Method for maintaining the electrochromic activity of an electrochromic material
Assignee: Ford Motor Co
•
Filing: 1988-10-05
•
Granted: 1990-10-02
•
Expires: 2008-10-05
Abstract
Abstract This specification teaches a method for maintaining the electrochromic activity of an electrochromic material positioned between electrodes of an electrochromic device. The method disclosed for maintaining the electrochromic activity of the electrochromic material comprises applying a voltage across the electrodes of such level so to maintain an absolute single polarity charge abundance in the electrochromic material sufficient to keep it in an electrochromic state.
Inventors
- 👤 Hulya Demiryont
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-11-04 17:56
CPC Classifications
G; G02; G02F; G02F1/00; G02F1/01; G02F1/15; G02F1/163; G02F1/1514; G02F1/1523; G02F1/1524
Claims Analysis
Total Claims: 11
Claim 1
Independent Claim
95 words
A method of maintaining the electrochromic activity of a cathodic electrochromic material having a non-stoichiometric composition provided between electrodes of an electrochromic device, which method comprises: applying a voltage, at least during operation of said device, across said electrodes of such level that the absolute value of an applied negative voltage is greater than the absolute value of an applied positive voltage, so as to continuously maintain a negative charge abundance in said electrochromic material sufficient to keep said electrochromic material in a non-stoichiometric state and whereby oxidation of said electrochromic material is substantially prevented.
Claim 2
Independent Claim
95 words
A method of maintaining the electrochromic activity of a cathodic electrochromic material having a non-stoichiometric composition provided between electrodes of an electrochromic device, which method comprises: applying a voltage, at least during operation of said device, across said electrodes of such level that the absolute value of an applied negative voltage is greater than the absolute value of an applied positive voltage, so as to continuously maintain a negative charge abundance in said electrochromic material sufficient to keep said electrochromic material in a non-stoichiometric state and whereby oxidation of said electrochromic material is substantially prevented.
Claim 3
Dependent Claim
38 words
The method according to claim 1, wherein said voltage consists essentially of a voltage of reversible polarity of such level that the absolute value of its negative voltage is greater than the absolute value of its positive voltage.
Claim 4
Dependent Claim
43 words
The method according to claim 1, wherein said voltage comprises (i) a negative biasing voltage and (ii) a voltage of reversible polarity of such level that the absolute value of its negative voltage is equal to the absolute value of its positive voltage.
Claim 5
Dependent Claim
17 words
The method according to claim 1, wherein said cathodic electrochromic material includes non-stoichiometric, oxygen deficient tungsten oxide.
Claim 6
Independent Claim
110 words
A method of operating an electrochromic device to maintain the electrochromic activity of a cathodic electrochromic material provided therein, which method comprises: forming an electrochromic device comprising (1) electrodes and (2) cathodic electrochromic material having a non-stoichiometric composition located therebetween; and applying a voltage, at least during operation of said device, across said electrodes of such level that the absolute value of an applied negative voltage is greater than the absolute value of an applied positive voltage, so as to continuously maintain a negative charge abundance in said electrochromic material sufficient to keep said electrochromic material in a non-stoichiometric state and whereby oxidation of said electrochromic material is substantially prevented.
Claim 7
Independent Claim
110 words
A method of operating an electrochromic device to maintain the electrochromic activity of a cathodic electrochromic material provided therein, which method comprises: forming an electrochromic device comprising (1) electrodes and (2) cathodic electrochromic material having a non-stoichiometric composition located therebetween; and applying a voltage, at least during operation of said device, across said electrodes of such level that the absolute value of an applied negative voltage is greater than the absolute value of an applied positive voltage, so as to continuously maintain a negative charge abundance in said electrochromic material sufficient to keep said electrochromic material in a non-stoichiometric state and whereby oxidation of said electrochromic material is substantially prevented.
Claim 8
Dependent Claim
38 words
The method according to claim 5, wherein said voltage consists essentially of a voltage of reversible polarity of such level that the absolute value of its negative voltage is greater than the absolute value of its positive voltage.
Claim 9
Dependent Claim
43 words
The method according to claim 5, wherein said voltage comprises (i) a negative biasing voltage and (ii) a voltage of reversible polarity of such level that the absolute value of its negative voltage is equal to the absolute value of its positive voltage.
Claim 10
Dependent Claim
116 words
An electrochromic device capable of maintaining the electrochromic activity of a cathodic electrochromic material located therein, said device comprising: electrodes and cathodic electrochromic material located therebetween, said electrochromic material having a non-stoichiometric composition; and an external electrical circuit means coupled to said electrochromic device for applying a voltage, at least during operation of said device, across said electrodes of such level that the absolute value of an applied negative voltage is greater than the absolute value of an applied positive voltage, so as to continuously maintain a negative charge abundance in said cathodic electrochromic material sufficient to keep said cathodic electrochromic material in a non-stoichiometric state and whereby oxidation of said electrochromic material is substantially prevented.
Claim 11
Dependent Claim
116 words
An electrochromic device capable of maintaining the electrochromic activity of a cathodic electrochromic material located therein, said device comprising: electrodes and cathodic electrochromic material located therebetween, said electrochromic material having a non-stoichiometric composition; and an external electrical circuit means coupled to said electrochromic device for applying a voltage, at least during operation of said device, across said electrodes of such level that the absolute value of an applied negative voltage is greater than the absolute value of an applied positive voltage, so as to continuously maintain a negative charge abundance in said cathodic electrochromic material sufficient to keep said cathodic electrochromic material in a non-stoichiometric state and whereby oxidation of said electrochromic material is substantially prevented.
References Cited (Backward Citations)
US3521941A
Cited
US4194812A
Cited
JPS5273756A
Cited
JPS5337050A
Cited
JPS547956A
Cited
US4170406A
Cited
US4350414A
Cited
US4435048A
Cited
US4344674A
Cited
JPS5746290A
Cited
US4505538A
Cited
US4645307A
Cited
JPS60242429A
Cited
US4645308A
Cited
US4762401A
Cited
JPS62186233A
Cited
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1993-10-01 | 1994-04-02 | 1994-10-02 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 1997-10-01 | 1998-04-02 | 1998-10-02 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 2001-10-01 | 2002-04-02 | 2002-10-02 | $7700.00 | Window Closed / Lapsed |