Abstract

Abstract Epoxy resin is pretreated with an organic solvent such as furfuryl alcohol, methyl alcohol, ethyl alcohol, n-propyl alcohol, iso-propyl alcohol, formic acid, acetic acid, propionic acid, butyric acid, methyl formate, ethyl formate, propyl formate, methyl acetate, ethyl acetate, propyl acetate, methyl propionate, ethyl propionate, propyl propionate, methyl butyrate, ethyl butyrate, propyl butyrate, acetone, diethyl ketone, dipropyl ketone, methylethyl ketone, diisopropyl ketone, methylpropyl ketone, ethylpropyl ketone, acetonitrile and nitromethane as a pretreating solution, and the pretreated resin is then etched with an etching solution containing hydrogen peroxide or a persulfate and sulfuric acid, or the resin is pretreated with an organic solvent containing furfuryl alcohol, methyl alcohol, ethyl alcohol, n-propyl alcohol or isopropyl alcohol, and formamide or ethylene glycol, 1,2-propylene glycol or glycerine, and the pretreated resin is etched with an etching solution containing hydrogen peroxide and sulfuric acid to roughen the surface of the resin. A good adhesiveness is obtained between the surface of the resin and a film of metal when the resin is coated with a metal.

Inventors

  • 👤 Akitoshi Sugio
  • 👤 Yukiya Masuda
  • 👤 Toshihiko Kobayashi
  • 👤 Koichi Nakano
  • 👤 Tsukasa Sawai

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-01 18:14
CPC Classifications
C; C08; C08J; C08J7/00; C08J7/12; C08J7/14; C23; C23C; C23C18/00; C23C18/16; C23C18/18; C23C18/20; C23C18/22; C08J2363/00

Claims Analysis

Total Claims: 30
Claim 1
Independent Claim 191 words
A process for roughening a surface of epoxy resin, which comprises pretreating an epoxy resin with (1) an organic solvent comprising at least one compound selected from the group consisting of: (a) a compound represented by the general formula, R 1 --OH, wherein R 1 is an alkyl group or furfuryl group, (b) a compound represented by the general formula, ##STR3## wherein R 2 is a hydrogen atom, or an alkyl group, R 3 is an alkyl group, an alkoxyl group, or a hydroxyl group, and when R 2 is a hydrogen atom, R 3 is an alkoxyl group or a hydroxyl group, and (c) a compound represented by the general formula, CH 3 --X, wherein X is a nitrile group, or a nitro group, or (2) an organic solvent comprising: (a) a compound represented by the general formula, R 1 --OH, wherein R 1 has the same meaning as defined above, and (d) at least one compound selected from the group consisting of formamide and a polyhydric alcohol as a pretreating solution, and then etching the resulting pretreated epoxy resin with an etching solution containing hydrogen peroxide and sulfuric acid.
Claim 2
Dependent Claim 191 words
A process for roughening a surface of epoxy resin, which comprises pretreating an epoxy resin with (1) an organic solvent comprising at least one compound selected from the group consisting of: (a) a compound represented by the general formula, R 1 --OH, wherein R 1 is an alkyl group or furfuryl group, (b) a compound represented by the general formula, ##STR3## wherein R 2 is a hydrogen atom, or an alkyl group, R 3 is an alkyl group, an alkoxyl group, or a hydroxyl group, and when R 2 is a hydrogen atom, R 3 is an alkoxyl group or a hydroxyl group, and (c) a compound represented by the general formula, CH 3 --X, wherein X is a nitrile group, or a nitro group, or (2) an organic solvent comprising: (a) a compound represented by the general formula, R 1 --OH, wherein R 1 has the same meaning as defined above, and (d) at least one compound selected from the group consisting of formamide and a polyhydric alcohol as a pretreating solution, and then etching the resulting pretreated epoxy resin with an etching solution containing hydrogen peroxide and sulfuric acid.
Claim 3
Dependent Claim 33 words
A process according to claim 1, wherein the compounds (a), (b) and (c) have alkyl groups of not more than three carbon atoms as R 1 , R 2 and R 3 .
Claim 4
Dependent Claim 25 words
A process according to claim 1, wherein the compound (c) has an alkoxyl group of not more than three carbon atoms as R 3 .
Claim 5
Dependent Claim 75 words
A process according to claim 1, wherein the compounds (a), (b) and (c) are furfuryl alcohol, methyl alcohol, ethyl alcohol, n-propyl alcohol, isopropyl alcohol, formic acid, acetic acid, propionic acid, butyric acid, methyl formate, ethyl formate, propyl formate, methyl acetate, ethyl acetate, propyl acetate, methyl propionate, ethyl propionate, propyl propionate, methyl butyrate, ethyl butyrate, propyl butyrate, acetone, diethyl ketone, dipropyl ketone, methyl ethyl ketone, diisopropyl ketone, methyl propyl ketone, ethyl propyl ketone, acetonitrile and nitromethane.
Claim 6
Dependent Claim 36 words
A process according to claim 1, wherein the compounds (a), (b) and (c) are furfuryl alcohol, methyl alcohol, ethyl alcohol, n-propyl alcohol, formic acid, acetic acid, methyl formate, ethyl formate, acetone, methylethyl ketone, acetonitrile and nitromethane.
Claim 7
Dependent Claim 16 words
A process according to claim 1, wherein the polyhydric alcohol has 2 to 3 carbon atoms.
Claim 8
Dependent Claim 17 words
A process according to claim 6, wherein the polyhydric alcohol is ethylene glycol, 1,2-propylene glycol or glycerin.
Claim 9
Dependent Claim 24 words
A process according to claim 1, wherein the pretreating solution is an aqueous solution containing at least 15% by volume of the organic compound.
Claim 10
Dependent Claim 24 words
A process according to claim 1, wherein a mixing ratio of the compound (a) to the compound (d) is 1:0.1 to 10 by volume.
Claim 11
Dependent Claim 28 words
A process according to claim 1, wherein the etching solution contains at least 1 W/V % of hydrogen peroxide and at least 30% by volume of sulfuric acid.
Claim 12
Dependent Claim 24 words
A process according to claim 1, wherein the pretreatment is carried out by dipping, by spraying or contacting with vapors of the pretreating solution.
Claim 13
Dependent Claim 31 words
A process according to claim 1, wherein the pretreatment is carried out at a temperature of 20° C to a boiling point of the pretreating solution for 3 to 60 minutes.
Claim 14
Dependent Claim 17 words
A process according to claim 1, wherein the epoxy resin is washed with water after the pretreatment.
Claim 15
Dependent Claim 16 words
A process according to claim 1, wherein the etching is carried out by dipping or spraying.
Claim 16
Dependent Claim 22 words
A process according to claim 1, wherein the etching is carried out at 30° to 80° C for 3 to 60 minutes.
Claim 17
Dependent Claim 146 words
A process for roughening a surface of epoxy resin, which comprises pretreating an epoxy resin with an organic solvent comprising at least one compound selected from the group consisting of: (a) a compound represented by the general formula, R 1 --OH, wherein R 1 is an alkyl group or furfuryl group, (b) a compound represented by the general formula, ##STR4## wherein R 2 is a hydrogen atom, or an alkyl group, R 3 is an alkyl group, an alkoxyl group, or a hydroxyl group, and when R 2 is a hydrogen atom, R 3 is an alkoxyl group or a hydroxyl group, and (c) a compound represented by the general formula, CH 3 --X, wherein X is a nitrile group, or a nitro group as a pretreating solution, and then etching the resulting pretreated epoxy resin with an etching solution containing a persulfate and sulfuric acid.
Claim 18
Dependent Claim 146 words
A process for roughening a surface of epoxy resin, which comprises pretreating an epoxy resin with an organic solvent comprising at least one compound selected from the group consisting of: (a) a compound represented by the general formula, R 1 --OH, wherein R 1 is an alkyl group or furfuryl group, (b) a compound represented by the general formula, ##STR4## wherein R 2 is a hydrogen atom, or an alkyl group, R 3 is an alkyl group, an alkoxyl group, or a hydroxyl group, and when R 2 is a hydrogen atom, R 3 is an alkoxyl group or a hydroxyl group, and (c) a compound represented by the general formula, CH 3 --X, wherein X is a nitrile group, or a nitro group as a pretreating solution, and then etching the resulting pretreated epoxy resin with an etching solution containing a persulfate and sulfuric acid.
Claim 19
Dependent Claim 33 words
A process according to claim 16, wherein the compounds (a), (b) and (c) have alkyl groups of not more than three carbon atoms as R 1 , R 2 and R 3 .
Claim 20
Dependent Claim 25 words
A process according to claim 16, wherein the compound (c) has an alkoxyl group of not more than three carbon atoms as R 3 .
Claim 21
Dependent Claim 74 words
A process according to claim 16, wherein the compounds (a), (b) and (c) are furfuryl alcohol, methyl alcohol, ethyl alcohol, n-propyl alcohol, iso-propyl alcohol, formic acid, acetic acid, propionic acid, butyric acid, methyl formate, ethyl formate, propyl formate, methyl acetate, ethyl acetate, propyl acetate, methyl propionate, ethyl propionate, propyl propionate, methyl butyrate, ethyl butyrate, propyl butyrate, acetone, diethyl ketone, dipropyl ketone, methylethyl ketone, diisopropyl ketone, methyl propyl ketone, ethyl propyl ketone, acetonitrile and nitromethane.
Claim 22
Dependent Claim 35 words
A process according to claim 16, wherein the compounds (a), (b) and (c) are furfuryl alcohol, methyl alcohol, ethyl alcohol, n-propyl alcohol, formic acid, acetic acid, methyl formate, ethyl formate, acetone, methylethylketone, acetonitrile, and nitromethane.
Claim 23
Dependent Claim 24 words
A process according to claim 16, wherein the pretreating solution is an aqueous solution containing at least 15% by volume of the organic compounds.
Claim 24
Dependent Claim 27 words
A process according to claim 16, wherein the etching solution contains at least 1 W/V % of persulfate and at least 30% by volume of sulfuric acid.
Claim 25
Dependent Claim 17 words
A process according to claim 22, wherein the persulfate is ammonium persulfate, sodium persulfate or potassium persulfate.
Claim 26
Dependent Claim 23 words
A process according to claim 16, wherein the pretreatment is carried out by dipping, by spraying, contacting with vapors of the pretreating solution.
Claim 27
Dependent Claim 31 words
A process according to claim 16, wherein the pretreatment is carried out at a temperature of 20° C to a boiling point of the pretreating solution for 3 to 60 minutes.
Claim 28
Dependent Claim 17 words
A process according to claim 16, wherein the epoxy resin is washed with water after the pretreatment.
Claim 29
Dependent Claim 16 words
A process according to claim 16, wherein the etching is carried out by dipping or spraying.
Claim 30
Dependent Claim 22 words
A process according to claim 16, wherein the etching is carried out at 30° to 80° C for 3 to 60 minutes.

References Cited (Backward Citations)

US3553085A Cited
US3808028A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1981-04-24 1981-10-24 1982-04-25 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1985-04-24 1985-10-24 1986-04-25 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1989-04-24 1989-10-24 1990-04-25 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag