← Back to Patent Explorer
US5795953A Expired / Lapsed US ⏱️ 0.0 years remaining

Soluble, electroconductive polypyrrole and method for preparing the same

Assignee: Korea Institute of Science and Technology
•
Filing: 1995-09-22
•
Granted: 1998-08-18
•
Expires: 2015-09-22
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract Polypyrrole represented as the following structural formula II: ##STR1## wherein A - = ##STR2## which is synthesized by a method comprising the step of polymerizing pyrrole monomer in an aqueous solution containing dodecylbenzene sulfonic acid as a dopant, in the presence of an oxidant, resulting in polypyrrole which is easily dissolved in organic solvents.

Inventors

  • 👤 Chung Yup Kim
  • 👤 Jun Young Lee
  • 👤 Dong Young Kim

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-01 18:22
CPC Classifications
C; C08; C08G; C08G61/00; C08G61/12; C08G61/122; C08G61/123; C08G61/124

Claims Analysis

Total Claims: 7
Claim 1
Independent Claim 52 words
A method for preparing soluble, electroconductive polypyrrole comprising the step of polymerizing pyrrole monomer in an aqueous solution containing dodecylbenzene sulfonic acid as a dopant, in the presence of about 0.05 moles to about 0.5 moles of a persulfate oxidant per mole of said pyrrole monomer to produce said soluble, electroconductive polypyrrole.
Claim 2
Independent Claim 52 words
A method for preparing soluble, electroconductive polypyrrole comprising the step of polymerizing pyrrole monomer in an aqueous solution containing dodecylbenzene sulfonic acid as a dopant, in the presence of about 0.05 moles to about 0.5 moles of a persulfate oxidant per mole of said pyrrole monomer to produce said soluble, electroconductive polypyrrole.
Claim 3
Dependent Claim 22 words
The method in accordance with claim 1, wherein said step of polymerizing is carried out at a temperature of about 5° C.
Claim 4
Dependent Claim 26 words
The method in accordance with claim 1, wherein said polypyrrole has an intrinsic viscosity in m-cresol from about 0.07 dl/g to 0.3 dl/g at 30° C.
Claim 5
Dependent Claim 22 words
The method in accordance with claim 1, wherein said polypyrrole is soluble in chloroform in the presence of additional dodecylbenzene sulfonic acid.
Claim 6
Dependent Claim 17 words
A method in accordance with claim 1, wherein said persulfate oxidant is ammonium persulfate or potassium persulfate.
Claim 7
Dependent Claim 30 words
The method in accordance with claim 1, wherein said dodecylbenzene sulfonic acid is added at an amount of about 0.1 to about 1.0 moles per mole of said pyrrole monomers.

References Cited (Backward Citations)

No citation records indexed.

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 2001-08-17 2002-02-16 2002-08-18 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 2005-08-17 2006-02-16 2006-08-18 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 2009-08-17 2010-02-16 2010-08-18 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag