Patent US3168369A successfully refreshed from Google Patents.
← Back to Patent Explorer
US3168369A Expired / Lapsed US ⏱️ 0.0 years remaining

Uranium processing

Assignee: WR Grace and Co
•
Filing: 1961-12-18
•
Granted: 1965-02-02
•
Expires: 1981-12-18
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

No abstract record available.

Inventors

  • 👤 Stanton L Reese
  • 👤 Thomas C Runion

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-08 23:30
CPC Classifications
C; C01; C01G; C01G43/00; C01G43/01; C01G43/025; C01G43/04; C01G43/06; C01P; C01P2004/00; C01P2004/60; C01P2004/61; C01P2004/62; C01P2006/00; C01P2006/11; C01P2006/14; C01P2006/60; C01P2006/80

Claims Analysis

Total Claims: 4
Claim 1
Independent Claim 74 words
A PROCESS FOR THE PREPARATION OF URANIUM TRIOXIDE WHICH COMPRISES CONVERTING GASEOUS URANIUM HEXAFLUORIDE TO URANYL FLUORIDE BY TREATING THE HEXAFLUORIDE WITH STEAM AT A TEMPERATURE OF ABOUT 230* TO 350*F. AT ATMOSPHERIC PRESSURE FOLLOWED BY CONVERSION OF THE URANYL FLUORIDE TO URANYL OXIDE BY TREATMENT OF THE FLUORIDE AT A TEMPERATURE ABOUT 800* TO 1000*F. IN THE PRESENCE OF STEAM WHILE CAREFULLY EXCLUDING AIR FROM THE REACTOR AND RECOVERING THE URANIUM TRIOXIDE PRODUCT.
Claim 2
Dependent Claim 74 words
A PROCESS FOR THE PREPARATION OF URANIUM TRIOXIDE WHICH COMPRISES CONVERTING GASEOUS URANIUM HEXAFLUORIDE TO URANYL FLUORIDE BY TREATING THE HEXAFLUORIDE WITH STEAM AT A TEMPERATURE OF ABOUT 230* TO 350*F. AT ATMOSPHERIC PRESSURE FOLLOWED BY CONVERSION OF THE URANYL FLUORIDE TO URANYL OXIDE BY TREATMENT OF THE FLUORIDE AT A TEMPERATURE ABOUT 800* TO 1000*F. IN THE PRESENCE OF STEAM WHILE CAREFULLY EXCLUDING AIR FROM THE REACTOR AND RECOVERING THE URANIUM TRIOXIDE PRODUCT.
Claim 3
Dependent Claim 37 words
A PROCESS FOR PREPARING URANIUM DIOXIDE WITH AN AVERAGE PARTICLE DIAMETER OF 0.55 TO 2.5 MICRONS AND A BULK DENSITY OF 0.65 TO 1.5 GRAMS PER CC. WHICH COMPRISES TREATING GASEOUS URANIUM HEXAFLUOIDE WITH STEAM AT A
Claim 4
Dependent Claim 37 words
A PROCESS FOR PREPARING URANIUM DIOXIDE WITH AN AVERAGE PARTICLE DIAMETER OF 0.55 TO 2.5 MICRONS AND A BULK DENSITY OF 0.65 TO 1.5 GRAMS PER CC. WHICH COMPRISES TREATING GASEOUS URANIUM HEXAFLUOIDE WITH STEAM AT A

References Cited (Backward Citations)

US2906598A Cited
US3051566A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1968-02-02 1968-08-03 1969-02-02 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1972-02-02 1972-08-03 1973-02-02 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1976-02-02 1976-08-03 1977-02-02 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag