Liquid developer for use in electrostatic photography comprising natural resins and natural resin-modified thermosetting resins combined with polymers
Assignee: Ricoh Co Ltd
•
Filing: 1976-12-16
•
Granted: 1978-08-01
•
Expires: 1996-12-16
Abstract
Abstract A liquid developer for use in electrostatic photography which comprises at least one kind of resin which is substantially insoluble in a carrier liquid consisting of a non-aqueous solvent with high insulating property and low dielectric constant, a polymer consisting essentially of at least one kind of monomer which can dissolve said resin and a coloring agent, each component being contained in said carrier liquid, is excellent in dispersion stability, fixability and redispersibility so that it is suitable for use in offset printing and various transfers as well.
Inventors
- 👤 Kazuo Tsubuko
- 👤 Yasuo Kizu
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-11-03 11:41
CPC Classifications
G; G03; G03G; G03G9/00; G03G9/08; G03G9/12; G03G9/13; G03G9/131; Y; Y10; Y10S; Y10S524/00; Y10S524/901
Claims Analysis
Total Claims: 12
Claim 1
Independent Claim
185 words
A liquid developer for use in electrostatic photography consisting essentially of a toner dispersed in a carrier liquid having a high resistivity and a low dielectric constant, said toner consisting essentially of pigment or dye particles and a non-aqueous resin dispersion, said non-aqueous resin dispersion consisting essentially of a non-aqueous solvent having a high insulating property and a low dielectric constant selected from the group consisting of aliphatic hydrocarbons and halogen derivatives thereof, said solvent having dispersed therein at least one resin which is substantially insoluble in said solvent, said resin being selected from the group consisting of natural resins and natural resin-modified thermosetting resins, said solvent also having dispersed therein a polymer of at least one monomer A which has the formula ##STR2## wherein R is hydrogen or CH 3 , D is --COOC n H 2n+1 or --OC n H 2n+1 , and n is an integer ranging from 6 to 20, said monomer A being capable of dissolving said resin, the weight ratio of said resin:said polymer being in the range of from about 5-50:50-95, said polymer being solvated by said solvent.
Claim 2
Dependent Claim
185 words
A liquid developer for use in electrostatic photography consisting essentially of a toner dispersed in a carrier liquid having a high resistivity and a low dielectric constant, said toner consisting essentially of pigment or dye particles and a non-aqueous resin dispersion, said non-aqueous resin dispersion consisting essentially of a non-aqueous solvent having a high insulating property and a low dielectric constant selected from the group consisting of aliphatic hydrocarbons and halogen derivatives thereof, said solvent having dispersed therein at least one resin which is substantially insoluble in said solvent, said resin being selected from the group consisting of natural resins and natural resin-modified thermosetting resins, said solvent also having dispersed therein a polymer of at least one monomer A which has the formula ##STR2## wherein R is hydrogen or CH 3 , D is --COOC n H 2n+1 or --OC n H 2n+1 , and n is an integer ranging from 6 to 20, said monomer A being capable of dissolving said resin, the weight ratio of said resin:said polymer being in the range of from about 5-50:50-95, said polymer being solvated by said solvent.
Claim 3
Dependent Claim
60 words
A liquid developer according to claim 1, which further comprises at least one dispersant selected from the group consisting of wax and polyolefins having a softening temperature in the range of 60° - 130° C, wherein the amount of said dispersant is in the range of 10 - 50 parts by weight per 100 parts by weight of said polymer.
Claim 4
Dependent Claim
18 words
A liquid developer according to claim 1, wherein said polymer consists essentially of a homopolymer of monomer A.
Claim 5
Dependent Claim
65 words
A liquid developer according to claim 1, wherein said polymer consists essentially of a copolymer of said monomer A and at least one monomer B selected from the group consisting of glycidyl methacrylate, glycidyl acrylate, propylene glycol monoacrylate, propylene glycol methacrylate, hydroxyethyl methacrylate, acrylonitrile and methacrylonitrile, wherein the weight ratio of said monomer A to said monomer B is in the range of about 70-99:30-1.
Claim 6
Dependent Claim
77 words
A liquid developer according to claim 1, wherein said polymer consists essentially of a copolymer of said monomer A and at least one monomer C selected from the group consisting of acrylic acid, methacrylic acid, lower alkyl esters of acrylic acid and methacrylic acid in which said alkyl has 1 to 4 carbon atoms, styrene, methyl styrene, vinyl toluene and vinyl acetate, wherein the weight ratio of monomer A:monomer C is in the range of about 50-90:50-10.
Claim 7
Dependent Claim
115 words
A liquid developer according to claim 1 wherein said polymer consists essentially of a terpolymer of said monomer A, monomer B and monomer C, wherein monomer B is at least one monomer selected from the group consisting of glycidyl methacrylate, glycidyl acrylate, propylene glycol monoacrylate, propylene glycol methacrylate, hydroxyethyl methacrylate, acrylonitrile and methacrylonitrile, wherein monomer C is at least one monomer selected from the group consisting of acrylic acid, methacrylic acid, lower alkyl esters of acrylic acid and methacrylic acid in which said alkyl has 1 to 4 carbon atoms, styrene, methyl styrene, vinyl toluene and vinyl acetate, and wherein the weight ratio of monomer A:monomer B:monomer C is in the range of about 60-90:20-1:20-1.
Claim 8
Dependent Claim
43 words
A liquid developer according to claim 1 wherein said resin is selected from the group consisting of natural ester gum resins, natural hardened rosin, natural resin-modified maleic resins, natural resin-modified phenol resins, natural resin-modified polyester resins, natural resin-modified pentaerythritol resins and mixtures thereof.
Claim 9
Dependent Claim
29 words
A liquid developer according to claim 1 containing from 0.5 to 10 parts by weight of said polymer, per one part by weight of said pigment or dye particles.
Claim 10
Dependent Claim
19 words
A liquid developer according to claim 1 in which said carrier liquid and said non-aqueous solvent are the same.
Claim 11
Dependent Claim
41 words
A liquid developer according to claim 1, in which said dispersion has been prepared by dissolving said resin in said monomer A to form a solution thereof, and polymerizing said monomer in said solution, in the presence of said non-aqueous solvent.
Claim 12
Dependent Claim
24 words
A process for developing an electrostatic latent image which comprises applying to said electrostatic latent image a liquid developer as claimed in claim 1.
References Cited (Backward Citations)
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1981-07-31 | 1982-01-30 | 1982-08-01 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 1985-07-31 | 1986-01-30 | 1986-08-01 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 1989-07-31 | 1990-01-30 | 1990-08-01 | $7700.00 | Window Closed / Lapsed |