Abstract
Abstract Polyol compositions are disclosed which comprise a mixture of alkoxylated dihalobutenediol and a second polyhydroxy compound wherein the hydroxyl number of said polyol composition is from about 200 to 700. A process for preparing the polyol composition and flame-retardant polyurethane foams prepared from said polyol compositions are also disclosed.
Inventors
- 👤 J Feltzin
- 👤 E Kuehn
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-10-30 04:07
CPC Classifications
C; C08; C08G; C08G65/00; C08G65/34; C08G18/00; C08G18/06; C08G18/28; C08G18/67; C08G18/6795
Claims Analysis
Total Claims: 4
Claim 1
Independent Claim
53 words
A polyol composition according to claim 1 wherein the hydroxyl number of said mixture is from 300 to 600, the concentration of 2,3-dibromo-2-butene-1,4-diol moiety in the mixture is from about 15 to about 50 weight percent and the alkoxylated dihalobutenediol contains an average of from 1 to 4 oxyalkylene groups per dihalobutenediol moiety.
Claim 2
Dependent Claim
15 words
A polyol composition according to claim 1 wherein the oxyalkylene group is oxypropylene or oxyethylene.
Claim 3
Dependent Claim
131 words
A process of preparing a polyol composition which comprises mixing an amine free polyhydroxy compound selected from the group consisting of polyhydroxy alkanes, alkoxylated polyhydroxy alkanes, sugars, alkoxylated sugars, hydroxyl terminated polyesters, and hydroxyl terminated aromatic polyethers and butynediol so that at least 3.5 weight percent of the resulting mixture is butynediol; adding halogen to said mixture in a molar ratio of from about 0.9 to 1.2 mols of halogen per mol of butynediol, at a temperature of less than about 100*C.; and reacting the resulting halogenated product with from 0.5 to 2 mols of alkylene oxide per hydroxyl equivalent of halogenated product; wherein said polyhydroxy compound and the amount of alkylene oxide are so chosen that the final hydroxyl number of the resultant polyol blend is from 200 to 700.
Claim 4
Dependent Claim
56 words
A process for preparing a polyol composition in accordance with claim 4 wherein the weight percent of butynediol is chosen so that the final weight percent of dihalobutynediol moiety in the polyol blend is from 15 to 40 weight percent of the composItion, wherein the hydroxyl number of the polyol composition is from 300 to 600.
References Cited (Backward Citations)
GB1037392A
Cited
US3379778A
Cited
GB1132034A
Cited
US3409679A
Cited
US3507933A
Cited
US3391200A
Cited
US3723392A
Cited
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1976-10-08 | 1977-04-09 | 1977-10-09 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 1980-10-08 | 1981-04-09 | 1981-10-09 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 1984-10-08 | 1985-04-09 | 1985-10-09 | $7700.00 | Window Closed / Lapsed |