← Back to Patent Explorer
US4500621A Expired / Lapsed US ⏱️ 0.0 years remaining

Sensitive electrophotographic plates containing squaric acid methine dyes suspended in a binder

Assignee: Ricoh Co Ltd
•
Filing: 1983-04-11
•
Granted: 1985-02-19
•
Expires: 2003-04-11
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract Electrographic imaging process and electrographic plates utilized therein are provided wherein the photoconductive layer comprises a squaric acid methine dye admixed with a binder or a photoconductive material. The photoconductive layer may also comprise the squaric acid methine dye, a binder and a charge transport material.

Inventors

  • 👤 Herbert K. Wurster

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-04 23:10
CPC Classifications
G; G03; G03G; G03G5/00; G03G5/02; G03G5/04; G03G5/06; G03G5/0601; G03G5/0605; G03G5/0607; C; C09; C09B; C09B23/00; C09B23/0066; G03G5/0609; G03G5/0611; G03G5/0622; G03G5/0624; G03G5/0627; G03G5/0629; G03G5/0631; G03G5/0644; G03G5/0646; G03G5/065

Claims Analysis

Total Claims: 10
Claim 1
Independent Claim 221 words
A single layer photoreceptor plate comprising a solid continuous photoconductor layer of uniform thickness in the range of 1-60 microns consisting essentially of a noncharge-transporting binder material and a charge-generating, charge-transporting squaric acid methine dye selected from the group consisting of compounds of the Formula I: ##STR8## wherein A and B are independently, ##STR9## ##STR10## ##STR11## wherein R 1 , R 2 , R 3 are independently H, OH or alkyl of 1 to 6 carbon atoms, NR 4 R 5 , wherein R 4 and R 5 are independnetly alkyl of 1 to 6 carbon atoms; ##STR12## R 6 and R 7 are independently alkyl of 1 to 6 carbon atoms; and R 8 is independently H, OR 9 or halogen, wherein R 9 is alkyl of 1 to 6 carbon atoms; ##STR13## wherein R 10 , R 11 , R 12 and R 13 are independently H, OH or alkyl of 1 to 6 carbon atoms; ##STR14## wherein R 14 , R 15 and R 16 are independently alkyl of 1 to 6 carbon atoms; and R 17 is independently H, OR 18 or halogen, wherein R 18 is alkyl of 1 to 6 carbon atoms; or ##STR15## wherein the proportion of said dye to said binder material in said photoconductor is in the range of 1:1 to 1:40.
Claim 2
Dependent Claim 221 words
A single layer photoreceptor plate comprising a solid continuous photoconductor layer of uniform thickness in the range of 1-60 microns consisting essentially of a noncharge-transporting binder material and a charge-generating, charge-transporting squaric acid methine dye selected from the group consisting of compounds of the Formula I: ##STR8## wherein A and B are independently, ##STR9## ##STR10## ##STR11## wherein R 1 , R 2 , R 3 are independently H, OH or alkyl of 1 to 6 carbon atoms, NR 4 R 5 , wherein R 4 and R 5 are independnetly alkyl of 1 to 6 carbon atoms; ##STR12## R 6 and R 7 are independently alkyl of 1 to 6 carbon atoms; and R 8 is independently H, OR 9 or halogen, wherein R 9 is alkyl of 1 to 6 carbon atoms; ##STR13## wherein R 10 , R 11 , R 12 and R 13 are independently H, OH or alkyl of 1 to 6 carbon atoms; ##STR14## wherein R 14 , R 15 and R 16 are independently alkyl of 1 to 6 carbon atoms; and R 17 is independently H, OR 18 or halogen, wherein R 18 is alkyl of 1 to 6 carbon atoms; or ##STR15## wherein the proportion of said dye to said binder material in said photoconductor is in the range of 1:1 to 1:40.
Claim 3
Dependent Claim 14 words
A photoreceptor plate according to claim 1 wherein A and B are independently ##STR16##
Claim 4
Dependent Claim 28 words
A photoreceptor plate according to claim 2 wherein R 1 is methyl, R 2 is hydrogen, R 3 is dimethyl- amino and A and B are the same.
Claim 5
Dependent Claim 24 words
A photoreceptor plate according to claim 1 wherein said binder is selected from the group consisting of polycarbonate resin, epoxy resins, and acrylic polymers.
Claim 6
Dependent Claim 240 words
An electrophotographic imaging process comprising the steps of subjecting a solid continuous photoconductor layer of a uniform thickness in the range of 1-60 microns, consisting essentially of a noncharge-transporting binder material and a charge-generating, charge-transporting squaric acid methine dye selected from the group consisting of compounds of the Formula I: ##STR17## wherein A and B are independently ##STR18## wherein R 1 , R 2 , R 3 are independently H, OH or alkyl of 1 to 6 carbon atoms, NR 4 R 5 , wherein R 4 and R 5 are independently alkyl of 1 to 6 carbon atoms; ##STR19## ##STR20## ##STR21## R 6 and R 7 independently alkyl of 1 to 6 carbon atoms; and R 8 is independently H, OR9 or halogen and wherein R 9 is alkyl of 1 to 6 carbon atoms; ##STR22## wherein R 10 , R 11 , R 12 and R 13 are independently H, OH or alkyl of 1 to 6 carbon atoms; ##STR23## wherein R 14 , R 15 and R 16 are independently alkyl of 1 to 6 carbon atoms and R 17 is independently OH, OR 18 or halogen, wherein R 18 is alkyl of 1 to 6 carbon atoms; or ##STR24## wherein the proportion of said dye to said binder material in said photoconductor is in the range of 1:1 to 1:40; and exposing said layer to an image pattern of radiation to which said layer is photosensitive.
Claim 7
Dependent Claim 240 words
An electrophotographic imaging process comprising the steps of subjecting a solid continuous photoconductor layer of a uniform thickness in the range of 1-60 microns, consisting essentially of a noncharge-transporting binder material and a charge-generating, charge-transporting squaric acid methine dye selected from the group consisting of compounds of the Formula I: ##STR17## wherein A and B are independently ##STR18## wherein R 1 , R 2 , R 3 are independently H, OH or alkyl of 1 to 6 carbon atoms, NR 4 R 5 , wherein R 4 and R 5 are independently alkyl of 1 to 6 carbon atoms; ##STR19## ##STR20## ##STR21## R 6 and R 7 independently alkyl of 1 to 6 carbon atoms; and R 8 is independently H, OR9 or halogen and wherein R 9 is alkyl of 1 to 6 carbon atoms; ##STR22## wherein R 10 , R 11 , R 12 and R 13 are independently H, OH or alkyl of 1 to 6 carbon atoms; ##STR23## wherein R 14 , R 15 and R 16 are independently alkyl of 1 to 6 carbon atoms and R 17 is independently OH, OR 18 or halogen, wherein R 18 is alkyl of 1 to 6 carbon atoms; or ##STR24## wherein the proportion of said dye to said binder material in said photoconductor is in the range of 1:1 to 1:40; and exposing said layer to an image pattern of radiation to which said layer is photosensitive.
Claim 8
Dependent Claim 13 words
A process according to claim 5 wherein A and B are independently. ##STR25##
Claim 9
Dependent Claim 26 words
A process according to claim 6 wherein R 1 is methyl, R 2 is hydrogen, R 3 is dimethylamino and A and B are the same.
Claim 10
Dependent Claim 23 words
A process according to claim 5 wherein said binder is selected from the group consisting of polycarbonate resin, epoxy resins, and acrylic polymers.

References Cited (Backward Citations)

US3140182A Cited
US3816118A Cited
US3617270A Cited
GB1343671A Cited
DE2314867A1 Cited
US3824099A Cited
US4123269A Cited
US4175956A Cited
US4353971A Cited
JPS57144558A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1988-02-19 1988-08-20 1989-02-19 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1992-02-19 1992-08-20 1993-02-19 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1996-02-19 1996-08-20 1997-02-19 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag