Metallurgical vessel

Assignee: Pennsylvania Engineering Corp
•
Filing: 1979-11-13
•
Granted: 1981-06-09
•
Expires: 1999-11-13
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract A metallurgical vessel has releasably coupled, semicylindrical upper and lower sections arranged such that the axis of revolution of one section lies in a plane normal relative to the rotational axis of the other. The dimension of each section in the axial direction being the same as the dimension of the other section in the direction normal to the axis. The vessel is mounted for rotation about the axis of the lower section and an elongate charging mouth is formed in the upper section and is arranged with its major axis parallel to the axis of the lower section. A plurality of tuyeres extend through the lower section of the vessel and each tuyere includes a first tuyere pipe for injecting oxygen beneath the level of molten metal within the vessel, a second tuyere pipe disposed in surrounding relation to the oxygen pipe for injecting powdered materials entrained in a nonoxidizing gas and a third pipe surrounding the second pipe for injecting a hydrocarbon shielding fluid. The vessel is mounted for rotation about the axis of the lower sections by means of a pair of rings.

Inventors

  • 👤 Eberhard G. Schempp

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-08 11:00
CPC Classifications
C; C21; C21C; C21C5/00; C21C5/28; C21C5/30; C21C5/34; C21C5/42; C21C5/46; C21C5/48; C21C5/50

Claims Analysis

Total Claims: 5
Claim 1
Independent Claim 81 words
A method of treating a molten ferrous metal comprising the steps of containing said metal in a metallurgical vessel, delivering oxygen to said metal in a first flow passage, entraining a highly oxidizable desulfurizing agent in a nonoxidizing gas and delivering the same to said molten metal through a separate second passage concentric with said first passage and delivering hydrocarbon shielding fluid to said vessel through a third flow passage disposed in surrounding relation to said first and second flow passages.
Claim 2
Independent Claim 81 words
A method of treating a molten ferrous metal comprising the steps of containing said metal in a metallurgical vessel, delivering oxygen to said metal in a first flow passage, entraining a highly oxidizable desulfurizing agent in a nonoxidizing gas and delivering the same to said molten metal through a separate second passage concentric with said first passage and delivering hydrocarbon shielding fluid to said vessel through a third flow passage disposed in surrounding relation to said first and second flow passages.
Claim 3
Dependent Claim 30 words
The method set forth in claim 1 wherein said desulfurizing agent is taken from a group consisting of calcium carbide, calcium silicate, phosphorous and a mixture of phosphorous and lime.
Claim 4
Dependent Claim 26 words
The method set forth in claim 2 wherein said desulfurizing agent is entrained in a non-oxidizing gas taken from a group consisting of nitrogen and argon.
Claim 5
Dependent Claim 27 words
The method set forth in claim 1, 2 or 3 wherein said second passage surrounds said first passage and is disposed between said first and third passages.

References Cited (Backward Citations)

US3771998A Cited
US3832161A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1984-06-08 1984-12-08 1985-06-09 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1988-06-08 1988-12-08 1989-06-09 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1992-06-08 1992-12-08 1993-06-09 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag