Abstract

Abstract An immobilized biocatalyst suitable for fermenting to produce ethanol is prepared by mixing a biocatalyst such as a microorganism with a reaction product of a homogeneous dispersion of an anionic polysaccharide such as alginate and a cationic polymer such as polyethyleneimine, and combining the resultant dispersion with an oil phase to form beads. A surtactant may be present when combining the dispersion with the oil phase. A water soluble-oil insoluble curing powder includinga salt of a multivalent cation such as calcium chloride is mixed with the beads in the oil phase to gell and dehydrate the beads and to prevent the beads from adhering to one another until individual bead surfaces become hardened.

Inventors

  • 👤 John J. Joung
  • 👤 Cavit Akin
  • 👤 Garfield P. Royer

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-08 20:46
CPC Classifications
C; C12; C12N; C12N11/00; C12N11/02; C12N11/10; C12N11/04; C12P; C12P7/00; C12P7/02; C12P7/04; C12P7/06; Y; Y02; Y02E; Y02E50/00; Y02E50/10

Claims Analysis

Total Claims: 21
Claim 1
Independent Claim 107 words
A method of making a biocatalyst system which comprises the steps of: mixing a biocatalytic entity with the reaction product of a homogeneous dispersion of an anionic polysaccharide polymer with a cationic polymer to form a polymer-biocatalyst dispersion; mixing said polymer biocatalyst dispersion with an oil phase to form beads, and mixing a powder with the beads in the oil phase wherein the powder comprises a water soluble and oil insoluble multivalent cation salt and said powder acts to gell and dehydrate the beads and to prevent the beads from adhering to one another until individual bead surfaces become hardened whereby said biocatalyst system is provided aim.
Claim 2
Independent Claim 107 words
A method of making a biocatalyst system which comprises the steps of: mixing a biocatalytic entity with the reaction product of a homogeneous dispersion of an anionic polysaccharide polymer with a cationic polymer to form a polymer-biocatalyst dispersion; mixing said polymer biocatalyst dispersion with an oil phase to form beads, and mixing a powder with the beads in the oil phase wherein the powder comprises a water soluble and oil insoluble multivalent cation salt and said powder acts to gell and dehydrate the beads and to prevent the beads from adhering to one another until individual bead surfaces become hardened whereby said biocatalyst system is provided aim.
Claim 3
Dependent Claim 20 words
The method of claim 1 wherein said powder is selected from the group consisting of calcium chloride and aluminum sulfate.
Claim 4
Dependent Claim 16 words
The method of claim 1 wherein said anionic polysaccharide polymer is an anionic form of alginate.
Claim 5
Dependent Claim 19 words
The method of claim 1 wherein said cationic polymer is selected from the group including polyalkane amines and imines.
Claim 6
Dependent Claim 11 words
The method of claim 1 wherein said cationic polymer is polyethyleneimine.
Claim 7
Dependent Claim 12 words
The method of claim 1 wherein said biocatalytic entity is a microorganism.
Claim 8
Dependent Claim 11 words
The method of claim 6 wherein said microorganism is a yeast.
Claim 9
Dependent Claim 25 words
The method of claim 1 wherein said step of mixing said polymer biocatalyst dispersion with an oil phase is performed in the presence of surfactants.
Claim 10
Dependent Claim 23 words
The method of claim 1 wherein said polymer biocatalyst dispersion has a pH and said pH is altered causing the dispersion to gel.
Claim 11
Dependent Claim 28 words
The method of claim 9 wherein the pH of the polymer biocatalyst dispersion is above approximately 7.5 and lowered after mixing with the oil phase to approximately 6.
Claim 12
Dependent Claim 22 words
The method of claim 8 wherein said surfactants are selected from the group consisting of water insoluble surfactants and water soluble surfactants.
Claim 13
Dependent Claim 23 words
The method of claim 11 wherein the relative amounts of water insoluble surfactants and water soluble surfactants are varied to adjust bead size.
Claim 14
Dependent Claim 27 words
The method of claim 1 wherein the biocatalyst system prepared is used to produce ethanol by contacting the system with a fermentable substrate and recovering ethanol therefrom.
Claim 15
Dependent Claim 15 words
The method of claim 13 wherein said polysaccharide polymer is an anionic form of alginate.
Claim 16
Dependent Claim 11 words
The method of claim 13 wherein said cationic polymer is polyethyleneimine.
Claim 17
Dependent Claim 12 words
The method of claim 13 wherein said biocatalytic entity is a microorganism.
Claim 18
Dependent Claim 24 words
The method of claim 13 wherein said mixing of said polymer biocatalyst dispersion with an oil phase is performed in the presence of surfactants.
Claim 19
Dependent Claim 10 words
A biocatalyst system prepared by the method of claim 1.
Claim 20
Independent Claim 118 words
A method of making a biocatalyst system which comprises the steps of: mixing a biocatalytic entity with the reaction product of a homogeneous dispersion of an anionic polysaccharide polymer with a cationic polymer to form a polymer-biocatalyst dispersion, said cationic polymer selected from the group consisting of polyalkane amines and imines; mixing said polymer-biocatalyst dispersion with an oil phase to form beads; and adding a powder to the beads in said oil phase wherein said powder includes water soluble and oil insoluble salts having multivalent cations, and said powder acts to gell and dehydrate the beads and to prevent the beds from adhering to one another until individual bead surfaces become hardened whereby said biocatalyst system is provided.
Claim 21
Independent Claim 118 words
A method of making a biocatalyst system which comprises the steps of: mixing a biocatalytic entity with the reaction product of a homogeneous dispersion of an anionic polysaccharide polymer with a cationic polymer to form a polymer-biocatalyst dispersion, said cationic polymer selected from the group consisting of polyalkane amines and imines; mixing said polymer-biocatalyst dispersion with an oil phase to form beads; and adding a powder to the beads in said oil phase wherein said powder includes water soluble and oil insoluble salts having multivalent cations, and said powder acts to gell and dehydrate the beads and to prevent the beds from adhering to one another until individual bead surfaces become hardened whereby said biocatalyst system is provided.

References Cited (Backward Citations)

GB1469072A Cited
US4138292A Cited
US4391909A Cited
US4334027A Cited
GB2082591A Cited
EP0052829A2 Cited
US4347320A Cited
JPS5974984A Cited
JPS59113889A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1994-02-25 1994-08-27 1995-02-26 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1998-02-25 1998-08-27 1999-02-26 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 2002-02-25 2002-08-27 2003-02-26 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag