Abstract

Abstract A method of welding two HY-steel members to produce a weld joint having improved impact toughness. The surface to be welded are first machined, roto-blasted and cleaned with acetone. Then, an insert of Inconel 600 is provided and cleaned with acetone. Next, the Inconel 600 insert is introduced between the surfaces to be welded and the HY-steel members are butted against the insert. Then, a laser welding beam is applied to the Inconel 600 insert to weld together the assembly of steel members and insert.

Inventors

  • 👤 Deug W. Moon
  • 👤 Edward A. Metzbower

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-08 07:08
CPC Classifications
B; B23; B23K; B23K35/00; B23K35/22; B23K35/24; B23K35/30; B23K35/3033; B23K35/304; B23K26/00; B23K26/20; B23K26/32; B23K2103/00; B23K2103/02; B23K2103/04; B23K2103/50

Claims Analysis

Total Claims: 19
Claim 1
Independent Claim 90 words
A method of welding two structural steel members to produce a weld joint having improved impact toughness comprising the step of: (a) introducing an inoculant comprising an insert of Inconel 600 in the range of 0.005 inch in thickness between the surfaces of the two steel members to be welded ranging in composition from HY-80 to HY-100 steel; (b) butting the surfaces to be welded of the two members against the inoculant; and (c) applying a laser beam to the inoculant to weld together the assembly of members and inoculant.
Claim 2
Independent Claim 90 words
A method of welding two structural steel members to produce a weld joint having improved impact toughness comprising the step of: (a) introducing an inoculant comprising an insert of Inconel 600 in the range of 0.005 inch in thickness between the surfaces of the two steel members to be welded ranging in composition from HY-80 to HY-100 steel; (b) butting the surfaces to be welded of the two members against the inoculant; and (c) applying a laser beam to the inoculant to weld together the assembly of members and inoculant.
Claim 3
Independent Claim 96 words
A method of welding two steel members to produce a weld joint having improved impact toughness comprising the steps of: (a) roto-blasting the surfaces to be welded of the two steel members; (b) cleaning the surfaces to be welded of the two steel members; (c) introducing an inoculant comprising an insert of Inconel 600 between the surfaces to be welded of the two members; (d) butting the surfaces to be welded of the two members against the inoculant; and (e) applying a laser beam to the inoculant to weld together the assembly of members and inoculant.
Claim 4
Independent Claim 96 words
A method of welding two steel members to produce a weld joint having improved impact toughness comprising the steps of: (a) roto-blasting the surfaces to be welded of the two steel members; (b) cleaning the surfaces to be welded of the two steel members; (c) introducing an inoculant comprising an insert of Inconel 600 between the surfaces to be welded of the two members; (d) butting the surfaces to be welded of the two members against the inoculant; and (e) applying a laser beam to the inoculant to weld together the assembly of members and inoculant.
Claim 5
Dependent Claim 26 words
The method recited in claim 2 including the step of: machining the surfaces to be welded of the two steel members prior to the roto-blasting step.
Claim 6
Dependent Claim 30 words
The method recited in claim 3 including the step of: cleaning the insert prior to the step of introducing it between the surfaces to be welded of the two members.
Claim 7
Dependent Claim 11 words
The welded assembly produced by the method recited in claim 1.
Claim 8
Independent Claim 121 words
A method of welding two steel members to produce a weld joint having improved impact toughness, comprising the steps of: (a) machining the surfaces to be welded of the two steel members; (b) roto-blasting the surfaces to be welded of the two steel members; (c) cleaning the surfaces to be welded of the two steel members; (d) providing an insert of Inconel 600; (e) cleaning the Inconel 600 insert; (f) introducing the Inconel 600 insert between the surfaces to be welded of the two steel members; (g) butting the surfaces to be welded of the two steel members against the insert; and (h) applying a laser welding beam to the insert to weld together the assembly of steel members and insert.
Claim 9
Independent Claim 121 words
A method of welding two steel members to produce a weld joint having improved impact toughness, comprising the steps of: (a) machining the surfaces to be welded of the two steel members; (b) roto-blasting the surfaces to be welded of the two steel members; (c) cleaning the surfaces to be welded of the two steel members; (d) providing an insert of Inconel 600; (e) cleaning the Inconel 600 insert; (f) introducing the Inconel 600 insert between the surfaces to be welded of the two steel members; (g) butting the surfaces to be welded of the two steel members against the insert; and (h) applying a laser welding beam to the insert to weld together the assembly of steel members and insert.
Claim 10
Dependent Claim 15 words
The method recited in claim 6 wherein: step (b) is accomplished with a carbon-dioxide laser.
Claim 11
Dependent Claim 19 words
The method recited in claim 7 wherein step (h) includes the step of: protecting the weld with helium gas.
Claim 12
Dependent Claim 12 words
The method recited in claim 8 wherein: the steel is HY-80 steel.
Claim 13
Dependent Claim 12 words
The method recited in claim 8 wherein: the steel is HY-100 steel.
Claim 14
Dependent Claim 11 words
The welded assembly produced by the method recited in claim 4.
Claim 15
Independent Claim 141 words
A method of welding two HY- steel members to produce a weld joint having improved impact toughness, comprising the steps of: (a) machining the surfaces to be welded of the two HY- steel members; (b) roto-blasting the surfaces to be welded of the two HY- steel members; (c) cleaning the surfaces to be welded of the two HY- steel members; (d) providing an insert of Inconel 600; (e) cleaning the Inconel 600 insert; (f) introducing the Inconel 600 insert between the surfaces to be welded of the two HY- steel members; (g) butting the surfaces to be welded of the two HY- steel members against the insert; and (h) applying a continuous wave, carbon-dioxide laser welding beam to the insert to weld together the assembly of HY- steel members and insert; wherein step (h) includes protecting the weld with helium gas.
Claim 16
Independent Claim 141 words
A method of welding two HY- steel members to produce a weld joint having improved impact toughness, comprising the steps of: (a) machining the surfaces to be welded of the two HY- steel members; (b) roto-blasting the surfaces to be welded of the two HY- steel members; (c) cleaning the surfaces to be welded of the two HY- steel members; (d) providing an insert of Inconel 600; (e) cleaning the Inconel 600 insert; (f) introducing the Inconel 600 insert between the surfaces to be welded of the two HY- steel members; (g) butting the surfaces to be welded of the two HY- steel members against the insert; and (h) applying a continuous wave, carbon-dioxide laser welding beam to the insert to weld together the assembly of HY- steel members and insert; wherein step (h) includes protecting the weld with helium gas.
Claim 17
Dependent Claim 19 words
The method recited in claim 12 wherein: the surfaces to be welded are cleaned with acetone in step (c).
Claim 18
Dependent Claim 18 words
The method recited in claim 13 wherein: the Inconel 600 insert is cleaned with acetone in step (e).
Claim 19
Dependent Claim 11 words
The welded assembly produced by the method recited in claim 12.

References Cited (Backward Citations)

US3303319A Cited
US3463898A Cited
US3560700A Cited
US3585350A Cited
US3808395A Cited
US3975612A Cited
US3949186A Cited
US4001543A Cited
US4063062A Cited
US4152573A Cited
US4080525A Cited
US4219720A Cited
US4341942A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1988-07-01 1988-12-31 1989-07-02 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1992-07-01 1992-12-31 1993-07-02 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1996-07-01 1996-12-31 1997-07-02 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag