Abstract

Abstract Cobalt catalyst values are recovered from mother liquors remaining from oxidations to mono- or polycarboxylic acids in lower aliphatic monocarboxylic acids in presence of catalysts comprising cobalt and bromide ions by (1) if necessary, adjusting the cobalt and bromide concentrations so that they are within specified limits (2) adsorbing cobalt and bromide ions (differentially with respect to extraneous ions) on a strongly basic anion exchange resin and (3) desorbing cobalt and bromide ions with lower aliphatic monocarboxylic acid containing more than 10% by weight of water.

Inventors

  • 👤 Peter J. V. Jones

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-31 22:05
CPC Classifications
B; B01; B01J; B01J23/00; B01J23/70; B01J23/74; B01J23/75; B01J23/90; B01J23/94; B01J27/00; B01J27/28; B01J27/32

Claims Analysis

Total Claims: 11
Claim 1
Independent Claim 173 words
A process for recovering cobalt catalyst values from the reaction mother liquor resulting from the oxidation in the liquid phase to a mono or polycarboxylic acid of a feedstock oxidisable thereto by means of a molecular oxygen-containing gas in presence of a lower aliphatic monocarboxylic acid and of a catalyst comprising cobalt and bromide ions followed by separation of the said mono or polycarboxylic acid from the said reaction mother liquor, which process comprises, (1) providing in the said reaction a mother liquor having a cobalt concentration from 0.1% to 10% by weight of cobalt in said lower aliphatic monocarboxylic acid, and, having the bromide concentration so that the ratio of bromide to cobalt is from 1.5:1 to 4.5:1 by weight, (2) contacting the resulting solution containing cobalt and bromide ions with a strongly basic anion exchange resin whereby cobalt and bromide values are adsorbed on said resin, and (3) eluting cobalt and bromide values from said anion exchange resin with lower aliphatic monocarboxylic acid containing more than 10% by weight of water.
Claim 2
Dependent Claim 173 words
A process for recovering cobalt catalyst values from the reaction mother liquor resulting from the oxidation in the liquid phase to a mono or polycarboxylic acid of a feedstock oxidisable thereto by means of a molecular oxygen-containing gas in presence of a lower aliphatic monocarboxylic acid and of a catalyst comprising cobalt and bromide ions followed by separation of the said mono or polycarboxylic acid from the said reaction mother liquor, which process comprises, (1) providing in the said reaction a mother liquor having a cobalt concentration from 0.1% to 10% by weight of cobalt in said lower aliphatic monocarboxylic acid, and, having the bromide concentration so that the ratio of bromide to cobalt is from 1.5:1 to 4.5:1 by weight, (2) contacting the resulting solution containing cobalt and bromide ions with a strongly basic anion exchange resin whereby cobalt and bromide values are adsorbed on said resin, and (3) eluting cobalt and bromide values from said anion exchange resin with lower aliphatic monocarboxylic acid containing more than 10% by weight of water.
Claim 3
Dependent Claim 20 words
The process of claim 1 in which the mother liquor is concentrated by distillation prior to contacting with the resin.
Claim 4
Dependent Claim 23 words
The process of claim 1 in which the solution to be fed to the resin contains less than 10% by weight of water.
Claim 5
Dependent Claim 23 words
The process of claim 1 in which, in step 1, the ratio of bromide to cobalt is adjusted by adding more bromide ion.
Claim 6
Dependent Claim 27 words
The process of claim 1 in which cobalt and bromide values eluted from the resin in step 3 are recycled to provide catalyst values for the oxidation.
Claim 7
Dependent Claim 26 words
The process of claim 1 in which the lower aliphatic monocarboxylic acid used for elution in step 3 contains more than 25% by weight of water.
Claim 8
Dependent Claim 25 words
The process of claim 1 in which the ratio of bromide to cobalt in the solution fed to the resin is from 2.7:1 to 3.3:1.
Claim 9
Dependent Claim 58 words
The process of claim 1 in which cobalt and bromide values are separated from ions of corrosion metals and/or alkali metal ions and/or organic impurities formed in the oxidation which comprises adsorbing cobalt and bromide ions on the said resin in step 2 while at least a part of the remaining ions pass through the said resin unabsorbed.
Claim 10
Dependent Claim 23 words
The process of claim 1 in which from 10% to 50% by weight of the mother liquor resulting from the oxidation are treated.
Claim 11
Dependent Claim 41 words
The process of claim 1 in which cobalt catalyst values are recovered from the oxidation of p-xylene to terephthalic acid in the presence of a cobalt, manganese and bromide catalyst and an acetic acid solvent, for recycle to the oxidation process.

References Cited (Backward Citations)

GB899288A Cited
US3235377A Cited
US3650688A Cited
US3880920A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1982-07-30 1983-01-29 1983-07-31 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1986-07-30 1987-01-29 1987-07-31 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1990-07-30 1991-01-29 1991-07-31 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag