Abstract

Abstract A multilayer dielectric mirror wherein the mirror substrate is of garnet. Chemical-mechanical final polishing of the substrate provides a surface relatively free of inhomogeneous strain for the deposition thereon of relatively homogeneous individual layers for a multilayer dielectric mirror coating.

Inventors

  • 👤 Rodney D. Henry

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-28 12:15
CPC Classifications
G; G02; G02B; G02B5/00; G02B5/08; G02B5/0816; G02B5/0825; G02B5/0833; G02B1/00; G02B1/02; H; H01; H01S; H01S3/00; H01S3/05; H01S3/08; H01S3/08059; Y; Y10; Y10S; Y10S117/00; Y10S117/903; Y10S117/904; Y10S428/00; Y10S428/913; Y10T; Y10T428/00; Y10T428/31

Claims Analysis

Total Claims: 5
Claim 1
Independent Claim 225 words
A multilayer dielectric laser mirror comprising: a garnet substrate having a substantially rectangular cross-section wherein at least one side of said substrate is a mirror surface chemical-mechanical polished to be relatively free of inhomogeneous strain and wherein said garnet is a metal oxide having the general formula J 3 Q 5 O 12 wherein O is oxygen, J is at least one element selected from the group consisting of the lanthanide series of the Periodic Table, lanthanum, yttrium, magnesium, calcium, strontium, barium, lead, cadmium, lithium, sodium, and potassium, and Q is at least one element selected from the group consisting of gallium, indium, scandium, titanium, vanadium, chromium, manganese, rhodium, zirconium, hafnium, molybdenum, niobium, tantalum, tungsten, and alluminum; and a mirror coating deposited on said mirror surface of said substrate, said mirror coating consisting of a first plurality of layers of a first non-magnetic dielectric material having a relatively higher index of refraction and a second plurality of layers of a second non-magnetic dielectric material having a relatively lower index of refraction wherein said layers of said first dielectric material are interleaved alternately with said layers of said second dielectric material in a stacked relationship relative to each other and relative to said mirror, and wherein said first and second dielectric materials are selected from the group consisting of titanium dioxide, magnesium fluoride, and silicon dioxide.
Claim 2
Dependent Claim 225 words
A multilayer dielectric laser mirror comprising: a garnet substrate having a substantially rectangular cross-section wherein at least one side of said substrate is a mirror surface chemical-mechanical polished to be relatively free of inhomogeneous strain and wherein said garnet is a metal oxide having the general formula J 3 Q 5 O 12 wherein O is oxygen, J is at least one element selected from the group consisting of the lanthanide series of the Periodic Table, lanthanum, yttrium, magnesium, calcium, strontium, barium, lead, cadmium, lithium, sodium, and potassium, and Q is at least one element selected from the group consisting of gallium, indium, scandium, titanium, vanadium, chromium, manganese, rhodium, zirconium, hafnium, molybdenum, niobium, tantalum, tungsten, and alluminum; and a mirror coating deposited on said mirror surface of said substrate, said mirror coating consisting of a first plurality of layers of a first non-magnetic dielectric material having a relatively higher index of refraction and a second plurality of layers of a second non-magnetic dielectric material having a relatively lower index of refraction wherein said layers of said first dielectric material are interleaved alternately with said layers of said second dielectric material in a stacked relationship relative to each other and relative to said mirror, and wherein said first and second dielectric materials are selected from the group consisting of titanium dioxide, magnesium fluoride, and silicon dioxide.
Claim 3
Dependent Claim 28 words
A mirror as recited in claim 1 wherein said plurality of layers have a mirror coating surface roughness due to physical thickness inhomogeneity of less than 100 angstroms.
Claim 4
Independent Claim 155 words
A method of forming a multilayer dielectric laser mirror which comprises: providing a garnet substrate having a substantially rectangular cross-section; polishing a selected side of said substrate to form a mirror surface thereon; providing an abrasive slurry; adjusting the pH of said abrasive slurry by the addition thereto of an etchant for said garnet; final polishing said mirror surface of said garnet substrate using said pH-adjusted abrasive slurry; and depositing a mirror coating on said mirror surface of said substrate, said mirror coating consisting of a first plurality of layers of a first non-magnetic dielectric material having a relatively higher index of refraction and a second plurality of layers of a second non-magnetic dielectric material having a relatively lower index of refraction wherein said layers of said first dielectric material are interleaved alternately with said layers of said second dielectric material in a stacked relationship relative to each other and relative to said mirror surface.
Claim 5
Independent Claim 155 words
A method of forming a multilayer dielectric laser mirror which comprises: providing a garnet substrate having a substantially rectangular cross-section; polishing a selected side of said substrate to form a mirror surface thereon; providing an abrasive slurry; adjusting the pH of said abrasive slurry by the addition thereto of an etchant for said garnet; final polishing said mirror surface of said garnet substrate using said pH-adjusted abrasive slurry; and depositing a mirror coating on said mirror surface of said substrate, said mirror coating consisting of a first plurality of layers of a first non-magnetic dielectric material having a relatively higher index of refraction and a second plurality of layers of a second non-magnetic dielectric material having a relatively lower index of refraction wherein said layers of said first dielectric material are interleaved alternately with said layers of said second dielectric material in a stacked relationship relative to each other and relative to said mirror surface.

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1981-07-17 1982-01-16 1982-07-18 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1985-07-17 1986-01-16 1986-07-18 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1989-07-17 1990-01-16 1990-07-18 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag