Claims Analysis
Total Claims: 10
Claim 1
Independent Claim
164 words
METHOD OF MAKING A VARIABLE DEPTH POSITIVE, CONTOUR, IMAGE ON A SUBSTRATE WHICH COMPRISES COATING THE SUBSTRATE WITH A PHOTOPOLYMERIZABLE COATING COMPOSITION CONTAINING (1) A NON-GASEOUS ETHYLENICALLY UNSATURATED COMPOUND CAPABLE OF ADDITION POLYMERIZATION BY FREE-RADICAL INITIATED CHAIN PROPAGATION, (2) 0.001 TI 1.0 PART BY WEIGHT PER PART OF POLYMERIZABLE COMPOUND OF AN ORGANIC LIGHT-SENSITIVE FREE-RADICAL GENERATING SYSTEM, AND (3) 0.1 TO 10 PERCENT BY WEIGHT BASED ON THE COATING COMPOSITION OF A PHOTODISSOCIABLE NITROSO DIMER HAVING A DISSOCIATION CONSTANT OF 10**-2 TO 10**10 AND A DISSOCIATION HALF-LIFE OF AT LEAST 30 SECONDS IN SOLUTION AT 25*C EXPOSING THE PHOTO-POLYNERIZABLE COATING TO LIGHT HAVING WAVELENGTHS BOTH ABOVE 3400A WHICH EFFECT POLYMERIZATION AND BELOW 3400A WHICH DIISOCIATE NITROSO DIMER TO NITROSO MONOMER, THROUGH A TRANSPARENT FILM OF VARIABLE OPTICAL DENSITY TO LIGHT HAVING A WAVELENGTH OF LESS THAN 3400A AND TRANSPARENT TO LIGHT HAVING A WAVELENGTH ABOVE 3400A, AND DEVELOPING A VARIABLE DEPTH, POSITIVE, POLYMERIC, CONTOUR IMAGE BY REMOVING THE NONPOLYMERIZED PORTION OF THE POLYMER COATING
Claim 2
Dependent Claim
164 words
METHOD OF MAKING A VARIABLE DEPTH POSITIVE, CONTOUR, IMAGE ON A SUBSTRATE WHICH COMPRISES COATING THE SUBSTRATE WITH A PHOTOPOLYMERIZABLE COATING COMPOSITION CONTAINING (1) A NON-GASEOUS ETHYLENICALLY UNSATURATED COMPOUND CAPABLE OF ADDITION POLYMERIZATION BY FREE-RADICAL INITIATED CHAIN PROPAGATION, (2) 0.001 TI 1.0 PART BY WEIGHT PER PART OF POLYMERIZABLE COMPOUND OF AN ORGANIC LIGHT-SENSITIVE FREE-RADICAL GENERATING SYSTEM, AND (3) 0.1 TO 10 PERCENT BY WEIGHT BASED ON THE COATING COMPOSITION OF A PHOTODISSOCIABLE NITROSO DIMER HAVING A DISSOCIATION CONSTANT OF 10**-2 TO 10**10 AND A DISSOCIATION HALF-LIFE OF AT LEAST 30 SECONDS IN SOLUTION AT 25*C EXPOSING THE PHOTO-POLYNERIZABLE COATING TO LIGHT HAVING WAVELENGTHS BOTH ABOVE 3400A WHICH EFFECT POLYMERIZATION AND BELOW 3400A WHICH DIISOCIATE NITROSO DIMER TO NITROSO MONOMER, THROUGH A TRANSPARENT FILM OF VARIABLE OPTICAL DENSITY TO LIGHT HAVING A WAVELENGTH OF LESS THAN 3400A AND TRANSPARENT TO LIGHT HAVING A WAVELENGTH ABOVE 3400A, AND DEVELOPING A VARIABLE DEPTH, POSITIVE, POLYMERIC, CONTOUR IMAGE BY REMOVING THE NONPOLYMERIZED PORTION OF THE POLYMER COATING
Claim 3
Dependent Claim
22 words
The method of claim 1 in which the polymerizable compound is an unsaturated ester of a polyol and an Alpha -methylenecarboxylic acid.
Claim 4
Dependent Claim
14 words
The method of claim 2 in which the polymerizable compound is an acrylic ester.
Claim 5
Dependent Claim
31 words
The method of claim 3 in which the coating composition contains 0.01 to 0.7 part by weight per part of polymerizable compound of a benzoin ether as the free-radical generating system.
Claim 6
Dependent Claim
15 words
The method of claim 4 in which the free-radical generating system is benzoin methyl ether.
Claim 7
Dependent Claim
25 words
The method of claim 4 in which the coating composition contains 0.2 to 2 percent by weight based on the coating composition of 2,4-dimethyl-2-nitroso-3-pentanone dimer.
Claim 8
Dependent Claim
25 words
The method of claim 4 in which the coating composition contains 0.2 to 2 percent by weight based on the coating composition of nitrosocyclohexane dimer.
Claim 9
Dependent Claim
25 words
The method of claim 4 in which the coating composition contains 0.2 to 2 percent by weight based on the coating composition of 1-nitroso-3-methylcyclohexane dimer.
Claim 10
Dependent Claim
25 words
The method of claim 4 in which the coating composition contains 0.2 to 2 percent by weight based on the coating composition of 2-nitroso-3-methylbutane dimer.