Abstract
Abstract Mixtures which can be cross-linked by photopolymerization and are based on soluble elastomeric block copolymers, photopolymerizable monomers which are compatible with these, photoinitiators and plasticizers contain, as the plasticizer, a chloroalkane of 8 to 40 carbon atoms which has a chlorine content of from 30 to 73% by weight.
Inventors
- 👤 Gerhard Hoffmann
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-11-06 19:19
CPC Classifications
G; G03; G03F; G03F7/00; G03F7/004; G03F7/027; Y; Y10; Y10S; Y10S430/00; Y10S430/1053; Y10S430/1055; Y10S430/106; Y10S430/108; Y10S430/113
Claims Analysis
Total Claims: 6
Claim 1
Independent Claim
214 words
In a process for improving the ozone resistance of the surface of flexographic relief printing plates, wherein the reliefs are prepared by imagewise exposure with actinic radiation and by liquid solvent washout development of the unexposed areas of a layer of a photopolymerizable elastomeric composition, the improvement which comprises: imagewise exposing to actinic radiation a photopolymerizable elastomeric composition consisting essentially of (a) from 58 to 92% by weight, based on the sum of all the components of the photopolymerizable elastomeric composition, of a solvent soluble elastomeric diene block copolymer containing at least one vinylaromatic and at least one diene polymer block, (b) from 2 to 16% by weight, based on the sum of elastomeric composition, of one or more photopolymerizable, ethylenically unsaturated monomers being compatible with the elastomeric diene block copolymer (a), (c) from 0.4 to 6% by weight, based on the sum of all the components of the photopolymerizable elastomeric composition, of one or more photoinitiators, and (d) from 3 to 22% by weight, based on the sum of all of the components of the photopolymerizable elastomeric composition, of a chloroalkane of 8 to 40 carbons which has a chlorine content of about 49% by weight and then developing the unexposed areas to obtain a flexographic relief printing plate having improved ozone resistance.
Claim 2
Dependent Claim
214 words
In a process for improving the ozone resistance of the surface of flexographic relief printing plates, wherein the reliefs are prepared by imagewise exposure with actinic radiation and by liquid solvent washout development of the unexposed areas of a layer of a photopolymerizable elastomeric composition, the improvement which comprises: imagewise exposing to actinic radiation a photopolymerizable elastomeric composition consisting essentially of (a) from 58 to 92% by weight, based on the sum of all the components of the photopolymerizable elastomeric composition, of a solvent soluble elastomeric diene block copolymer containing at least one vinylaromatic and at least one diene polymer block, (b) from 2 to 16% by weight, based on the sum of elastomeric composition, of one or more photopolymerizable, ethylenically unsaturated monomers being compatible with the elastomeric diene block copolymer (a), (c) from 0.4 to 6% by weight, based on the sum of all the components of the photopolymerizable elastomeric composition, of one or more photoinitiators, and (d) from 3 to 22% by weight, based on the sum of all of the components of the photopolymerizable elastomeric composition, of a chloroalkane of 8 to 40 carbons which has a chlorine content of about 49% by weight and then developing the unexposed areas to obtain a flexographic relief printing plate having improved ozone resistance.
Claim 3
Dependent Claim
42 words
The process of claim 1, wherein the mixture contains from 68 to 82% by weight of (a), from 5 to 12% by weight of (b), from 1.2 to 2.5% by weight of (c) and from 8 to 18% by weight of (d).
Claim 4
Dependent Claim
17 words
The process of claim 1, wherein said elastomeric diene block copolymer is prepared by sequential anionic polymerization.
Claim 5
Dependent Claim
16 words
The process of claim 1, wherein the chloroalkane has a density of 1.24 g/cm 3 .
Claim 6
Dependent Claim
11 words
The process of claim 4, wherein the chloroalkane is an oil.
References Cited (Backward Citations)
GB1095518A
Cited
GB1366769A
Cited
US4369246A
Cited
US3897255A
Cited
US4001174A
Cited
US4045231A
Cited
US4201642A
Cited
US4339527A
Cited
US4400460A
Cited
US4452879A
Cited
US4636453A
Cited
EP0217324A2
Cited
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1993-05-14 | 1993-11-13 | 1994-05-15 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 1997-05-14 | 1997-11-13 | 1998-05-15 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 2001-05-14 | 2001-11-13 | 2002-05-15 | $7700.00 | Window Closed / Lapsed |