US4124401A
Expired / Lapsed
US
⏱️ 0.0 years remaining
Polycrystalline diamond body
Assignee: General Electric Co
•
Filing: 1977-10-21
•
Granted: 1978-11-07
•
Expires: 1997-10-21
Abstract
Abstract A mass of diamond crystals in contact with a mass of eutectiferous silicon-rich alloy are disposed in a container and placed within a pressure transmitting powder medium. Pressure is applied to the powder medium resulting in substantially isostatic pressure being applied to the container and its contents sufficient to dimensionally stabilize the container and its contents. The resulting shaped substantially isostatic system of powder-enveloped container is hot-pressed whereby fluid eutectiferous silicon-rich alloy is produced and infiltrated through the interstices between the diamond crystals producing, upon cooling, an adherently bonded integral body.
Inventors
- 👤 Minyoung Lee
- 👤 Lawrence E. Szala
- 👤 Robert C. DeVries
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-10-24 15:14
CPC Classifications
C; C04; C04B; C04B35/00; C04B35/622; C04B35/64; C04B35/645; B; B01; B01J; B01J3/00; B01J3/06; B01J3/062; C04B35/515; C04B35/52; C04B35/626; C04B35/63; C04B35/6303; C04B35/6316; B01J2203/00; B01J2203/06; B01J2203/0605; B01J2203/062; B01J2203/065; B01J2203/0655; B01J2203/0675; B01J2203/0685; B22; B22F; B22F5/00; B22F2005/001; C04B2235/00; C04B2235/02; C04B2235/30; C04B2235/38; C04B2235/3817; C04B2235/3826; C04B2235/3839; C04B2235/3843; C04B2235/3847; C04B2235/3891; C04B2235/40; C04B2235/404; C04B2235/405; C04B2235/408; C04B2235/42; C04B2235/422; C04B2235/427; C04B2235/428; C04B2235/50; C04B2235/54; C04B2235/5418; C04B2235/5436; C04B2235/5463; C04B2235/5472; C04B2235/60; C04B2235/616; C04B2235/65; C04B2235/658; C04B2235/6587; C04B2235/70; C04B2235/72; C04B2235/721; C04B2235/728; C04B2235/80; C04B2235/96
Claims Analysis
Total Claims: 11
Claim 1
Independent Claim
143 words
A polycrystalline diamond body comprised of a mass of diamond crystals adherently bonded together by a silicon atom-containing bonding medium comprised of silicon carbide and a carbide and/or silicide of a metal component which forms a silicide with silicon, said diamond crystals ranging in size from about 1 micron to about 1000 microns, the density of said diamond crystals ranging from at least about 70% by volume up to about but less than 90% by volume of said body, said silicon atom-containing bonding medium being present in an amount ranging up to about 30% by volume of said body, said bonding medium being distributed at least substantially uniformly throughout said body, the portion of said bonding medium in contact with the surfaces of said diamond crystals being at least in a major amount silicon carbide, said diamond body being at least substantially pore-free.
Claim 2
Dependent Claim
143 words
A polycrystalline diamond body comprised of a mass of diamond crystals adherently bonded together by a silicon atom-containing bonding medium comprised of silicon carbide and a carbide and/or silicide of a metal component which forms a silicide with silicon, said diamond crystals ranging in size from about 1 micron to about 1000 microns, the density of said diamond crystals ranging from at least about 70% by volume up to about but less than 90% by volume of said body, said silicon atom-containing bonding medium being present in an amount ranging up to about 30% by volume of said body, said bonding medium being distributed at least substantially uniformly throughout said body, the portion of said bonding medium in contact with the surfaces of said diamond crystals being at least in a major amount silicon carbide, said diamond body being at least substantially pore-free.
Claim 3
Dependent Claim
16 words
The polycrystalline diamond body according to claim 1 wherein said bonding medium also contains elemental silicon.
Claim 4
Dependent Claim
27 words
The polycrystalline diamond body according to claim 1 wherein the density of said diamond crystals ranges from about 70% to about 89% by volume of said body.
Claim 5
Dependent Claim
22 words
The polycrystalline diamond body according to claim 1 wherein said crystals are size-graded ranging from about 1 micron to about 60 microns.
Claim 6
Dependent Claim
21 words
The polycrystalline diamond body according to claim 1 wherein said bonding medium is comprised of silicon carbide and said metal silicide.
Claim 7
Dependent Claim
15 words
The polycrystalline diamond body according to claim 5 wherein said bonding medium contains elemental silicon.
Claim 8
Dependent Claim
47 words
The polycrystalline diamond body according to claim 5 wherein the metal component of said metal silicide is selected from the group consisting of cobalt, chromium, iron, hafnium, manganese, molybdenum, niobium, nickel, palladium, platinum, rhenium, rhodium, ruthenium, tantalum, thorium, titanium, uranium, vanadium, tungsten, yttrium, zirconium and alloys thereof.
Claim 9
Dependent Claim
21 words
The polycrystalline diamond body according to claim 1 wherein said bonding medium is comprised of silicon carbide and said metal carbide.
Claim 10
Dependent Claim
15 words
The polycrystalline diamond body according to claim 8 wherein said bonding medium contains element silicon.
Claim 11
Dependent Claim
34 words
The polycrystalline diamond body according to claim 8 wherein said metal component of said metal carbide is selected from the group consisting of chromium, hafnium, titanium, zirconium, tantalum, vanadium, tungsten, molybdenum and alloys thereof.
References Cited (Backward Citations)
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1981-11-06 | 1982-05-08 | 1982-11-07 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 1985-11-06 | 1986-05-08 | 1986-11-07 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 1989-11-06 | 1990-05-08 | 1990-11-07 | $7700.00 | Window Closed / Lapsed |