Abstract

Abstract This invention relates to a photographic element comprising at least one photosensitive layer, and a base material comprising an upper and lower biaxially oriented polymer sheet separated by a paper sheet, wherein said base material has a thickness of greater than 254 micrometers, a stiffness of greater than 325 millinewtons in any direction, and an upper surface roughness of less than 0.45 micrometers at a spatial frequency of between 0.30 and 6.35 millimeters, and a transmission percent of less than 15 percent.

Inventors

  • 👤 Peter Thomas c/o Eastman Kodak Company Aylward
  • 👤 Robert Paul c/o Eastman Kodak Company Bourdelais
  • 👤 Alphonse Dominic c/o Eastman Kodak Company Camp

Bibliographic Details

Application Number —
Jurisdiction EP
Data Source google_patents
Last Synchronized 2026-10-31 08:53
CPC Classifications
G; G03; G03C; G03C1/00; G03C1/76; G03C1/775; G03C1/79; G03C11/00; G03C11/08; G03C5/00; G03C5/04; Y; Y10; Y10S; Y10S430/00; Y10S430/162

Claims Analysis

Total Claims: 10
Claim 1
Independent Claim 78 words
A photographic element comprising at least one photosensitive layer, and a base material comprising an upper and lower biaxially oriented polymer sheet separated by a paper sheet, wherein said base material has a thickness of greater than 254 micrometers, a stiffness of greater than 325 millinewtons in any direction, and an upper surface roughness of less than 0.45 micrometers at a spatial frequency of between 0.30 and 6.35 millimeters, and a transmission percent of less than 15 percent.
Claim 2
Dependent Claim 20 words
The photographic element of Claim 1 wherein said paper sheet has a basis weight of greater than 200g/m 2 .
Claim 3
Dependent Claim 21 words
The photographic element of Claims 1 or 2 wherein said photographic element has a stiffness of between 325 and 650 millinewtons.
Claim 4
Dependent Claim 22 words
The photographic element of any of Claims 1-3 wherein said photographic element has upper surface roughness of between 0.20 and 0.50 micrometers.
Claim 5
Dependent Claim 21 words
The photographic element of any of Claims 1-4 wherein said paper sheet has a thickness of between 6.7 and 9.0 mils.
Claim 6
Dependent Claim 43 words
The photographic element of any of Claims 1-5 wherein said base material comprising an upper and lower biaxially oriented polymer sheet separated by a paper sheet further comprises an adhesive layer between said upper and lower biaxially oriented polymer sheets and paper sheet.
Claim 7
Dependent Claim 96 words
A reflection display material comprising an image, a laminated base material, and a scratch resistant polymer sheet laminated onto the top surface of said image, wherein said laminated base material comprises an upper and lower biaxially oriented polymer sheet separated by a paper sheet, wherein said laminated base material has a thickness of greater than 254 micrometers, a stiffness of greater than 325 millinewtons in any direction, and an upper surface roughness of less than 0.45 micrometers at a spatial frequency of between 0.30 and 6.35 millimeters, and a transmission percent of less than 15 percent.
Claim 8
Dependent Claim 17 words
The reflection display material of Claim 7 wherein said scratch resistant polymer sheet comprises a polycarbonate sheet.
Claim 9
Dependent Claim 24 words
The reflection display material of Claims 7 or 8 wherein said scratch resistant polymer sheet has a scratch resistance of greater than 3 grams.
Claim 10
Independent Claim 114 words
A method of forming a reflection display material comprising providing a photographic element comprising at least one photosensitive layer, and a base material comprising an upper and lower biaxially oriented polymer sheet separated by a paper sheet, wherein said base material has a thickness of greater than 254 micrometers, a stiffness of greater than 325 millinewtons in any direction, and an upper surface roughness of less than 0.45 micrometers at a spatial frequency of between 0.30 and 6.35 millimeters, and a transmission percent of less than 15 percent, imaging said photographic element, developing said photographic element to produce an image, and bringing the developed photographic element into contact with a scratch resistant polymer sheet.

References Cited (Backward Citations)

No citation records indexed.

USPTO Annuity & Maintenance Windows

Maintenance schedule is calculated for granted US utility patents.

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag