← Back to Patent Explorer
US4480928A Expired / Lapsed US ⏱️ 0.0 years remaining

Methods of flaw detection in billets

Assignee: Elkem ASA
•
Filing: 1982-10-28
•
Granted: 1984-11-06
•
Expires: 2002-10-28
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract Cracks and surface flaws in billets are detected by heating the surface of the work-piece by means of high frequency current, the heating taking place while the work-piece is brought to pass in its longitudinal direction through a high frequency induction coil. That part of the work-piece, which has just left the coil is immediately, while the work-piece is still passing through the coil, scanned by means of infrared recording equipment which records the temperature distribution across the work-piece. The emission coefficient for the different work-pieces is increased and differences equalized by moistening the surface of the work-piece with an appropriate liquid, for instance water, to which have been added components for reduction of the surface tension.

Inventors

  • 👤 Svein R. Halsor
  • 👤 Magnar K. Storset

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-26 00:11
CPC Classifications
G; G01; G01N; G01N25/00; G01N25/72

Claims Analysis

Total Claims: 7
Claim 1
Independent Claim 154 words
In the method of detecting flaws in the surface of metal workpieces which are heated by a high frequency current induction heater and scanned by infrared equipment to record the temperature disturbance across the surface of the workpiece and thereby indicate surface flaws by heat emitted from the surface, the improvement which comprises the steps of: (a) passing the metal workpiece in longitudinal direction through a high frequency induction heater; (b) immediately scanning the surface of the workpiece with infrared equipment to record the temperature distribution across the workpiece as it passes from said heater; and (c) prior to said immediate scanning, applying to the surface of the workpiece water having surface tension below that of ordinary water and of sufficiently low surface tension to wet and coat the surface of the workpiece to be inspected by scanning and thereby change the emission coefficient and compensate for differences in the characteristics of workpiece surfaces.
Claim 2
Dependent Claim 154 words
In the method of detecting flaws in the surface of metal workpieces which are heated by a high frequency current induction heater and scanned by infrared equipment to record the temperature disturbance across the surface of the workpiece and thereby indicate surface flaws by heat emitted from the surface, the improvement which comprises the steps of: (a) passing the metal workpiece in longitudinal direction through a high frequency induction heater; (b) immediately scanning the surface of the workpiece with infrared equipment to record the temperature distribution across the workpiece as it passes from said heater; and (c) prior to said immediate scanning, applying to the surface of the workpiece water having surface tension below that of ordinary water and of sufficiently low surface tension to wet and coat the surface of the workpiece to be inspected by scanning and thereby change the emission coefficient and compensate for differences in the characteristics of workpiece surfaces.
Claim 3
Dependent Claim 20 words
The method of claim 1 in which said water has a freezing point below the freezing point of ordinary water.
Claim 4
Dependent Claim 159 words
In the method of detecting flaws in the surface of metal billets which are heated by high frequency induction heating and scanned by infrared equipment to record the temperature disturbance across the surface of the billet and thereby indicate surface flaws by heat emitted from the surface, the improvement which comprises the steps of: (a) passing the metal billet in longitudinal direction through a high frequency induction coil; (b) immediately scanning the surface of the billet with infrared equipment to record the temperature distribution across the surface of the billet as it passes from said coil; and (c) prior to said immediate scanning, coating the surface of billet with a liquid selected to have surface tension characteristics below that of ordinary water necessary to wet the surface of the metal billet to be inspected by scanning and thereby change the emission coefficient of the surface of the metal billet and compensate for differences in the characteristics of billet surfaces.
Claim 5
Dependent Claim 159 words
In the method of detecting flaws in the surface of metal billets which are heated by high frequency induction heating and scanned by infrared equipment to record the temperature disturbance across the surface of the billet and thereby indicate surface flaws by heat emitted from the surface, the improvement which comprises the steps of: (a) passing the metal billet in longitudinal direction through a high frequency induction coil; (b) immediately scanning the surface of the billet with infrared equipment to record the temperature distribution across the surface of the billet as it passes from said coil; and (c) prior to said immediate scanning, coating the surface of billet with a liquid selected to have surface tension characteristics below that of ordinary water necessary to wet the surface of the metal billet to be inspected by scanning and thereby change the emission coefficient of the surface of the metal billet and compensate for differences in the characteristics of billet surfaces.
Claim 6
Dependent Claim 23 words
The method of claim 3 in which the metal billet is pretreated to brighten the surface prior to said high frequency induction heating.
Claim 7
Dependent Claim 24 words
The method of claim 3 which includes the step of shot blasting the surface of the billet prior to said high frequency induction heating.

References Cited (Backward Citations)

US3020745A Cited
US3378685A Cited
US3945245A Cited
US4109508A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1987-11-06 1988-05-07 1988-11-06 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1991-11-06 1992-05-07 1992-11-06 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1995-11-06 1996-05-07 1996-11-06 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag