US4080561A
Expired / Lapsed
US
⏱️ 0.0 years remaining
Method and apparatus for testing dielectric adequacy and for indicating physical defects in a nonconducting material
Assignee: Westinghouse Electric Corp
•
Filing: 1976-09-21
•
Granted: 1978-03-21
•
Expires: 1996-09-21
Abstract
Abstract An elastomer impregnated with carbon is utilized in conjunction with a conductor to test the dielectric adequacy of a nonconductor and to indicate physical defects, such as cracks, pinholes or a thickness below a predetermined minimum, by depositing traces of carbon on the non-conductor in the area of the defect or the area where the thickness is below the predetermined minimum.
Inventors
- 👤 Robert W. Thompson
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-11-08 13:42
CPC Classifications
G; G01; G01R; G01R27/00; G01R27/02; G01R27/025; G01N; G01N27/00; G01N27/02; G01N27/04; G01N27/20; G01N27/205; G01R31/00; G01R31/12; G01R31/1227; G01R31/1263
Claims Analysis
Total Claims: 2
Claim 1
Independent Claim
254 words
A method for testing a non-conducting container for deterioration due to exposure to sunlight and other atmospheric conditions, said method comprising the steps of: placing a first conductor which generally conforms to the area to be tested on one side of the container; placing another conductor which generally conforms to the area to be tested on the side opposite the side having the first conductor; applying a predetermined DC voltage across the conductor and recording the current flowing therebetween; utilizing the container whereby it is exposed to sunlight and other atmospheric conditions; placing the first conductor which generally conforms to the area to be tested on one side of the area to be tested; placing a second conductor which generally conforms to the area to be tested on the other side of the area to be tested; applying a predetermined DC voltage across the conductors; recording the current flowing between the conductors; comparing the previous current with the latest recorded current to determine the degree of degradation of the dielectric properties of the nonconductor which are then correlated to the degradation of the physical properties of the container; connecting the first conductor and a conductor having a wiper blade impregnated with particulate conducting material to a DC power source; imposing a predetermined DC voltage across the first conductor and the conductor having a wiper blade; traversing the area to be tested with the wiper blade, whereby marks will appear outlining physical defects and smudges will appear if the thickness is below a predetermined value.
Claim 2
Independent Claim
254 words
A method for testing a non-conducting container for deterioration due to exposure to sunlight and other atmospheric conditions, said method comprising the steps of: placing a first conductor which generally conforms to the area to be tested on one side of the container; placing another conductor which generally conforms to the area to be tested on the side opposite the side having the first conductor; applying a predetermined DC voltage across the conductor and recording the current flowing therebetween; utilizing the container whereby it is exposed to sunlight and other atmospheric conditions; placing the first conductor which generally conforms to the area to be tested on one side of the area to be tested; placing a second conductor which generally conforms to the area to be tested on the other side of the area to be tested; applying a predetermined DC voltage across the conductors; recording the current flowing between the conductors; comparing the previous current with the latest recorded current to determine the degree of degradation of the dielectric properties of the nonconductor which are then correlated to the degradation of the physical properties of the container; connecting the first conductor and a conductor having a wiper blade impregnated with particulate conducting material to a DC power source; imposing a predetermined DC voltage across the first conductor and the conductor having a wiper blade; traversing the area to be tested with the wiper blade, whereby marks will appear outlining physical defects and smudges will appear if the thickness is below a predetermined value.
References Cited (Backward Citations)
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1981-03-20 | 1981-09-19 | 1982-03-21 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 1985-03-20 | 1985-09-19 | 1986-03-21 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 1989-03-20 | 1989-09-19 | 1990-03-21 | $7700.00 | Window Closed / Lapsed |