← Back to Patent Explorer
US3992178A Expired / Lapsed US ⏱️ 0.0 years remaining

Flexible coated abrasive with graphite outer layer

Assignee: Fabrika Eka AB
•
Filing: 1974-04-09
•
Granted: 1976-11-16
•
Expires: 1994-04-09
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract A flexible abrasive article carries a layer of particles of electroconductive material on the outer surface of the abrasive side to reduce the buildup of electrostatic charge during use in sanding wood or grinding metal. Metallic and non-metallic electroconductive materials may be employed.

Inventors

  • 👤 Erik L. Markoo
  • 👤 Hans S. Ekblom
  • 👤 Torsten Wilhelm Sandell

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-31 12:58
CPC Classifications
B; B24; B24D; B24D11/00; B24D11/001; B24D11/005

Claims Analysis

Total Claims: 5
Claim 1
Independent Claim 94 words
In a flexible abrasive article, comprising a flexible backing, an adhesive layer on said backing, and abrasive grits embedded in said adhesive layer, the improvement comprising an outer layer coated over said adhesive layer and said grits, said outer layer comprising an adhesive containing graphite particles having a size from 0.1 to 100 microns, the amount of graphite being from 1 to 100 grams per square meter of said abrasive article and sufficient to provide said outer layer with an electrical resistance of less than 5 megohm as measured between points 1 cm. apart.
Claim 2
Dependent Claim 94 words
In a flexible abrasive article, comprising a flexible backing, an adhesive layer on said backing, and abrasive grits embedded in said adhesive layer, the improvement comprising an outer layer coated over said adhesive layer and said grits, said outer layer comprising an adhesive containing graphite particles having a size from 0.1 to 100 microns, the amount of graphite being from 1 to 100 grams per square meter of said abrasive article and sufficient to provide said outer layer with an electrical resistance of less than 5 megohm as measured between points 1 cm. apart.
Claim 3
Dependent Claim 19 words
The article according to claim 1, wherein said graphite is of a particle size of 1 to 10 microns.
Claim 4
Dependent Claim 17 words
The article according to claim 1, wherein said graphite is of 5 to 7 micron particle size.
Claim 5
Dependent Claim 18 words
The article according to claim 1, wherein said graphite is of 90% less than 1 micron particle size.

References Cited (Backward Citations)

US2050992A Cited
US2233175A Cited
US3168387A Cited
US3282665A Cited
US3163968A Cited
US3377264A Cited
GB1256520A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1979-11-16 1980-05-17 1980-11-16 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1983-11-16 1984-05-17 1984-11-16 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1987-11-16 1988-05-17 1988-11-16 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.