← Back to Patent Explorer
US5055165A Expired / Lapsed US ⏱️ 0.0 years remaining

Method and apparatus for the prevention of fouling and/or corrosion of structures in seawater, brackish water and fresh water

Assignee: Marine Environmental Research Inc
•
Filing: 1990-05-15
•
Granted: 1991-10-08
•
Expires: 2010-05-15
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract A device and method for preventing fouling and/or corrosion of the exposed surfaces of a structure which is at in contact with seawater, brackish water; or fresh water. The system includes a conductive zinc-containing coating applied to the exposed surfaces of the structures which are susceptible to fouling and/or corrosion. At the coating and water interface a negative capacitive charge or an asymmetric alternating electrostatic is induced and maintained.

Inventors

  • 👤 William J. Riffe
  • 👤 Jack D. Carter

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-28 11:11
CPC Classifications
B; B08; B08B; B08B17/00; B08B17/02; B63; B63B; B63B59/00; B63B59/04; C; C23; C23F; C23F13/00; C23F15/00

Claims Analysis

Total Claims: 19
Claim 1
Independent Claim 137 words
A system comprising: (a) a conductive structure suitable for being contacted by seawater, brackish water, or fresh water; (b) a conductive zinc-containing coating applied to and conductively coupled with at least the portion of said structure suitable for being contacted by water, said zinc-containing coating forming an interfacial layer between said structure and said water when said structure is contacted by said water; and (c) means for (c1) inducing and maintaining a net negative capacitive charge on said zinc-containing coating or (c2) inducing and maintaining an asymmetric alternating electrostatic potential on said zinc-containing coating, sufficient to prevent corrosion or fouling of said structure, said means comprising at least one condenser bank attached to said structure, wherein, when said structure is contacted by said water, said at least one condenser bank is protected from contact by said water.
Claim 2
Independent Claim 137 words
A system comprising: (a) a conductive structure suitable for being contacted by seawater, brackish water, or fresh water; (b) a conductive zinc-containing coating applied to and conductively coupled with at least the portion of said structure suitable for being contacted by water, said zinc-containing coating forming an interfacial layer between said structure and said water when said structure is contacted by said water; and (c) means for (c1) inducing and maintaining a net negative capacitive charge on said zinc-containing coating or (c2) inducing and maintaining an asymmetric alternating electrostatic potential on said zinc-containing coating, sufficient to prevent corrosion or fouling of said structure, said means comprising at least one condenser bank attached to said structure, wherein, when said structure is contacted by said water, said at least one condenser bank is protected from contact by said water.
Claim 3
Dependent Claim 21 words
The system of claim 1, comprising said means for inducing and maintaining a negative capacitive charge on said conductive zinc-containing coating.
Claim 4
Dependent Claim 21 words
The system of claim 1, comprising said means for inducing an asymmetric alternating electrostatic potential on said conductive zinc-containing coating structure.
Claim 5
Dependent Claim 110 words
The system of claim 3, wherein said means for inducing an asymmetric alternating electrostatic potential on said structure comprises: (c1) means for interposing a dielectric between a first and a second conductor means, wherein said first conductor means is a power source of asymmetric alternating current attached conductively to a condenser bank so arranged with alternately directed diodes that the supplied current is converted to an asymmetric alternating electrostatic potential and said second conductor means is said structure; and (c2) means for generating a potential difference between said first conductor means and said second conductor means, with said second conductor means being negative with respect to said first conductor means.
Claim 6
Dependent Claim 12 words
The system of claim 4, wherein said structure comprises a ship's hull.
Claim 7
Dependent Claim 29 words
The system of claim 5, further including a faradic inductor system to convert an equipotential galvanic current source to an asymmetric alternating electrostatic potential mounted within said metallic structure.
Claim 8
Dependent Claim 128 words
In a ship, the improvement comprising: (a) a conductive hull; (b) a conductive zinc-containing coating applied to and conductively coupled with at least the portion of said hull which is submerged when said ship is in water, said conductive zinc coating forming an interfacial layer between said water and said conductive hull; and (c) means for (c1) inducing and maintaining a negative capacitive charge on said conductive zinc-containing coating or (c2) inducing and maintaining an asymmetric alternating electrostatic potential on said hull sufficient to prevent corrosion or fouling of said hull, said means comprising at least one condenser bank attached to said hull, wherein, when said hull is at least partially submerged in said water, said at least one condenser bank is protected from contact by said water.
Claim 9
Dependent Claim 128 words
In a ship, the improvement comprising: (a) a conductive hull; (b) a conductive zinc-containing coating applied to and conductively coupled with at least the portion of said hull which is submerged when said ship is in water, said conductive zinc coating forming an interfacial layer between said water and said conductive hull; and (c) means for (c1) inducing and maintaining a negative capacitive charge on said conductive zinc-containing coating or (c2) inducing and maintaining an asymmetric alternating electrostatic potential on said hull sufficient to prevent corrosion or fouling of said hull, said means comprising at least one condenser bank attached to said hull, wherein, when said hull is at least partially submerged in said water, said at least one condenser bank is protected from contact by said water.
Claim 10
Dependent Claim 21 words
The ship of claim 7, comprising said means for inducing and maintaining a negative capacitive charge on said conductive zinc-containing coating.
Claim 11
Dependent Claim 20 words
The ship of claim 7, comprising said means for inducing an asymmetric alternating electrostatic potential on said conductive zinc-containing coating.
Claim 12
Dependent Claim 109 words
In a structure which is in contact with seawater, brackish water, or fresh water, the improvement comprising: (a) said structure being conductive and having applied thereto and conductively coupled thereto a conductive zinc-containing coating, said conductive zinc-containing coating forming an interfacial layer between said structure and said water; and (b) means for (b1) inducing and maintaining a negative capacitive charge on said conductive zinc-containing coating or for (b2) inducing and maintaining an asymmetric alternating electrostatic potential on said conductive zinc-containing coating, sufficient to prevent corroding or fouling of said structure, said means comprising at least one condenser bank attached to said structure and protected from contact by said water.
Claim 13
Dependent Claim 109 words
In a structure which is in contact with seawater, brackish water, or fresh water, the improvement comprising: (a) said structure being conductive and having applied thereto and conductively coupled thereto a conductive zinc-containing coating, said conductive zinc-containing coating forming an interfacial layer between said structure and said water; and (b) means for (b1) inducing and maintaining a negative capacitive charge on said conductive zinc-containing coating or for (b2) inducing and maintaining an asymmetric alternating electrostatic potential on said conductive zinc-containing coating, sufficient to prevent corroding or fouling of said structure, said means comprising at least one condenser bank attached to said structure and protected from contact by said water.
Claim 14
Dependent Claim 21 words
The structure of claim 10, comprising said means for inducing and maintaining a negative capacitive charge on said conductive zinc-containing coating.
Claim 15
Dependent Claim 22 words
The structure of claim 10, comprising said means for inducing and maintaining an asymmetric alternating electrostatic potential on said conductive zinc-containing coating.
Claim 16
Independent Claim 142 words
A method for preventing the fouling or corrosion of a conductive structure bearing a zinc-coating applied thereto and conductively coupled thereto, said conductive structure being in contact with seawater, brackish water, or fresh water, wherein said conductive zinc-containing coating forms an interfacial layer between said conductive structure and said water, said method comprising: (a) inducing and maintaining a negative capacitive charge on said conductive zinc-containing coating sufficient to prevent said fouling or said corroding; or (b) inducing and maintaining an asymmetric alternating electrostatic potential on said conductive zinc-containing coating sufficient to prevent said fouling or said corroding; further comprising using a means for inducing said negative capacitive charge or for inducing said asymmetric alternating electrostatic potential, said means comprising at least one condenser bank attached to said structure, wherein said at least one condenser bank is protected from contact by said water.
Claim 17
Independent Claim 142 words
A method for preventing the fouling or corrosion of a conductive structure bearing a zinc-coating applied thereto and conductively coupled thereto, said conductive structure being in contact with seawater, brackish water, or fresh water, wherein said conductive zinc-containing coating forms an interfacial layer between said conductive structure and said water, said method comprising: (a) inducing and maintaining a negative capacitive charge on said conductive zinc-containing coating sufficient to prevent said fouling or said corroding; or (b) inducing and maintaining an asymmetric alternating electrostatic potential on said conductive zinc-containing coating sufficient to prevent said fouling or said corroding; further comprising using a means for inducing said negative capacitive charge or for inducing said asymmetric alternating electrostatic potential, said means comprising at least one condenser bank attached to said structure, wherein said at least one condenser bank is protected from contact by said water.
Claim 18
Dependent Claim 18 words
The method of claim 13, comprising inducing and maintaining said negative capacitive charge on said conductive zinc-containing coating.
Claim 19
Dependent Claim 17 words
The method of claim 13, comprising inducing said asymmetric alternating electrostatic potential on said conductive zinc-containing coating.

References Cited (Backward Citations)

US3497434A Cited
US4767512A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1994-10-07 1995-04-08 1995-10-08 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1998-10-07 1999-04-08 1999-10-08 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 2002-10-07 2003-04-08 2003-10-08 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag