Patent US3947474A successfully refreshed from Google Patents.
← Back to Patent Explorer
US3947474A Expired / Lapsed US ⏱️ 0.0 years remaining

Catalyst and use thereof

Assignee: Scientific Design LLC
•
Filing: 1974-01-15
•
Granted: 1976-03-30
•
Expires: 1994-01-15
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract A catalyst useful for the oxidation of organic compounds, particularly vapor-phase oxidation of benzene with molecular oxygen to produce maleic anhydride, comprises the oxides of molybdenum, vanadium, phosphorus, sodium and boron in combination with an oxide of at least one metal of the group consisting of manganese, tin, tungsten and bismuth, and preferably also in combination with an oxide of at least one member of the group consisting of iron, cobalt and nickel.

Inventors

  • 👤 Robert S. Barker

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-02 18:01
CPC Classifications
B; B01; B01J; B01J23/00; B01J23/70; B01J23/76; B01J23/84; B01J23/85; B01J23/88; B01J23/887; B01J23/8872; B01J23/16; B01J23/24; B01J23/28; B01J23/30; B01J23/31; B01J23/32; B01J23/8875; B01J23/8876; B01J23/8877; B01J27/00; B01J27/14; B01J27/186; B01J27/195; B01J27/198; B01J27/199; C; C07; C07C; C07C51/00; C07C51/16; C07C51/31; C07C51/313; B01J2523/00

Claims Analysis

Total Claims: 5
Claim 1
Independent Claim 123 words
A process for the preparation of maleic anhydride which comprises oxidizing benzene in the vapor-phase with molecular oxygen in the oxygen in the presence of a catalyst consisting essentially of oxides of molybdenum, vanadium, phosphorus, sodium and boron in combination with an oxide of at least one metal selected from the group consisting of manganese, tin, tungsten and bismuth, the relative amounts of said oxides expressed as Mo, V, P, Na, B, Mn, Sn, W and Bi, being per mol of V, 0.1 to 95 mol Mo, 0.01 to 0.5 mol P, 0.02 to 0.6 mol Na, 0.005 to 0.3 mol B, 0.005 to 0.1 mol Mn, 0.005 to 0.1 mol Sn, 0.005 to 0.1 mol W, and 0.005 to 0.1 mol Bi.
Claim 2
Dependent Claim 123 words
A process for the preparation of maleic anhydride which comprises oxidizing benzene in the vapor-phase with molecular oxygen in the oxygen in the presence of a catalyst consisting essentially of oxides of molybdenum, vanadium, phosphorus, sodium and boron in combination with an oxide of at least one metal selected from the group consisting of manganese, tin, tungsten and bismuth, the relative amounts of said oxides expressed as Mo, V, P, Na, B, Mn, Sn, W and Bi, being per mol of V, 0.1 to 95 mol Mo, 0.01 to 0.5 mol P, 0.02 to 0.6 mol Na, 0.005 to 0.3 mol B, 0.005 to 0.1 mol Mn, 0.005 to 0.1 mol Sn, 0.005 to 0.1 mol W, and 0.005 to 0.1 mol Bi.
Claim 3
Dependent Claim 33 words
A process as defined in claim 1, wherein said catalyst further contains 0.005 to 0.1 mol of an oxide of at least one member of the group consisting of cobalt, nickel or iron.
Claim 4
Dependent Claim 119 words
A process for the preparation of maleic anhydride which comprises oxidizing benzene in the vapor-phase with molecular oxygen in the presence of a molybdenum oxide-vanadium oxide-phosphorus oxide-sodium oxide-boron oxide catalyst wherein said molybdenum oxide, vanadium oxide, phosphorus oxide, sodium oxide and boron oxide, expressed as Mo, V, P, Na and B, are present per mol of V in the amount of 0.1 to 0.95 mol Mo, 0.01 to 0.5 mol P, 0.02 to 0.6 mol Na and 0.005 to 0.3 mol B, and in combination with said catalyst a small amount of an oxide of at least one metal selected from the group consisting of manganese, tin, tungsten and bismuth, effective to prolong the active life of said catalyst.
Claim 5
Dependent Claim 119 words
A process for the preparation of maleic anhydride which comprises oxidizing benzene in the vapor-phase with molecular oxygen in the presence of a molybdenum oxide-vanadium oxide-phosphorus oxide-sodium oxide-boron oxide catalyst wherein said molybdenum oxide, vanadium oxide, phosphorus oxide, sodium oxide and boron oxide, expressed as Mo, V, P, Na and B, are present per mol of V in the amount of 0.1 to 0.95 mol Mo, 0.01 to 0.5 mol P, 0.02 to 0.6 mol Na and 0.005 to 0.3 mol B, and in combination with said catalyst a small amount of an oxide of at least one metal selected from the group consisting of manganese, tin, tungsten and bismuth, effective to prolong the active life of said catalyst.

References Cited (Backward Citations)

DE1965401A1 Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1979-03-30 1979-09-29 1980-03-30 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1983-03-30 1983-09-29 1984-03-30 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1987-03-30 1987-09-29 1988-03-30 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag