Abstract

Abstract In a method of making decorative panels, a liquid masking material is applied to a surface of a panel, and is cured to form a substantially solid masking layer on the surface. A pattern comprising at least one unmasked area and at least one masked area is formed in the masking layer either simultaneously with the application of the liquid masking material or subsequent to the curing step. The surface of the panel is then treated to render the unmasked areas of the surface of the panel visually distinguishable from the masked areas. In one embodiment of the invention the masking layer is elastomeric and the surface of the panel is treated by sandblasting, after which the masking layer is removed. The entire process may then be repeated to provide a dual density effect. In another embodiment of the invention an asphaltum masking layer is applied to a mirror forming layer on a panel, after which the portions of the mirror forming layer corresponding to the unmasked areas are chemically removed.

Inventors

  • 👤 Robert C. Parsons

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-01 11:42
CPC Classifications
B; B24; B24C; B24C1/00; B24C1/04; B41; B41M; B41M1/00; B41M1/12; B44; B44C; B44C1/00; B44C1/22; B44C1/221

Claims Analysis

Total Claims: 3
Claim 1
Independent Claim 175 words
A method of making decorative panels comprising: covering a screen with a photosensitive emulsion; photographically exposing the photosensitive emulsion on the screen with a predetermined image; developing the exposed photosensitive emulsion such that portions of the screen corresponding to the image photographically exposed on the screen permits the passage of liquid therethrough; directing a liquid asphaltum masking material through the screen onto a mirror forming layer on a surface of a plastic panel and thereby applying the liquid asphaltum masking material in accordance with a high degree of resolution of the predetermined pattern; curing the liquid asphaltum masking material and thereby forming a solid asphaltum masking layer on the mirror forming layer on the surface of the plastic panel in accordance with a high degree of resolution of the predetermined pattern; and subsequently dissolving the portions of the mirror forming layer on the surface of the plastic panel corresponding to the unmasked areas and thereby providing a plastic panel comprising mirrored and nonmirrored areas corresponding to a high degree of resolution of the predetermined pattern.
Claim 2
Independent Claim 175 words
A method of making decorative panels comprising: covering a screen with a photosensitive emulsion; photographically exposing the photosensitive emulsion on the screen with a predetermined image; developing the exposed photosensitive emulsion such that portions of the screen corresponding to the image photographically exposed on the screen permits the passage of liquid therethrough; directing a liquid asphaltum masking material through the screen onto a mirror forming layer on a surface of a plastic panel and thereby applying the liquid asphaltum masking material in accordance with a high degree of resolution of the predetermined pattern; curing the liquid asphaltum masking material and thereby forming a solid asphaltum masking layer on the mirror forming layer on the surface of the plastic panel in accordance with a high degree of resolution of the predetermined pattern; and subsequently dissolving the portions of the mirror forming layer on the surface of the plastic panel corresponding to the unmasked areas and thereby providing a plastic panel comprising mirrored and nonmirrored areas corresponding to a high degree of resolution of the predetermined pattern.
Claim 3
Dependent Claim 35 words
The method of making decorative panels according to claim 1 wherein the step of dissolving the unmasked portions of the mirror forming layer is carried out by dissolving the mirror forming layer in sodium hydroxide.

References Cited (Backward Citations)

US504543A Cited
US1869695A Cited
US2204147A Cited
US2358710A Cited
US3507740A Cited
US3532052A Cited
US3579926A Cited
US4076535A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1983-04-22 1983-10-22 1984-04-22 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1987-04-22 1987-10-22 1988-04-22 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1991-04-22 1991-10-22 1992-04-22 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag