILM AND SAID STRIP TO ABOUT ROOM TEMPERATURE BY CONTACTING WITH A COOLING FLUID; WHEREBY A FULLY CURED POLYAMIDE-EPOXY RESIN COATING IS CONTINUOUSLY AND RAPIDLY FORMED IN-LINE ON SAID STRIP OF METAL.
References Cited (Backward Citations)
US2538091A
Cited
US2736719A
Cited
US2852477A
Cited
US2881091A
Cited
US2967161A
Cited
US2948639A
Cited
US3006877A
Cited
US2940874A
Cited
US3039986A
Cited
US3154605A
Cited
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1969-05-16 | 1969-11-15 | 1970-05-17 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 1973-05-16 | 1973-11-15 | 1974-05-17 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 1977-05-16 | 1977-11-15 | 1978-05-17 | $7700.00 | Window Closed / Lapsed |