Abstract

Abstract A method of conditioning separator mold plates for repeated use in high temperature sequential molding of printed circuit board laminates comprises the step of integrally applying at least one thin, continuous coat, preferably on the order of about 1 microinch, of a silane-based mold release composition prior to each sequential molding operation for facilitating repeated use of the plates in sequential molding operations the silane-based mold release composition is preferably applied in a continuous automated process including a spray gun, preferably of an air atomized type and more preferably of a high transfer efficiency type, for applying the coating followed by an infrared heating step, the separator mold plates being carried by a conveyor through a tunnel including the spray gun and infrared heater. Separator mold plates formed as a product of the process are adapted for use in large numbers of sequential molding operations with an additional coat of the silane-based mold release compound being applied prior to each operation because of the microinch thickness of each coating.

Inventors

  • 👤 John J. Dagostino
  • 👤 Gregory L. Lucas

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-02 14:19
CPC Classifications
B; B28; B28B; B28B7/00; B28B7/38; B29; B29C; B29C33/00; B29C33/56; B29C33/58; H; H05; H05K; H05K3/00; H05K3/46; H05K3/4611; B29C33/60; B29C33/62; B29C33/64; B29L; B29L2031/00; B29L2031/34; B29L2031/3425; H05K2203/00; H05K2203/06; H05K2203/068

Claims Analysis

Total Claims: 9
Claim 1
Independent Claim 161 words
A method of high temperature sequential molding of multiple printed circuit board laminates comprising the steps of arranging separator mold plates between mold die elements and adjacent laminate surfaces and between facing laminate surfaces of different printed circuit board laminates are simultaneously molded, integrally applying at least one thin, continuous coat of about one microinch thickness of a silane-based mold release composition to opposite surfaces of each separator mold plate prior to each sequential molding operation for facilitating repeated use of the plates in sequential molding operations and to maintain dimensionally accurate surfaces on the respective printed circuit board laminates while avoiding the need for hard abrasive cleaning of the separator mold plates between sequential molding operations, and selecting the thickness of the silane-based mold release coating to permit application of an additional coat prior to each sequential molding operation to assure coating continuity on opposite surfaces of the plates without excessive build-up even after use in many sequential molding operations.
Claim 2
Independent Claim 161 words
A method of high temperature sequential molding of multiple printed circuit board laminates comprising the steps of arranging separator mold plates between mold die elements and adjacent laminate surfaces and between facing laminate surfaces of different printed circuit board laminates are simultaneously molded, integrally applying at least one thin, continuous coat of about one microinch thickness of a silane-based mold release composition to opposite surfaces of each separator mold plate prior to each sequential molding operation for facilitating repeated use of the plates in sequential molding operations and to maintain dimensionally accurate surfaces on the respective printed circuit board laminates while avoiding the need for hard abrasive cleaning of the separator mold plates between sequential molding operations, and selecting the thickness of the silane-based mold release coating to permit application of an additional coat prior to each sequential molding operation to assure coating continuity on opposite surfaces of the plates without excessive build-up even after use in many sequential molding operations.
Claim 3
Dependent Claim 31 words
The method of claim 1 further comprising the step of applying at least two coats to each opposite surface of the plate prior to its use in a first molding operation.
Claim 4
Dependent Claim 44 words
The method of claim 1 further comprising the step of forming holes in the separator mold plates for receiving tooling pins also passing through the printed circuit board laminates, the integrally applied silane-base mold release composition assuring continuity of the coat about the holes.
Claim 5
Independent Claim 167 words
A method of conditioning separator mold plates for repeated use in high temperature sequential molding of assemblies of multiple printed circuit board laminates, comprising the steps of: (a) carrying a progression of separator mold plates through automated sections of a continuous process by conveyor means; (b) spraying a thin, integral coating of about one microinch thickness of a silane-based mold release agent in a reciprocating zig-zag pattern on opposite surfaces of each separator mold plate prior to each sequential mold operation in one automated station of the process; (c) curing the coating on the progression of separator mold plates in a subsequent automated drying station enclosed by tunnel means; and (d) repeating steps (a)-(c) prior to re-use of the mold plates in each sequential molding operation, whereby repeated use of the plates is facilitated in an efficient manner while maintaining dimensionally accurate surfaces on the multiple printed circuit board laminates and avoiding the need for hard abrasive cleaning of the separator mold plates between sequential molding operations.
Claim 6
Independent Claim 167 words
A method of conditioning separator mold plates for repeated use in high temperature sequential molding of assemblies of multiple printed circuit board laminates, comprising the steps of: (a) carrying a progression of separator mold plates through automated sections of a continuous process by conveyor means; (b) spraying a thin, integral coating of about one microinch thickness of a silane-based mold release agent in a reciprocating zig-zag pattern on opposite surfaces of each separator mold plate prior to each sequential mold operation in one automated station of the process; (c) curing the coating on the progression of separator mold plates in a subsequent automated drying station enclosed by tunnel means; and (d) repeating steps (a)-(c) prior to re-use of the mold plates in each sequential molding operation, whereby repeated use of the plates is facilitated in an efficient manner while maintaining dimensionally accurate surfaces on the multiple printed circuit board laminates and avoiding the need for hard abrasive cleaning of the separator mold plates between sequential molding operations.
Claim 7
Dependent Claim 31 words
The method of claim 4 further comprising the step of applying at least two coats to each opposite surface of the plate prior to its use in a first molding operation.
Claim 8
Dependent Claim 23 words
The method of claim 4 wherein spraying is carried out by a spray gun of an air atomizing and high transfer efficiency type.
Claim 9
Dependent Claim 30 words
The method of claim 4 wherein the step of curing is carried out by infrared heating after each application of silane-based mold release composition in order to cure the coating.

References Cited (Backward Citations)

US2674619A Cited
US2786080A Cited
US3290760A Cited
US3421211A Cited
US3984598A Cited
US4201616A Cited
US4371476A Cited
US4571279A Cited
US4753847A Cited
US4713284A Cited
US4855184A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1994-11-11 1995-05-13 1995-11-12 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1998-11-11 1999-05-13 1999-11-12 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 2002-11-11 2003-05-13 2003-11-12 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag