Abstract A process for the manufacture of paper pulp from waste paper in which the waste paper is comminuted in water in a pulper, pre-cleaned for removal of coarse foreign contaminants, dewatered, kneaded at high concentration, diluted, after-cleaned for removal of finer or coherent soft foreign contaminants and adjusted to a concentration suitable for paper-making, the water respectively used for dilution and obtained during dewatering being circulated in two separate circuits upstream and downstream respectively of the kneading apparatus.
Inventors
- 👤 Erik Folke Eriksson
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-11-07 14:04
CPC Classifications
D; D21; D21B; D21B1/00; D21B1/04; D21B1/12; D21B1/30; D21B1/32; Y; Y02; Y02W; Y02W30/00; Y02W30/50; Y02W30/64
Claims Analysis
Total Claims: 5
Claim 1
Independent Claim
240 words
In a process for the manufacture of paper pulp from waste paper material, of the type wherein the waste paper material is diluted and comminuted in water in a pulper, precleaned for removal of coarse foreign contaminants, de-watered, kneaded in a kneading apparatus at high concentration, again diluted, after-cleaned for removal of finer or coherent soft foreign contaminants and dewatered to a concentration suitable for introduction into a paper-making machine in that order, characterized in that water respectively used for dilution and obtained during de-watering is circulated in two separate circuits upstream and downstream respectively of the kneading apparatus, that the dwelling time of the waste paper in the pulper is shorter than the time necessary for complete impregnation of the paper with water and just sufficient for obtaining pumpability, that the dewatering before kneading is performd so that the paper is completely impregnated, that the kneading apparatus comprises screw or vane-shaped working means operating in a casing and discharging said material at a final temperature of about 70° to 90°C, and that the concentration of the material discharged from the kneading apparatus is reduced to pumpability in a mixer in which the material is permitted to dwell a time sufficient to cause components of asphalt and bitumen type contained in the waste paper and dispersed in said material to agglomerate to lumps of such a size that they can be screened-off during after-cleaning, and screening off said agglomerated lumps.
Claim 2
Dependent Claim
240 words
In a process for the manufacture of paper pulp from waste paper material, of the type wherein the waste paper material is diluted and comminuted in water in a pulper, precleaned for removal of coarse foreign contaminants, de-watered, kneaded in a kneading apparatus at high concentration, again diluted, after-cleaned for removal of finer or coherent soft foreign contaminants and dewatered to a concentration suitable for introduction into a paper-making machine in that order, characterized in that water respectively used for dilution and obtained during de-watering is circulated in two separate circuits upstream and downstream respectively of the kneading apparatus, that the dwelling time of the waste paper in the pulper is shorter than the time necessary for complete impregnation of the paper with water and just sufficient for obtaining pumpability, that the dewatering before kneading is performd so that the paper is completely impregnated, that the kneading apparatus comprises screw or vane-shaped working means operating in a casing and discharging said material at a final temperature of about 70° to 90°C, and that the concentration of the material discharged from the kneading apparatus is reduced to pumpability in a mixer in which the material is permitted to dwell a time sufficient to cause components of asphalt and bitumen type contained in the waste paper and dispersed in said material to agglomerate to lumps of such a size that they can be screened-off during after-cleaning, and screening off said agglomerated lumps.
Claim 3
Dependent Claim
39 words
The process of claim 1 wherein said step of de-watering before kneading comprises further supporting said material with a screen while simultaneously exposing it to a counter-pressure acting against the feed pressure to obtain a determined degree of de-watering.
Claim 4
Dependent Claim
248 words
In a process for the manufacture of paper pulp from waste paper material having asphalt or bitumen type components of the type comprising the steps of: a. comminuting the waste paper in water, b. pre-cleaning the comminuted material to remove contaminants, c. de-watering the pre-cleaned material, d. kneading the de-watered material at high concentration, and heating said dewatered material to a temperature of from 70°C to 90°C wherein said asphalt and bitumen type components become dispersed, e. diluting the de-watered kneaded material while mixing said kneaded material for a time sufficient to cause said asphalt and bitumen type components dispersed in said kneaded material to agglomerate into lumps, f. after cleaning said kneaded diluted material by removing finer soft contaminants from said diluted kneaded material and by screening off said agglomerated lumps, and g. adjusting the concentration of the diluted material to be suitable for use in a paper-making machine, in that order; the improvement wherein said step of comminuting comprises comminuting said waste paper partly with water removed from said pre-cleaned material in said de-watering step for a time less than that required for complete impregnation of the waste paper with water and a time just sufficient that the comminuted waste paper is pumpable, said step of de-watering comprises completely impregnating said pre-cleaned material with water, and said step of adjusting the concentration of said diluted material comprises concentrating the diluted material and further comprising employing water obtained in said step of concentrating in said diluting step.
Claim 5
Dependent Claim
248 words
In a process for the manufacture of paper pulp from waste paper material having asphalt or bitumen type components of the type comprising the steps of: a. comminuting the waste paper in water, b. pre-cleaning the comminuted material to remove contaminants, c. de-watering the pre-cleaned material, d. kneading the de-watered material at high concentration, and heating said dewatered material to a temperature of from 70°C to 90°C wherein said asphalt and bitumen type components become dispersed, e. diluting the de-watered kneaded material while mixing said kneaded material for a time sufficient to cause said asphalt and bitumen type components dispersed in said kneaded material to agglomerate into lumps, f. after cleaning said kneaded diluted material by removing finer soft contaminants from said diluted kneaded material and by screening off said agglomerated lumps, and g. adjusting the concentration of the diluted material to be suitable for use in a paper-making machine, in that order; the improvement wherein said step of comminuting comprises comminuting said waste paper partly with water removed from said pre-cleaned material in said de-watering step for a time less than that required for complete impregnation of the waste paper with water and a time just sufficient that the comminuted waste paper is pumpable, said step of de-watering comprises completely impregnating said pre-cleaned material with water, and said step of adjusting the concentration of said diluted material comprises concentrating the diluted material and further comprising employing water obtained in said step of concentrating in said diluting step.
References Cited (Backward Citations)
US2062442A
Cited
US3057769A
Cited
US2887430A
Cited
SE314288B
Cited
US3549092A
Cited
US3849246A
Cited
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1979-05-18 | 1979-11-17 | 1980-05-18 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 1983-05-18 | 1983-11-17 | 1984-05-18 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 1987-05-18 | 1987-11-17 | 1988-05-18 | $7700.00 | Window Closed / Lapsed |