Pressure-sensitive adhesive composition comprising poly-4-methyl-1-pentene as tackifier

Assignee: Mitsui Chemicals Inc
•
Filing: 1987-10-08
•
Granted: 1991-05-07
•
Expires: 2007-10-08
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract In the present invention, a polymer having a number average molecular weight (Mn) of from 200 to 40,000 and a glass transition point of from -75° C. to +10° C. which is obtained by the cationic polymerization of a branched alpha-olenin is used as a tackifier (a tacky producer) for a hot melt adhesive or a pressure-sensitive adhesive. An adhesive composition containing the polymer described above as a tackifier has excellent heat resistance, hue, weather resistance, and the like and has such excellent characteristics that its odor is weak.

Inventors

  • 👤 Kinya Mizui

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-03 09:59
CPC Classifications
C; C09; C09J; C09J201/00; C08; C08L; C08L2666/00; C08L2666/02; C08L2666/04; Y; Y10; Y10S; Y10S525/00; Y10S525/918

Claims Analysis

Total Claims: 4
Claim 1
Independent Claim 69 words
A pressure-sensitive adhesive composition comprising a rubbery hydrocarbon polymer or polychloroprene as a base resin and from 20 to 200 parts by weight of a tackifier per 100 parts by weight of the base resin, the improvement wherein said tackifier comprises a cationically polymerized poly-4-methyl-1-pentene having a number average molecular weight (Mn) of from 200 to 40,000 and a glass transition point of from -75° C. to +10° C.
Claim 2
Dependent Claim 69 words
A pressure-sensitive adhesive composition comprising a rubbery hydrocarbon polymer or polychloroprene as a base resin and from 20 to 200 parts by weight of a tackifier per 100 parts by weight of the base resin, the improvement wherein said tackifier comprises a cationically polymerized poly-4-methyl-1-pentene having a number average molecular weight (Mn) of from 200 to 40,000 and a glass transition point of from -75° C. to +10° C.
Claim 3
Dependent Claim 65 words
The pressure sensitive adhesive composition according to claim 1, wherein said base resin is selected from the group consisting of a natural rubber, a styrene-butadiene copolymer rubber, polybutadiene, polyisoprene, polyisobutylene, a butyl rubber, polychloroprene, an ethylene-propylene copolymer rubber, an ethylene-propylene-alpha-olefin copolymer rubber, an ethylene-propylene-diene copolymer rubber, a styrene-butadiene-styrene block copolymer, a styrene-isoprene-styrene block copolymer, a hydrogenated styrene-butadiene-styrene block copolymer, and a hydrogenated styrene-isoprene-styrene block copolymer.
Claim 4
Dependent Claim 56 words
The pressure sensitive-adhesive composition according to claim 1, wherein said poly-4-methyl-1-pentene has a number average molecular weight (Mn) of from 300 to 30,000, a ratio of a weight average molecular weight (Mw) to the number average molecular weight (Mn) of from 1.3 to 4.0, and a glass transition point of from -60° C. to -30° C.

References Cited (Backward Citations)

US3299022A Cited
US3317501A Cited
JPS5931717A Cited
EP0223858A1 Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1994-05-06 1994-11-05 1995-05-07 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1998-05-06 1998-11-05 1999-05-07 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 2002-05-06 2002-11-05 2003-05-07 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag