Bump structure for reflow bonding of IC devices

Assignee: National Semiconductor Corp
•
Filing: 1989-02-09
•
Granted: 1990-05-01
•
Expires: 2009-02-09
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract In a semiconductor device tape assembly bonding process the fingers of a copper tape are reflow soldered to metal bumps located on the semiconductor device. First, the semiconductor wafer is covered with a conductive film composed of thin layers of alumimum, nickel-vanadium alloy and gold. The bumps are then created by electroplating gold through openings in a photoresist mask. The gold bumps are overcoated with a controlled thickness tin layer and the tin is overcoated with a thin gold anticorrosion layer. The copper assembly tape is coated with a thin gold layer and are lightly pressed against the bumps by means of a thermode. The thermode is quickly heated to a temperature well above the gold-tin eutectic melting temperature and then rapidly cooled. The tin layer on the bump will combine with the adjacent gold to form a liquid phase eutetic which will form and contact both the copper finger and the gold bump. Upon cooling the eutectic melt will solder the finger to the bump. Since all of the tin is combined with the gold there is no metallic tin left in the system and the problems of tin whiskers and tin electromigration are avoided.

Inventors

  • 👤 Ranjan J. Mathew

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-31 16:44
CPC Classifications
H; H10; H10D; H10D84/00; H10W; H10W72/00; H10W72/20; H10W72/01; H10W72/012; H10W72/01251; H10W72/01255; H10W72/251; H10W72/90; H10W72/921; H10W72/923; H10W72/951; H10W72/952

Claims Analysis

Total Claims: 2
Claim 1
Independent Claim 90 words
A tape assembly bonded semiconductor device comprising: a semiconductor device having at least one aluminum bonding pad; layers of aluminum, nickel-vanadium alloy and gold successively overlying said aluminum bonding pad; a gold bump located on said semiconductor device over said gold layer, said gold bump having an outer surface; a copper tape finger associated with an assembly tape; and a gold-tin eutectic solder joining said copper tape finger to said outer surface of said gold bump wherein there is a complete absence of metallic tin in said bonded semiconductor device.
Claim 2
Dependent Claim 90 words
A tape assembly bonded semiconductor device comprising: a semiconductor device having at least one aluminum bonding pad; layers of aluminum, nickel-vanadium alloy and gold successively overlying said aluminum bonding pad; a gold bump located on said semiconductor device over said gold layer, said gold bump having an outer surface; a copper tape finger associated with an assembly tape; and a gold-tin eutectic solder joining said copper tape finger to said outer surface of said gold bump wherein there is a complete absence of metallic tin in said bonded semiconductor device.

References Cited (Backward Citations)

US3141226A Cited
US4244002A Cited
US4418857A Cited
US4494688A Cited
JPS57188848A Cited
US4502210A Cited
US4518112A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1993-04-30 1993-10-30 1994-05-01 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1997-04-30 1997-10-30 1998-05-01 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 2001-04-30 2001-10-30 2002-05-01 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag