Abstract

Abstract A method of recovering chromium values and potential energy from liquid and solid leather tannery wastes comprising pyrolyzing the tannery wastes to produce a burnable fuel product comprising gases and liquids and a substantially solid chromium-containing residue, recovering chromium compounds from the solid residue and using the fuel to supply energy for the system.

Inventors

  • 👤 H. S. Muralidhara

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-02 21:37
CPC Classifications
C; C02; C02F; C02F11/00; C02F11/10; C01; C01G; C01G37/00; C01G37/08; C02F2103/00; C02F2103/22; C02F2103/24; Y; Y02; Y02W; Y02W10/00; Y02W10/40

Claims Analysis

Total Claims: 16
Claim 1
Independent Claim 131 words
A method of treating substantially solid tannery waste material containing chromium and organic matter to recover chromium in the +3 valence state and to produce fuel products comprising: (a) pyrolyzing said solid tannery waste to produce a fuel product comprising burnable gases and liquids and substantially solid residue containing chromium in a +3 valence state as an organic chromium complex soluble in an about 1 M sulfuric acid solution, (b) separating said burnable fuel product from said chromium-containing residue, and (c) recovering chromium compounds from said residue by dissolution in an about 1 M sulfuric acid solution said pyrolysis comprising subjecting said solid tannery waste in a pyrolysis zone to a temperature between 500° F. and 932° F. in the absence of an amount of gaseous oxygen substantially above about 10%.
Claim 2
Independent Claim 131 words
A method of treating substantially solid tannery waste material containing chromium and organic matter to recover chromium in the +3 valence state and to produce fuel products comprising: (a) pyrolyzing said solid tannery waste to produce a fuel product comprising burnable gases and liquids and substantially solid residue containing chromium in a +3 valence state as an organic chromium complex soluble in an about 1 M sulfuric acid solution, (b) separating said burnable fuel product from said chromium-containing residue, and (c) recovering chromium compounds from said residue by dissolution in an about 1 M sulfuric acid solution said pyrolysis comprising subjecting said solid tannery waste in a pyrolysis zone to a temperature between 500° F. and 932° F. in the absence of an amount of gaseous oxygen substantially above about 10%.
Claim 3
Dependent Claim 28 words
The method of claim 1 wherein said substantially solid tannery waste material is a mixture of chrome-tanned leather scrap and a de-watered and substantially dried liquid tannery waste.
Claim 4
Dependent Claim 24 words
The method of claim 1 wherein said solid tannery waste is pyrolyzed at a temperature of from about 500° F. to about 700° F.
Claim 5
Dependent Claim 25 words
The method of claim 1 wherein at least a portion of said separated burnable fuel product is burned to supply heat to said pyrolysis zone.
Claim 6
Dependent Claim 27 words
The method of claim 1 wherein at least a portion of said separated burnable fuel product is burned in a boiler to produce hot water or steam.
Claim 7
Dependent Claim 18 words
The method of claim 1 wherein said chromium-containing residue is treated to separate carbonaceous material from said residue.
Claim 8
Dependent Claim 26 words
The method of claim 1 wherein substantially all of said chromium is recovered from said treated residue by digestion and leaching with dilute aqueous sulfuric acid.
Claim 9
Dependent Claim 21 words
The method of claim 1 wherein at least a portion of said substantially solid tannery waste material comprises chrome-tanned leather scrap.
Claim 10
Dependent Claim 20 words
The method of claim 1 wherein said substantially solid tannery waste is obtained by drying a substantially liquid tannery waste.
Claim 11
Independent Claim 179 words
A method of treating both liquid and solid tannery waste containing chromium and organic material to recover chromium and to produce burnable fuel products comprising: (a) de-watering and substantially drying said liquid tannery waste, (b) combining said de-watered and dried liquid tannery waste with said solid tannery waste (c) pyrolyzing said combined wastes in a pyrolysis zone at a temperature of from about 500° F. to about 932° F. in the absence of an amount of gaseous oxygen substantially above about 10% to produce a burnable fuel product comprising gases and liquids and a substantially solid residue containing chromium in a +3 valence state as an organic chromium complex soluble in an about 1 M sulfuric acid solution, (d) separating said burnable fuel product from said chromium-containing residue, (e) recovering chromium from said residue by dissolution in an about 1 M sulfuric acid solution, (f) burning a portion of said burnable fuel product to supply heat to said pyrolysis zone, and (g) burning a portion of said burnable fuel product in a boiler to produce hot water and/or steam.
Claim 12
Independent Claim 179 words
A method of treating both liquid and solid tannery waste containing chromium and organic material to recover chromium and to produce burnable fuel products comprising: (a) de-watering and substantially drying said liquid tannery waste, (b) combining said de-watered and dried liquid tannery waste with said solid tannery waste (c) pyrolyzing said combined wastes in a pyrolysis zone at a temperature of from about 500° F. to about 932° F. in the absence of an amount of gaseous oxygen substantially above about 10% to produce a burnable fuel product comprising gases and liquids and a substantially solid residue containing chromium in a +3 valence state as an organic chromium complex soluble in an about 1 M sulfuric acid solution, (d) separating said burnable fuel product from said chromium-containing residue, (e) recovering chromium from said residue by dissolution in an about 1 M sulfuric acid solution, (f) burning a portion of said burnable fuel product to supply heat to said pyrolysis zone, and (g) burning a portion of said burnable fuel product in a boiler to produce hot water and/or steam.
Claim 13
Dependent Claim 18 words
The method of claim 10 wherein said chromium-containing residue is treated to separate carbonaceous material from said residue.
Claim 14
Dependent Claim 28 words
The method of claim 10 wherein substantially all of said chromium is recovered from said treated residue by digestion and leaching and precipitation utilizing dilute aqueous sulfuric acid.
Claim 15
Dependent Claim 190 words
In a process for tanning leather with a chromium-containing compound whereby chromium compound containing liquid and solid leather waste materials are produced as by-products, the improvement comprising: (a) de-watering and substantially drying said liquid tannery waste, (b) combining said de-watered and dried liquid tannery waste with said solid tannery waste, (c) pyrolyzing said combined wastes in a pyrolysis zone at a temperature of from about 500° F. to about 932° F. in the absence of an amount of gaseous oxygen substantially above about 10% to produce a burnable fuel product comprising gases and liquids and a substantially solid residue containing chromium in a +3 valence state as an organic chromium complex soluble in an about 1 M sulfuric acid solution, (d) separating said burnable fuel product from said chromium-containing residue, (e) recovering chromium from said residue by leaching with an about 1 M sulfuric acid solution, (f) burning a portion of said burnable fuel product to supply heat to said pyrolysis zone, (g) burning a portion of said burnable fuel product in a boiler to produce hot water and/or steam, and (h) recycling said recovered chromium to said tanning step.
Claim 16
Dependent Claim 190 words
In a process for tanning leather with a chromium-containing compound whereby chromium compound containing liquid and solid leather waste materials are produced as by-products, the improvement comprising: (a) de-watering and substantially drying said liquid tannery waste, (b) combining said de-watered and dried liquid tannery waste with said solid tannery waste, (c) pyrolyzing said combined wastes in a pyrolysis zone at a temperature of from about 500° F. to about 932° F. in the absence of an amount of gaseous oxygen substantially above about 10% to produce a burnable fuel product comprising gases and liquids and a substantially solid residue containing chromium in a +3 valence state as an organic chromium complex soluble in an about 1 M sulfuric acid solution, (d) separating said burnable fuel product from said chromium-containing residue, (e) recovering chromium from said residue by leaching with an about 1 M sulfuric acid solution, (f) burning a portion of said burnable fuel product to supply heat to said pyrolysis zone, (g) burning a portion of said burnable fuel product in a boiler to produce hot water and/or steam, and (h) recycling said recovered chromium to said tanning step.

References Cited (Backward Citations)

DE1955747A1 Cited
US4086319A Cited
US4215989A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1985-05-31 1985-11-30 1986-06-01 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1989-05-31 1989-11-30 1990-06-01 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1993-05-31 1993-11-30 1994-06-01 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag