Boiler tubes of enhanced efficiency and method of producing same

Assignee: Individual
•
Filing: 1985-11-29
•
Granted: 1987-02-24
•
Expires: 2005-11-29
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract A composite boiler tube has a fireside surface and a water-side surface and comprises a metallic tubular member having an outer surface and an inner surface. One of the metallic surfaces has an efficiency enhancing coating adhered thereto and providing the composite tube with the fireside surface or the waterside surface. A method of enhancing the efficiency of a boiler tube which comprises a metallic tubular member having an outer surface and an inner surface includes the step of applying a coating of efficiency enhancing material adhered to one of the metallic tube member surfaces, thus to produce a composite boiler tube.

Inventors

  • 👤 Edward H. Hunter

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-27 22:39
CPC Classifications
F; F22; F22B; F22B37/00; F22B37/02; F22B37/04; F16; F16L; F16L58/00; F16L58/02; F16L58/04; F16L58/10; F16L58/1009; F16L58/1054; F22B37/10; Y; Y10; Y10S; Y10S122/00; Y10S122/13

Claims Analysis

Total Claims: 10
Claim 1
Independent Claim 87 words
A composite boiler tube having a fireside surface and a waterside surface and comprising a metallic tubular member having an outer surface and an inner surface, at least one of said metallic surfaces having an efficiency enhancing coating adhered thereto and providing said composite tube with one of said fireside surface and said waterside surface, wherein the material of said coating is dichlorodimethylsilane or its fluorocarbon composition version and wherein the radial thickness of said coating is on the order of 1×10 -6 inch (2.54×10 -6 cm).
Claim 2
Dependent Claim 87 words
A composite boiler tube having a fireside surface and a waterside surface and comprising a metallic tubular member having an outer surface and an inner surface, at least one of said metallic surfaces having an efficiency enhancing coating adhered thereto and providing said composite tube with one of said fireside surface and said waterside surface, wherein the material of said coating is dichlorodimethylsilane or its fluorocarbon composition version and wherein the radial thickness of said coating is on the order of 1×10 -6 inch (2.54×10 -6 cm).
Claim 3
Dependent Claim 17 words
A composite tube according to claim 1 wherein said one said metallic surface is said outer surface.
Claim 4
Dependent Claim 17 words
A composite tube according to claim 1 wherein said one said metallic surface is said inner surface.
Claim 5
Dependent Claim 31 words
A composite tube according to claim 1 wherein each said metallic surface has a said efficiency enhancing coating adhered thereto, said coatings providing both said fireside surface and said waterside surface.
Claim 6
Dependent Claim 23 words
A composite tube according to claim 1 wherein said one metallic surface is said outer surface and said coating provides said fireside surface.
Claim 7
Dependent Claim 12 words
A composite tube according to claim 5 wherein said coating is transparent.
Claim 8
Independent Claim 83 words
A method of enhancing the efficiency of a boiler tube comprising a metallic tubular member having an outer surface and an inner surface, said method including the step of applying by vaporization a coating of efficiency enhancing material adhered to one of said surfaces, thus to produce a composite boiler tube, wherein the material of said coating is dichlorodimethylsilane or its fluorocarbon composition version and said coating is applied to a radial thickness on the order of 1×10 -6 inch (2.54×10 -6 cm).
Claim 9
Independent Claim 83 words
A method of enhancing the efficiency of a boiler tube comprising a metallic tubular member having an outer surface and an inner surface, said method including the step of applying by vaporization a coating of efficiency enhancing material adhered to one of said surfaces, thus to produce a composite boiler tube, wherein the material of said coating is dichlorodimethylsilane or its fluorocarbon composition version and said coating is applied to a radial thickness on the order of 1×10 -6 inch (2.54×10 -6 cm).
Claim 10
Dependent Claim 26 words
A method according to claim 7 including the further step of applying a said coating of efficiency enhancing material adhered to the other of said surfaces.

References Cited (Backward Citations)

US3825064A Cited
US4116016A Cited
JPS5423801A Cited
US4427034A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1990-02-23 1990-08-25 1991-02-24 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1994-02-23 1994-08-25 1995-02-24 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1998-02-23 1998-08-25 1999-02-24 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag