← Back to Patent Explorer
US5425825A Expired / Lapsed US ⏱️ 0.0 years remaining

Reclosable zipper with tamper evident feature

Assignee: Minigrip Inc
•
Filing: 1993-04-22
•
Granted: 1995-06-20
•
Expires: 2013-04-22
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract A plastic bag having a reclosable plastic zipper is provided with a tamper-evident, non-reclosable peel seal formed by applying an adhesive to a treated strip adjacent to the interlocking zipper. The treatment is preferably by corona discharge, which causes the adhesive used to provide the peel seal to preferentially adhere to the treated strip when the peel seal is broken. A method for manufacturing the reclosable plastic zipper includes the steps of extruding a zipper profile, treating a portion of its surface, preferably by corona discharge, applying an adhesive to the treated portion, slitting the profile lengthwise, and folding over one of the resulting sides of the zipper to interlock them with one another.

Inventors

  • 👤 George Rasko
  • 👤 Lawrence Share

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-31 06:04
CPC Classifications
B; B65; B65D; B65D75/00; B65D75/28; B65D75/30; B65D75/32; B65D75/325; B65D75/326; B29; B29C; B29C59/00; B29C59/08; B29C59/10; B29C65/00; B29C65/48; B29C65/52; B29C65/54; B29C66/00; B29C66/004; B29C66/01; B29C66/02; B29C66/05; B29C66/10; B29C66/11; B29C66/112; B29C66/1122; B29C66/13; B29C66/131; B29C66/20; B29C66/24; B29C66/242; B29C66/2424; B29C66/24243; B29C66/24244; B29C66/40; B29C66/41; B29C66/43; B29C66/47; B29C66/474; B29C66/50; B29C66/51; B29C66/53; B29C66/532; B29C66/534; B29C66/5346; B29C66/53461; B29C66/80; B29C66/83; B29C66/834; B29C66/8341; B29C66/83411; B29C66/83413; B29D; B29D5/00; B29D5/10; B65D33/00; B65D33/16; B65D33/25; B65D33/2508; B65D33/2516; B65D33/2525; B65D33/2533; B65D77/00; B65D77/10; B65D77/20; B65D77/2024; B65D77/2068; B65D77/2072; B65D77/2088; A; A44; A44B; A44B19/00; A44B19/10; A44B19/16; B29C2793/00; B29C66/431; B29C66/4312; B29C66/43121; B29L; B29L2005/00; B29L2031/00; B29L2031/712; B29L2031/7128; B65D2575/00; B65D2575/28; B65D2575/30; B65D2575/32; B65D2575/3209; B65D2575/3218; B65D2575/3245; B65D2575/36; B65D2575/361; B65D2575/362; B65D2575/365; Y; Y10; Y10T; Y10T156/00; Y10T156/10; Y10T156/1052; Y10T156/1062; Y10T156/1067; Y10T156/1069; Y10T24/00; Y10T24/25; Y10T24/2532; Y10T24/2534

Claims Analysis

Total Claims: 30
Claim 1
Independent Claim 175 words
A method for forming a tamper-evident, nonreclosable peel seal for a reclosable plastic bag, comprising the steps: forming a first flexible plastic web having an interlockable rib and groove member and a side strip adjacent thereto; forming a second flexible plastic web having an interlockable rib and groove member, said second flexible plastic web being interlockable with said first flexible plastic web, and a side strip adjacent thereto; treating a surface of said side strip of said first flexible plastic web to enhance its receptiveness to an adhesive; applying an adhesive to said treated strip; pressing said side strips of said first and second flexible plastic webs together under heat, such that the temperature of said side strip of said first flexible plastic web is higher than the temperature of said side strip of said second flexible plastic web, said adhesive being between said side strips; and cooling said first and second flexible plastic webs to form a hermetic, tamper-evident nonreclosable peel seal between said side strips of said first and second flexible plastic webs.
Claim 2
Independent Claim 175 words
A method for forming a tamper-evident, nonreclosable peel seal for a reclosable plastic bag, comprising the steps: forming a first flexible plastic web having an interlockable rib and groove member and a side strip adjacent thereto; forming a second flexible plastic web having an interlockable rib and groove member, said second flexible plastic web being interlockable with said first flexible plastic web, and a side strip adjacent thereto; treating a surface of said side strip of said first flexible plastic web to enhance its receptiveness to an adhesive; applying an adhesive to said treated strip; pressing said side strips of said first and second flexible plastic webs together under heat, such that the temperature of said side strip of said first flexible plastic web is higher than the temperature of said side strip of said second flexible plastic web, said adhesive being between said side strips; and cooling said first and second flexible plastic webs to form a hermetic, tamper-evident nonreclosable peel seal between said side strips of said first and second flexible plastic webs.
Claim 3
Dependent Claim 80 words
A method as claimed in claim 1 wherein said step of pressing said side strips of said first and second flexible plastic webs together under heat comprises passing said side strip of said first flexible plastic web over a first sealing bar and passing said side strip of said second flexible plastic web over a second sealing bar, said first and second sealing bars being heated and pressing said side strips of said first and second flexible plastic webs together.
Claim 4
Dependent Claim 31 words
A method as claimed in claim 2 wherein said first sealing bar is at a temperature of 360° F., and said second sealing bar is at a temperature of 302° F.
Claim 5
Dependent Claim 39 words
A method as claimed in claim 1 wherein said step of treating a surface of said side strip of said first flexible plastic web to enhance its receptiveness to an adhesive is carried out using a flame treatment instrument.
Claim 6
Dependent Claim 39 words
A method as claimed in claim 1 wherein said step of treating a surface of said side strip of said first flexible plastic web to enhance its receptiveness to an adhesive is carried out using a corona discharge instrument.
Claim 7
Dependent Claim 53 words
A method as claimed in claim 1 further comprising the steps of: providing a first ply and a second ply of plastic sheet material; bonding said first ply of plastic sheet material to said first flexible plastic web; and bonding said second ply of plastic sheet material to said second flexible plastic web.
Claim 8
Independent Claim 166 words
A method for manufacturing a reclosable zipper having a tamper-evident, nonreclosable peel seal for a reclosable plastic bag, comprising: extruding a profile having interlockable rib and groove members and two plane areas from a synthetic polymeric material; treating one of said two plane areas longitudinally along said profile to enhance the receptiveness of the surface thereof to an adhesive; applying said adhesive to said treated plane area; slitting said profile longitudinally to produce two interlockable sides of said zipper, one side having said treated plane area; folding over one of said two sides of said zipper, so that said treated plane area having said adhesive faces the other of said two plane areas, and so that said rib and groove members may be interlocked with one another; and, pressing said plane areas together under heat, such that the temperature of the treated plane area is higher than the temperature of the other plane area, said adhesive being between said plane areas, to form said peel seal.
Claim 9
Independent Claim 166 words
A method for manufacturing a reclosable zipper having a tamper-evident, nonreclosable peel seal for a reclosable plastic bag, comprising: extruding a profile having interlockable rib and groove members and two plane areas from a synthetic polymeric material; treating one of said two plane areas longitudinally along said profile to enhance the receptiveness of the surface thereof to an adhesive; applying said adhesive to said treated plane area; slitting said profile longitudinally to produce two interlockable sides of said zipper, one side having said treated plane area; folding over one of said two sides of said zipper, so that said treated plane area having said adhesive faces the other of said two plane areas, and so that said rib and groove members may be interlocked with one another; and, pressing said plane areas together under heat, such that the temperature of the treated plane area is higher than the temperature of the other plane area, said adhesive being between said plane areas, to form said peel seal.
Claim 10
Dependent Claim 21 words
A method as claimed in claim 7 further comprising the step of interlocking said rib and groove members with one another.
Claim 11
Dependent Claim 19 words
A method as claimed in claim 7 wherein said treating step is carried out using a flame treatment instrument.
Claim 12
Dependent Claim 19 words
A method as claimed in claim 7 wherein said treating step is carried out using a corona discharge instrument.
Claim 13
Dependent Claim 21 words
A method as claimed in claim 7 wherein said slitting step is performed longitudinally through said interlockable rib and groove members.
Claim 14
Dependent Claim 19 words
A method as claimed in claim 7 wherein said slitting step is performed longitudinally between said two plane areas.
Claim 15
Dependent Claim 60 words
A method as claimed in claim 7 further comprising the steps of: providing a first ply and a second ply of plastic sheet material; bonding said first ply of plastic sheet material to one of said two sides of said zipper; and bonding said second ply of plastic sheet material to the other of said two sides of said zipper.
Claim 16
Dependent Claim 57 words
A method as claimed in claim 7 wherein said step of pressing said plane areas together under heat comprises passing said treated plane area over a first sealing bar and passing said other of said two plane areas over a second sealing bar, said first and second sealing bars being heated and pressing said plane areas together.
Claim 17
Dependent Claim 31 words
A method as claimed in claim 14 wherein said first sealing bar is at a temperature of 360° F., and said second sealing bar is at a temperature of 302° F.
Claim 18
Independent Claim 203 words
A method for forming a tamper-evident, nonreclosable peel seal for a reclosable plastic bag, comprising the steps: forming a first flexible plastic web having an interlockable rib and groove member and a side strip adjacent thereto; forming a second flexible plastic web having an interlockable rib and groove member, said second flexible plastic web being interlockable with said first flexible plastic web, and a side strip adjacent thereto; treating a surface of said side strip of said first flexible plastic web to cause an adhesive to preferentially adhere thereto, so that all of said adhesive may remain on said side strip when said peel seal is broken; applying said adhesive to said surface of said side strip of said first flexible plastic web; pressing said side strips of said first and second flexible plastic webs together under heat, such that the temperature of said side strip of said first flexible plastic web is higher than the temperature of said side strip of said second flexible plastic web, said adhesive being between said side strips; and cooling said first and second flexible plastic webs to form a hermetic, tamper-evident nonreclosable peel seal between said side strips of said first and second flexible plastic webs.
Claim 19
Independent Claim 203 words
A method for forming a tamper-evident, nonreclosable peel seal for a reclosable plastic bag, comprising the steps: forming a first flexible plastic web having an interlockable rib and groove member and a side strip adjacent thereto; forming a second flexible plastic web having an interlockable rib and groove member, said second flexible plastic web being interlockable with said first flexible plastic web, and a side strip adjacent thereto; treating a surface of said side strip of said first flexible plastic web to cause an adhesive to preferentially adhere thereto, so that all of said adhesive may remain on said side strip when said peel seal is broken; applying said adhesive to said surface of said side strip of said first flexible plastic web; pressing said side strips of said first and second flexible plastic webs together under heat, such that the temperature of said side strip of said first flexible plastic web is higher than the temperature of said side strip of said second flexible plastic web, said adhesive being between said side strips; and cooling said first and second flexible plastic webs to form a hermetic, tamper-evident nonreclosable peel seal between said side strips of said first and second flexible plastic webs.
Claim 20
Dependent Claim 80 words
A method as claimed in claim 16 wherein said step of pressing said side strips of said first and second flexible plastic webs together under heat comprises passing said side strip of said first flexible plastic web over a first sealing bar and passing said side strip of said second flexible plastic web over a second sealing bar, said first and second sealing bars being heated and pressing said side strips of said first and second flexible plastic webs together.
Claim 21
Dependent Claim 31 words
A method as claimed in claim 17 wherein said first sealing bar is at a temperature of 360° F., and said second sealing bar is at a temperature of 302° F.
Claim 22
Dependent Claim 53 words
A method as claimed in claim 16 further comprising the steps of: providing a first ply and a second ply of plastic sheet material; bonding said first ply of plastic sheet material to said first flexible plastic web; and bonding said second ply of plastic sheet material to said second flexible plastic web.
Claim 23
Independent Claim 185 words
A method for manufacturing a reclosable zipper having a tamper-evident, nonreclosable peel seal for a reclosable plastic bag, comprising: extruding a profile having interlockable rib and groove members and two plane areas from a synthetic polymeric material; treating one of said two plane areas to cause an adhesive to preferentially adhere thereto, so that all of said adhesive may remain on said one of said two plane areas when said seal is broken; applying said adhesive to said one of said two plane areas longitudinally along said profile; slitting said profile longitudinally to produce two interlockable sides of said zipper, one side having said adhesive; folding over one of said two sides of said zipper, so that said treated plane area having said adhesive faces the other of said two plane areas, and so that said rib and groove members may be interlocked with one another; and, pressing said plane areas together under heat, such that the temperature of the treated plane area is higher than the temperature of the other plane area, said adhesive being between said plane areas, to form said peel seal.
Claim 24
Independent Claim 185 words
A method for manufacturing a reclosable zipper having a tamper-evident, nonreclosable peel seal for a reclosable plastic bag, comprising: extruding a profile having interlockable rib and groove members and two plane areas from a synthetic polymeric material; treating one of said two plane areas to cause an adhesive to preferentially adhere thereto, so that all of said adhesive may remain on said one of said two plane areas when said seal is broken; applying said adhesive to said one of said two plane areas longitudinally along said profile; slitting said profile longitudinally to produce two interlockable sides of said zipper, one side having said adhesive; folding over one of said two sides of said zipper, so that said treated plane area having said adhesive faces the other of said two plane areas, and so that said rib and groove members may be interlocked with one another; and, pressing said plane areas together under heat, such that the temperature of the treated plane area is higher than the temperature of the other plane area, said adhesive being between said plane areas, to form said peel seal.
Claim 25
Dependent Claim 21 words
A method as claimed in claim 20 further comprising the step of interlocking said rib and groove members with one another.
Claim 26
Dependent Claim 21 words
A method as claimed in claim 20 wherein said slitting step is performed longitudinally through said interlockable rib and groove members.
Claim 27
Dependent Claim 19 words
A method as claimed in claim 20 wherein said slitting step is performed longitudinally between said two plane areas.
Claim 28
Dependent Claim 60 words
A method as claimed in claim 20 further comprising the steps of: providing a first ply and a second ply of plastic sheet material; bonding said first ply of plastic sheet material to one of said two sides of said zipper; and bonding said second ply of plastic sheet material to the other of said two sides of said zipper.
Claim 29
Dependent Claim 59 words
A method as claimed in claim 20 wherein said step of pressing said plane areas together under heat comprises passing said plane area having said adhesive over a first sealing bar and passing said other of said two plane areas over a second sealing bar, said first and second sealing bars being heated and pressing said plane areas together.
Claim 30
Dependent Claim 31 words
A method as claimed in claim 25 wherein said first sealing bar is at a temperature of 360° F., and said second sealing bar is at a temperature of 302° F.

References Cited (Backward Citations)

US3986914A Cited
US4540537A Cited
US4966470A Cited
US5224779A Cited
US4947525A Cited
US5238306A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1998-06-19 1998-12-19 1999-06-20 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 2002-06-19 2002-12-19 2003-06-20 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 2006-06-19 2006-12-19 2007-06-20 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag