Abstract
Abstract In a method for bleaching oxygen delignified cellulose-containing pulp such as sulphate, sodium and sulphite pulps with ozone and peroxide, the ozone treatment takes place at two stages, the alkaline solution which is added subsequent to the ozone treatment includes peroxide and complex formers, and 55 to 85% of the total amount of chemicals is added at the first stage.
Inventors
- 👤 Bjorn H. Fritzvold
- 👤 Nicolai Soteland
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-11-08 16:58
CPC Classifications
D; D21; D21C; D21C9/00; D21C9/10; D21C9/1057
Claims Analysis
Total Claims: 14
Claim 1
Independent Claim
183 words
In a method of bleaching coniferous wood pulp wherein said pulp is first oxygen delignified to a kappa number of 5 to 15 and then bleached by treatment with ozone and peroxide, the improvement consisting essentially of the sequential steps of: (A) a first stage having (1) an ozone treatment comprising the sequential steps of washing and pH adjustment with an acid to a pH≦7, dewatering to 25-60% dry matter, fluffing, and treatment with ozone, and immediately following the ozone treatment (2) an alkaline peroxide treatment comprising treatment with a composition consisting essentially of water, an alkaline, a complex former, and a peroxide; and (B) a second stage having (1) an ozone treatment comprising the sequential steps of washing and pH adjustment with an acid to a pH≦7, dewatering to 25-60% dry matter, fluffing, and treatment with ozone, and immediately following the ozone treatment (2) an alkaline peroxide treatment comprising treatment with a composition consisting essentially of water, an alkaline, a complex former, and a peroxide; with the proviso that 55-85% of the total quantity of chemicals are used in the first stage.
Claim 2
Dependent Claim
183 words
In a method of bleaching coniferous wood pulp wherein said pulp is first oxygen delignified to a kappa number of 5 to 15 and then bleached by treatment with ozone and peroxide, the improvement consisting essentially of the sequential steps of: (A) a first stage having (1) an ozone treatment comprising the sequential steps of washing and pH adjustment with an acid to a pH≦7, dewatering to 25-60% dry matter, fluffing, and treatment with ozone, and immediately following the ozone treatment (2) an alkaline peroxide treatment comprising treatment with a composition consisting essentially of water, an alkaline, a complex former, and a peroxide; and (B) a second stage having (1) an ozone treatment comprising the sequential steps of washing and pH adjustment with an acid to a pH≦7, dewatering to 25-60% dry matter, fluffing, and treatment with ozone, and immediately following the ozone treatment (2) an alkaline peroxide treatment comprising treatment with a composition consisting essentially of water, an alkaline, a complex former, and a peroxide; with the proviso that 55-85% of the total quantity of chemicals are used in the first stage.
Claim 3
Dependent Claim
27 words
The method of claim 1 wherein the pH adjustment with an acid is by the addition of sulfuric acid or acid condensates from a sulphite digestion process.
Claim 4
Dependent Claim
20 words
The method of claim 2 wherein the pulp being bleached is a sulphate pulp and the acid is sulfuric acid.
Claim 5
Dependent Claim
62 words
The method of claim 3 wherein the alkaline is NaOH, the peroxide is hydrogen peroxide, the complex former is diethylene triamine pentaacetate, the dewatering is to 30-45% dry matter, the amount of ozone employed is about 0.6% or less and the amount of peroxie employed is about 0.3% to 1% , both by weight based on the dry weight of the pulp.
Claim 6
Dependent Claim
25 words
The method of claim 2 wherein the pulp being bleached is a sulphite pulp and the acid is acid condensates from a sulphite digestion process.
Claim 7
Dependent Claim
61 words
The method of claim 5 wherein the alkaline is NaOH, the peroxide is hydrogen peroxide, the complex former is diethylene triamine pentaacetate, the dewatering is to 30-45% dry matter, the amount of ozone employed is about 0.6% or less and the amount of peroxide employed is about 0.3% to 1%, both by weight based on the dry weight of the pulp.
Claim 8
Dependent Claim
10 words
The method of claim 1 wherein the alkaline is NaOH.
Claim 9
Dependent Claim
11 words
The method of claim 1 wherein the peroxide is hydrogen peroxide.
Claim 10
Dependent Claim
27 words
The method of claim 8 wherein the total amount of peroxide employed is about 0.3% to 1%, by weight based on the dry weight of the pulp.
Claim 11
Dependent Claim
13 words
The method of claim 1 wherein the complex former is diethylene triamine pentaacetate.
Claim 12
Dependent Claim
13 words
The method of claim 1 wherein the dewatering is to 30-45% dry matter.
Claim 13
Dependent Claim
27 words
The method of claim 1 wherein the total amount of ozone employed is about 0.6% or less, by weight based on the dry weight of the pulp.
Claim 14
Dependent Claim
27 words
The method of claim 1 wherein the total amount of ozone employed is about 0.5% to 0.6%, by weight based on the dry weight of the pulp.
References Cited (Backward Citations)
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1987-05-22 | 1987-11-21 | 1988-05-22 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 1991-05-22 | 1991-11-21 | 1992-05-22 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 1995-05-22 | 1995-11-21 | 1996-05-22 | $7700.00 | Window Closed / Lapsed |