Abstract

Abstract An alkaline galvanic cell having a positive electrode containing a heavy metal oxide in contact with a metallic housing and a negative electrode containing an amalgamated zinc in contact with a cover, said cover being formed from an elastically resilient laminate having an exterior side consisting of a layer of nickel or a layer of a rust-proof nickel alloy and having a thickness of 0.05 to 0.5 mm. and an interior side consisting of a layer of copper, zinc, tin, lead or their alloys and having a thickness of 0.05 to 0.5 mm. at least one layer of said laminate consisting of a spring alloy.

Inventors

  • 👤 Paul Ruetschi

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-04 23:11
CPC Classifications
H; H01; H01M; H01M50/00; H01M50/10; H01M50/147; H01M50/166; H01M50/171; H01M50/167; Y; Y02; Y02E; Y02E60/00; Y02E60/10

Claims Analysis

Total Claims: 6
Claim 1
Independent Claim 35 words
An alkaline galvanic cell according to claim 1, which is characterized in that the exterior layer of the cover has a hardness of more than 250 Vickers degrees of hardness and is made elastically resilient.
Claim 2
Dependent Claim 35 words
An alkaline galvanic cell according to claim 1, which is characterized in that the exterior layer of the cover has a greater hardness than the metallic housing that is in contact with the positive electrode.
Claim 3
Dependent Claim 52 words
An alkaline galvanic cell according to claim 1, which is characterized in that thE interior layer of the cover consists of a spring bronze containing 5 - 15 percent tin and 85 - 95 percent copper and in that said layer has a hardness of more than 100 Vickers degrees of hardness.
Claim 4
Dependent Claim 20 words
An alkaline galvanic cell according to claim 4 wherein said spring bronze contains 8 percent tin and 92 percent copper.
Claim 5
Dependent Claim 51 words
An alkaline galvanic cell according to claim 1, which is characterized in that the interior layer of the cover consists of spring brass containing 30 - 40 percent zinc and 60 - 70 percent copper and in that said layer has a hardness of more than 100 Vickers degrees of hardness.
Claim 6
Dependent Claim 20 words
An alkaline galvanic cell according to claim 6 wherein said spring brass contains 37 percent zinc and 63 percent copper.

References Cited (Backward Citations)

US2712565A Cited
US2951891A Cited
US2985703A Cited
US3096217A Cited
US3418172A Cited
US3457117A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1975-04-18 1975-10-18 1976-04-18 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1979-04-18 1979-10-18 1980-04-18 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1983-04-18 1983-10-18 1984-04-18 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag