High selectivity thin film polarizer

Assignee: The AT&T MVPD Group LLC
•
Filing: 1979-07-02
•
Granted: 1981-09-15
•
Expires: 1999-07-02
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract A thin film polarizer for dividing electromagnetic energy into two mutually orthogonal components with a high degree of selectivity. A plurality of wire grids having an interelement spacing of less than one wavelength is supported by a substrate of electrically insulative material. The substrate is invisible to the wavelength of the polarized electromagnetic energy. The planar wire grids are substantially parallel and spaced less than one wavelength therebetween to achieve an efficient and compact thin film polarizer. The process of this invention for forming the plurality of wire grids comprises photolithographically defining each grid layer by the interference pattern of at least two coherent beams such as laser beams, one forming step being required for each grid, an anti-reflective layer being inserted between adjacent grid layers.

Inventors

  • 👤 Hugh L. Garvin
  • 👤 Douglas A. Pinnow

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-30 16:49
CPC Classifications
G; G02; G02B; G02B5/00; G02B5/30; G02B5/3025; G02B5/3058; Y; Y10; Y10S; Y10S359/00; Y10S359/90

Claims Analysis

Total Claims: 5
Claim 1
Independent Claim 118 words
A method for making a thin film polarizer on a substrate surface comprising: placing a first metal layer on said surface; first photolithographically forming a grid in said first metal layer defined by the interference pattern of at least two coherent beams; placing an insulating layer over said first metal layer; placing a second metal layer over said insulating layer; placing an anti-reflective coating over said second layer; placing a photoresistive layer over said anti-reflective coating; and second photolithographically forming a grid in said second metal layer defined by the interference pattern of at least two coherent beams, wherein said anti-reflective coating substantially prevents formation of standing waves within said photoresistive layer during said second photolithographic forming step.
Claim 2
Independent Claim 118 words
A method for making a thin film polarizer on a substrate surface comprising: placing a first metal layer on said surface; first photolithographically forming a grid in said first metal layer defined by the interference pattern of at least two coherent beams; placing an insulating layer over said first metal layer; placing a second metal layer over said insulating layer; placing an anti-reflective coating over said second layer; placing a photoresistive layer over said anti-reflective coating; and second photolithographically forming a grid in said second metal layer defined by the interference pattern of at least two coherent beams, wherein said anti-reflective coating substantially prevents formation of standing waves within said photoresistive layer during said second photolithographic forming step.
Claim 3
Dependent Claim 17 words
The method of claim 1 wherein said antireflective layer is removed after said second photolithographically forming step.
Claim 4
Dependent Claim 57 words
The method of claim 1 wherein said second forming step comprises forming a grid in said second metal layer which is sufficiently nearly parallel to said grid in said first metal layer formed during said first forming step so that the extinction ratio across the two grids is proportional to the product of their individual extinction ratios.
Claim 5
Dependent Claim 73 words
The method of claim 1 wherein said first and second photolithographic forming steps comprise forming said grids so as to have a grid spacing less the the wave length λ of incident radiation to be polarized, said forming steps further comprising forming said grids so that they are sufficiently nearly parallel to one another so that the extinction ratio across the two grids is proportional to the product of their individual extinction ratios.

References Cited (Backward Citations)

US3271771A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1984-09-14 1985-03-16 1985-09-15 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1988-09-14 1989-03-16 1989-09-15 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1992-09-14 1993-03-16 1993-09-15 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag