US4915971A
Expired / Lapsed
US
⏱️ 0.0 years remaining
Method for making an edible film and for retarding water transfer among multi-component food products
Assignee: Wisconsin Alumni Research Foundation
•
Filing: 1987-08-04
•
Granted: 1990-04-10
•
Expires: 2007-08-04
Abstract
Abstract An edible film for retarding water transfer among components of a multicomponent food product. The film includes a base film having a hydrophilic polymer layer and a base film lipid layer. The base film lipid layer has a hydrophobic surface presented away from the hydrophilic polymer layer. An additional lipid layer is laminated to the hydrophobic surface of the base film lipid layer. The invention further includes a method for making the edible film and a food product incorporating it.
Inventors
- 👤 Owen R. Fennema
- 👤 Susan L. Kamper
- 👤 Jeffrey J. Kester
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-10-31 07:05
CPC Classifications
A; A23; A23P; A23P20/00; A23P20/20; A21; A21D; A21D13/00; A21D13/20; A21D13/26; A21D13/40; A21D13/41; A23B; A23B4/00; A23B4/10; A23G; A23G3/00; A23G3/34; A23G3/343; A23P20/10; A23P20/105; A23G2200/00
Claims Analysis
Total Claims: 8
Claim 1
Independent Claim
286 words
A method for making an edible film and for retarding water transfer among components of a multi-component food product, the method comprising the steps of: (a) preparing a film-forming liquid by mixing an edible hydrophilic polymer that displays gelation and an edible lipid which is added in an amount sufficient to allow substantially complete coverage of the surface of the hydrophilic polymer when said film-forming liquid is dried by heat, said mixing of said polymer and said lipid occurring in an aqueous solvent system containing an alcohol; (b) plating the film-forming liquid on a non-food supporting surface to a depth such that upon drying of said film-forming liquid, a film of desired thickness is obtained, and drying the film-forming liquid on said surface to form a cohesive film such that the depth of the film-forming liquid selected is sufficient to contain enough polymer and lipid to result in a dried barrier film of said desired film thickness and such that the film comprises a hydrophilic polymer layer adjacent to the supporting surface and a hydrophobic lipid layer presented away from the supporting surface, the lipid layer having a concentration of at least approximately 0.8 milligrams lipid per square centimeter of hydrophilic polymer layer; (c) removing the film from the supporting surface; and (d) placing the film between food components that have different vapor pressures relative to each other such that said hydrophobic lipid layer is oriented toward the food components having the higher vapor pressure such that moisture transfer from the food components having a higher vapor pressure to food components having a lower vapor pressure is effectively retarded during an extended period of storage and upon heating will be consumable with the separated food components.
Claim 2
Independent Claim
286 words
A method for making an edible film and for retarding water transfer among components of a multi-component food product, the method comprising the steps of: (a) preparing a film-forming liquid by mixing an edible hydrophilic polymer that displays gelation and an edible lipid which is added in an amount sufficient to allow substantially complete coverage of the surface of the hydrophilic polymer when said film-forming liquid is dried by heat, said mixing of said polymer and said lipid occurring in an aqueous solvent system containing an alcohol; (b) plating the film-forming liquid on a non-food supporting surface to a depth such that upon drying of said film-forming liquid, a film of desired thickness is obtained, and drying the film-forming liquid on said surface to form a cohesive film such that the depth of the film-forming liquid selected is sufficient to contain enough polymer and lipid to result in a dried barrier film of said desired film thickness and such that the film comprises a hydrophilic polymer layer adjacent to the supporting surface and a hydrophobic lipid layer presented away from the supporting surface, the lipid layer having a concentration of at least approximately 0.8 milligrams lipid per square centimeter of hydrophilic polymer layer; (c) removing the film from the supporting surface; and (d) placing the film between food components that have different vapor pressures relative to each other such that said hydrophobic lipid layer is oriented toward the food components having the higher vapor pressure such that moisture transfer from the food components having a higher vapor pressure to food components having a lower vapor pressure is effectively retarded during an extended period of storage and upon heating will be consumable with the separated food components.
Claim 3
Dependent Claim
14 words
The method of claim 1 wherein the hydrophilic polymer is a water-soluble, film-forming carbohydrate.
Claim 4
Dependent Claim
32 words
The method of claim 1 wherein the aqueous solvent system includes water and alcohol and the lipid is selected from the group consisting of hydrogenated oils, saturated fatty acids and edible waxes.
Claim 5
Dependent Claim
21 words
The method of claim 1 wherein the step of preparing the film-forming liquid includes dissolving polyethylene glycol in the solvent system.
Claim 6
Dependent Claim
21 words
The method of claim 1 wherein the hydrophilic polymer is selected from the group consisting of starch, cellulose ethers and albumen.
Claim 7
Independent Claim
323 words
A method for making an edible film and for retarding water transfer among components of a multi-component food product, the method comprising the steps of: (a) preparing a film-forming liquid by mixing an edible hydrophilic polymer that displays gelation, the hydrophilic polymer being selected from the group consisting of starch, cellulose ethers, and albumen and an edible lipid which is added in an amount sufficient to allow substantially complete coverage of the surface of the hydrophilic polymer when said film forming liquid is dried by heat, the lipid being selected from the group consisting of hydrogenated oils, saturated fatty acids and edible waxes, said mixing of said polymer and said lipid occurring in an aqueous solvent system including water, alcohol and polyethylene glycol; (b) plating the film-forming liquid on a non-food supporting surface to a selected depth such that upon drying of said film-forming liquid, a film of desired thickness is obtained, and drying the film forming liquid on said surface to form a cohesive film such that the depth of the film-forming liquid selected is sufficient to contain enough polymer and lipid to result in a dried barrier film of said desired film thickness, and such that the film comprises a hydrophilic polymer layer adjacent to the supporting surface and a hydrophobic lipid layer presented away from the supporting surface, the lipid layer having a concentration of at least approximately 0.8 milligrams lipid per square centimeter of hydrophilic polymer layer; (c) removing the film from the supporting surface; and (d) placing the film between food components that have different vapor pressures relative to each other such that said hydrophobic lipid layer is oriented toward the food components having the higher vapor pressure such that moisture transfer from the food components having the higher vapor pressure to food components having a lower vapor pressure is retarded during an extended period of storage and upon heating will be consumable with the separated food components.
Claim 8
Independent Claim
323 words
A method for making an edible film and for retarding water transfer among components of a multi-component food product, the method comprising the steps of: (a) preparing a film-forming liquid by mixing an edible hydrophilic polymer that displays gelation, the hydrophilic polymer being selected from the group consisting of starch, cellulose ethers, and albumen and an edible lipid which is added in an amount sufficient to allow substantially complete coverage of the surface of the hydrophilic polymer when said film forming liquid is dried by heat, the lipid being selected from the group consisting of hydrogenated oils, saturated fatty acids and edible waxes, said mixing of said polymer and said lipid occurring in an aqueous solvent system including water, alcohol and polyethylene glycol; (b) plating the film-forming liquid on a non-food supporting surface to a selected depth such that upon drying of said film-forming liquid, a film of desired thickness is obtained, and drying the film forming liquid on said surface to form a cohesive film such that the depth of the film-forming liquid selected is sufficient to contain enough polymer and lipid to result in a dried barrier film of said desired film thickness, and such that the film comprises a hydrophilic polymer layer adjacent to the supporting surface and a hydrophobic lipid layer presented away from the supporting surface, the lipid layer having a concentration of at least approximately 0.8 milligrams lipid per square centimeter of hydrophilic polymer layer; (c) removing the film from the supporting surface; and (d) placing the film between food components that have different vapor pressures relative to each other such that said hydrophobic lipid layer is oriented toward the food components having the higher vapor pressure such that moisture transfer from the food components having the higher vapor pressure to food components having a lower vapor pressure is retarded during an extended period of storage and upon heating will be consumable with the separated food components.
References Cited (Backward Citations)
US2721142A
Cited
US2836498A
Cited
US2909435A
Cited
US3031309A
Cited
US3323922A
Cited
US3471304A
Cited
US3471303A
Cited
US3667963A
Cited
FR2087185A5
Cited
US3778515A
Cited
US3830944A
Cited
JPS5191359A
Cited
US3997674A
Cited
US4416910A
Cited
JPS5212943A
Cited
US4066796A
Cited
JPS5315100A
Cited
JPS5334939A
Cited
US4293572A
Cited
US4515819A
Cited
US4416904A
Cited
GB2105168A
Cited
US4401681A
Cited
US4661359A
Cited
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1993-04-09 | 1993-10-09 | 1994-04-10 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 1997-04-09 | 1997-10-09 | 1998-04-10 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 2001-04-09 | 2001-10-09 | 2002-04-10 | $7700.00 | Window Closed / Lapsed |