Abstract

Abstract A method for controlling the viscosity of dispersed clay slurries is disclosed. In accordance with the invention the problem associated with shipping or storing clay slurries in tank cars or tanks, that is, significant increases in the viscosity of the slurry which often results in the formation of a gelled mass, is overcome by the addition of the pentasodium salt of diethylenetriamine pentacetic acid (DTPA). The addition of the diethylenetriamine pentacetic acid salt serves to control the viscosity of the clay slurry in a manner such that it remains at a substantially uniform and low level even when the slurry is shipped or stored over extended periods of time. The diethylenetriamine pentacetic acid pentasodium salt is added to the slurry in relatively small quantities, i.e., up to 5.0 pounds/ton clay and unexpectedly does not affect the properties or characteristics of the clay pigment or product.

Inventors

  • 👤 William F. Abercrombie, Jr.

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-25 18:45
CPC Classifications
C; C09; C09D; C09D17/00; C09D17/004; C04; C04B; C04B33/00; C04B33/02; C04B33/13; C04B33/18; C09C; C09C1/00; C09C1/40; C09C1/42; C01; C01P; C01P2004/00; C01P2004/30; C01P2004/32; C01P2004/51; C01P2004/60; C01P2004/61; C01P2006/00; C01P2006/22

Claims Analysis

Total Claims: 8
Claim 1
Independent Claim 99 words
A method for controlling and maintaining the viscosity of aqueous slurries of finely divided daolin pigments, comprising the steps of refining kaolin clay particulates in an aqueous medium to reduce partical size and improve brightness and contacting the refined kaolin clay particulates in said aqueous medium, having a clay solids content in the range of from about 60 to 72% by weight, with the pentasodium salt of diethylenetriamine pentacetic acid in an amount in the range of from about 0.1 to 5.0 pounds acid per ton of said clay particulates, based on the dry weight of said clay particulates.
Claim 2
Independent Claim 99 words
A method for controlling and maintaining the viscosity of aqueous slurries of finely divided daolin pigments, comprising the steps of refining kaolin clay particulates in an aqueous medium to reduce partical size and improve brightness and contacting the refined kaolin clay particulates in said aqueous medium, having a clay solids content in the range of from about 60 to 72% by weight, with the pentasodium salt of diethylenetriamine pentacetic acid in an amount in the range of from about 0.1 to 5.0 pounds acid per ton of said clay particulates, based on the dry weight of said clay particulates.
Claim 3
Independent Claim 107 words
A method for controlling and maintaining the viscosity of an aqueous slurry of finely divided refined particulate kaolin clay pigments at a substantially uniform and low level during shipment and storage, said method consisting essentially of forming an aqueous slurry of finely divided refined particulate kaolin clay pigments having a clay solids content in the range of from about 60 to 72% by weight and then contacting said clay slurry with the pentasodium salt of diethylenetriamine pentacetic acid in an amount in the range of from about 0.1 to 5.0 pounds acid per ton of said clay pigments, based on the dry weight of said clay pigments.
Claim 4
Independent Claim 107 words
A method for controlling and maintaining the viscosity of an aqueous slurry of finely divided refined particulate kaolin clay pigments at a substantially uniform and low level during shipment and storage, said method consisting essentially of forming an aqueous slurry of finely divided refined particulate kaolin clay pigments having a clay solids content in the range of from about 60 to 72% by weight and then contacting said clay slurry with the pentasodium salt of diethylenetriamine pentacetic acid in an amount in the range of from about 0.1 to 5.0 pounds acid per ton of said clay pigments, based on the dry weight of said clay pigments.
Claim 5
Dependent Claim 46 words
The method in accordance with claim 2 wherein said diethylentriamine pentacetic salt is added to said slurry in an amount in the range of from about 0.5 to 3 pounds acid per ton of said clay pigments, based on the dry weight of said clay pigments.
Claim 6
Dependent Claim 36 words
The method of claim 2 wherein said clay pigments comprising finely divided, refined kaolin clay pigments having a particle size distribution such that 80% by weight is finer than 2 micron diameter particles, equivalent spherical diameter.
Claim 7
Dependent Claim 53 words
An aqueous slurry comprising from about 60 to 72% by weight of finely divided, refined kaolin clay pigments and, as a viscosity control agent, from about 0.1 to 5.0 pounds of the pentasodium salt of diethylenetriamine pentacetic acid per ton of said kaolin clay pigments, based on the dry weight of said pigments.
Claim 8
Dependent Claim 53 words
An aqueous slurry comprising from about 60 to 72% by weight of finely divided, refined kaolin clay pigments and, as a viscosity control agent, from about 0.1 to 5.0 pounds of the pentasodium salt of diethylenetriamine pentacetic acid per ton of said kaolin clay pigments, based on the dry weight of said pigments.

References Cited (Backward Citations)

US2982665A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1979-06-08 1979-12-08 1980-06-08 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1983-06-08 1983-12-08 1984-06-08 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1987-06-08 1987-12-08 1988-06-08 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag