Vacuum circuit breaker contacts consisting essentially of a copper matrix and solid solution particles of copper-tellurium and copper-selenium
Assignee: Toshiba Corp
•
Filing: 1969-07-24
•
Granted: 1971-07-27
•
Expires: 1989-07-24
Abstract
Abstract A vacuum circuit breaker containing a pair of contact members relatively movable for contact or separation in which at least one of the contact members is made of an alloy consisting of copper matrix and solid solution particles of a Cu2Te - Cu2Se system dispersed in said copper matrix, the content of Se ranges between 0.1 and 5.0 percent, and that of Te ranges from 0.1 to 25.9 percent, their total content being 2.5 to 26 percent.
Inventors
- 👤 Isao Okutomi
- 👤 Kazuo Suzuki
- 👤 Hikohiro Mizutani
- 👤 Kenichiro Ando
- 👤 Chiaki Hiruta
- 👤 Akira Nabae
- 👤 Tadahito Tsutsumi
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-10-31 21:04
CPC Classifications
H; H01; H01H; H01H1/00; H01H1/02; H01H1/0203
Claims Analysis
Total Claims: 3
Claim 1
Independent Claim
101 words
A vacuum circuit breaker having a pair of contact members relatively movable for contact and separation, where in at least one of the paired contact members is made of an alloy consisting essentially of a copper matrix and solid solution particles of a Cu2Te-Cu2Se system dispersed in said copper matrix, the content of selenium ranges between 0.1 and 5 percent on the basis of the alloy and that of tellurium ranges from 0.1 to 25.9 percent on the basis of the alloy, the total content of the selenium and tellurium being 2.5 to 26 percent on the basis of the alloy.
Claim 2
Dependent Claim
101 words
A vacuum circuit breaker having a pair of contact members relatively movable for contact and separation, where in at least one of the paired contact members is made of an alloy consisting essentially of a copper matrix and solid solution particles of a Cu2Te-Cu2Se system dispersed in said copper matrix, the content of selenium ranges between 0.1 and 5 percent on the basis of the alloy and that of tellurium ranges from 0.1 to 25.9 percent on the basis of the alloy, the total content of the selenium and tellurium being 2.5 to 26 percent on the basis of the alloy.
Claim 3
Dependent Claim
13 words
The vacuum circuit breaker according to claim l wherein said alloy contains silver.
References Cited (Backward Citations)
No citation records indexed.
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1974-07-26 | 1975-01-25 | 1975-07-27 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 1978-07-26 | 1979-01-25 | 1979-07-27 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 1982-07-26 | 1983-01-25 | 1983-07-27 | $7700.00 | Window Closed / Lapsed |