Abstract

Abstract Copper ore is leached by static leaching methods, and the effluent pregnant leach liquor is divided into portions forming a high-concentration pregnant leach liquor and a recycleable leach liquor.

Inventors

  • 👤 John C. Stauter
  • 👤 Gerald F. Pace

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-30 14:52
CPC Classifications
C; C22; C22B; C22B15/00; C22B15/0063; C22B15/0065; C22B15/0067; C22B15/0071; C22B15/0084; C22B15/0089; Y; Y02; Y02P; Y02P10/00; Y02P10/20

Claims Analysis

Total Claims: 9
Claim 1
Independent Claim 165 words
A process for static leaching copper mineral values from a source material selected from ore, scrap, and combinations thereof containing copper in the presence of at least one other metal selected from iron and aluminum and for producing a high copper concentration pregnant leach liquor comprising sizing said source material, placing said source material in a vessel, adding an aqueous acid leach solution containing an initial acid concentration of at least about 1 percent acid by weight to said source material and percolating said acid leach solution through said source material in a volume sufficient to cover said source material, adding a sweep solution to said source material to displace said acid leach solution, recovering an effluent pregnant leach liquor from said source material, and segregating about the first 10-30 volume percent of effluent pregnant leach liquor forming a concentrated pregnant leach liquor from the last 70-90 volume percent of effluent pregnant leach liquor and recycling said last 70-90 volume percent effluent pregnant leach liquor.
Claim 2
Dependent Claim 165 words
A process for static leaching copper mineral values from a source material selected from ore, scrap, and combinations thereof containing copper in the presence of at least one other metal selected from iron and aluminum and for producing a high copper concentration pregnant leach liquor comprising sizing said source material, placing said source material in a vessel, adding an aqueous acid leach solution containing an initial acid concentration of at least about 1 percent acid by weight to said source material and percolating said acid leach solution through said source material in a volume sufficient to cover said source material, adding a sweep solution to said source material to displace said acid leach solution, recovering an effluent pregnant leach liquor from said source material, and segregating about the first 10-30 volume percent of effluent pregnant leach liquor forming a concentrated pregnant leach liquor from the last 70-90 volume percent of effluent pregnant leach liquor and recycling said last 70-90 volume percent effluent pregnant leach liquor.
Claim 3
Dependent Claim 200 words
A process for static leaching copper mineral values from a source material comprising sizing said source material, contacting a first portion of said source material with an acid leach solution by adding said solution to said source material and percolating said acid leach solution through said source material, adding a sweep solution to said source material to displace said acid leach solution, recovering an effluent pregnant leach liquor from said source material, segregating the first portion of effluent pregnant leach liquor forming a first portion of concentrated pregnant leach liquor from the last portion of said effluent leach liquor forming a first portion of recycle leach liquor, contacting a second portion of said source material with said recycle acid leach solution by adding said recycle leach liquor to said source material and percolating said leach liquor through said source material, adding a sweep solution to said source material to displace said acid leach solution, recovering an effluent pregnant leach liquor from said source material, and segregating the first portion of effluent pregnant leach liquor forming a second portion of concentrated pregnant leach liquor from the last portion of said effluent leach liquor forming a second portion of recycle leach liquor.
Claim 4
Dependent Claim 200 words
A process for static leaching copper mineral values from a source material comprising sizing said source material, contacting a first portion of said source material with an acid leach solution by adding said solution to said source material and percolating said acid leach solution through said source material, adding a sweep solution to said source material to displace said acid leach solution, recovering an effluent pregnant leach liquor from said source material, segregating the first portion of effluent pregnant leach liquor forming a first portion of concentrated pregnant leach liquor from the last portion of said effluent leach liquor forming a first portion of recycle leach liquor, contacting a second portion of said source material with said recycle acid leach solution by adding said recycle leach liquor to said source material and percolating said leach liquor through said source material, adding a sweep solution to said source material to displace said acid leach solution, recovering an effluent pregnant leach liquor from said source material, and segregating the first portion of effluent pregnant leach liquor forming a second portion of concentrated pregnant leach liquor from the last portion of said effluent leach liquor forming a second portion of recycle leach liquor.
Claim 5
Dependent Claim 262 words
A process for static leaching copper mineral values from a source material selected from ore, scrap, and combinations thereof containing copper in the presence of at least one other metal selected from iron and aluminum and for producing a high copper concentration pregnant leach liquor comprising sizing said source material, placing said source material in a vessel, adding an acid leach solution containing at least about 1 percent acid by weight to said source material and percolating said acid leach solution through said source material in a volume sufficient to cover said source material, adding a sweep solution to said source material to displace said acid leach solution, recovering an effluent pregnant leach liquor from said source material, segregating about the first 10-30 volume percent of effluent pregnant leach liquor forming a concentrated pregnant leach liquor from the last 70-90 volume percent of effluent pregnant leach liquor forming a recycle leach liquor, adjusting the acid concentration of said recycle leach liquor to an acid concentration approximately equal to said initial acid concentration, adding said recycle leach liquor to source material in a second vessel and percolating said acid leach solution through said source material in a volume sufficient to cover said source material, adding a sweep solution to said source material to displace said acid leach solution, recovering an effluent pregnant leach liquor from said source material, and segregating about the first 10-30 volume percent of effluent pregnant leach liquor forming a concentrated pregnant leach liquor from the last 70-90 volume percent of effluent pregnant leach liquor forming a recycle leach liquor.
Claim 6
Dependent Claim 262 words
A process for static leaching copper mineral values from a source material selected from ore, scrap, and combinations thereof containing copper in the presence of at least one other metal selected from iron and aluminum and for producing a high copper concentration pregnant leach liquor comprising sizing said source material, placing said source material in a vessel, adding an acid leach solution containing at least about 1 percent acid by weight to said source material and percolating said acid leach solution through said source material in a volume sufficient to cover said source material, adding a sweep solution to said source material to displace said acid leach solution, recovering an effluent pregnant leach liquor from said source material, segregating about the first 10-30 volume percent of effluent pregnant leach liquor forming a concentrated pregnant leach liquor from the last 70-90 volume percent of effluent pregnant leach liquor forming a recycle leach liquor, adjusting the acid concentration of said recycle leach liquor to an acid concentration approximately equal to said initial acid concentration, adding said recycle leach liquor to source material in a second vessel and percolating said acid leach solution through said source material in a volume sufficient to cover said source material, adding a sweep solution to said source material to displace said acid leach solution, recovering an effluent pregnant leach liquor from said source material, and segregating about the first 10-30 volume percent of effluent pregnant leach liquor forming a concentrated pregnant leach liquor from the last 70-90 volume percent of effluent pregnant leach liquor forming a recycle leach liquor.
Claim 7
Dependent Claim 21 words
The process of claim 3 wherein the source material is an oxide ore and the acid leach solution is sulfuric acid.
Claim 8
Dependent Claim 199 words
A process for static leaching copper mineral values from a source material comprising sizing said source material, contacting a portion of said source material with an acid leach solution by adding said solution to said source material and percolating said acid leach solution through said source material, adding a sweep solution to said source material to displace said acid leach solution, recovering an effluent pregnant leach liquor from said source material, segregating the first portion of effluent pregnant leach liquor forming a first portion of concentrated pregnant leach liquor from the last portion of said effluent leach liquor forming a first portion of recycle leach liquor, contacting of a portion of said source material with said recycle acid leach solution by adding said recycle leach liquor to said source material and percolating said leach liquor through said source material, adding a sweep solution to said source material to displace said acid leach solution, recovering an effluent pregnant leach liquor from said source material, and segregating the first portion of effluent pregnant leach liquor forming a second portion of concentrated pregnant leach liquor from the last portion of said effluent leach liquor forming a second portion of recycle leach liquor.
Claim 9
Dependent Claim 199 words
A process for static leaching copper mineral values from a source material comprising sizing said source material, contacting a portion of said source material with an acid leach solution by adding said solution to said source material and percolating said acid leach solution through said source material, adding a sweep solution to said source material to displace said acid leach solution, recovering an effluent pregnant leach liquor from said source material, segregating the first portion of effluent pregnant leach liquor forming a first portion of concentrated pregnant leach liquor from the last portion of said effluent leach liquor forming a first portion of recycle leach liquor, contacting of a portion of said source material with said recycle acid leach solution by adding said recycle leach liquor to said source material and percolating said leach liquor through said source material, adding a sweep solution to said source material to displace said acid leach solution, recovering an effluent pregnant leach liquor from said source material, and segregating the first portion of effluent pregnant leach liquor forming a second portion of concentrated pregnant leach liquor from the last portion of said effluent leach liquor forming a second portion of recycle leach liquor.

References Cited (Backward Citations)

US650019A Cited
US899146A Cited
US1131986A Cited
US1581479A Cited
US3840365A Cited
US3777003A Cited
US3863002A Cited
US3801694A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1980-03-21 1980-09-20 1981-03-22 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1984-03-21 1984-09-20 1985-03-22 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1988-03-21 1988-09-20 1989-03-22 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag