Abstract

Abstract A process is disclosed for increasing the silica to alkali metal oxide weight ratio of aqueous alkali metal silicate solution by electrodialysis of the alkali metal silicate solution.

Inventors

  • 👤 William W. Carlin
  • 👤 Douglas W. McCann

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-01 21:58
CPC Classifications
C; C01; C01B; C01B33/00; C01B33/20; C01B33/32

Claims Analysis

Total Claims: 5
Claim 1
Independent Claim 231 words
A process for increasing the silica:alkali metal oxide weight ratio of aqueous alkali metal silicate solution comprising: (a) providing an electrolytic cell having a cathode compartment and an associated cathode and an anode compartment and an associated anode, said compartments separated by a cation selective permionic membrane; (b) charging aqueous alkali metal silicate solution to the anode compartment, said solution having a silica: alkali metal oxide weight ratio of up to about 2.5:1, a pH of at least 11, whereby to maintain the solution free of colloidal suspension or sol of finely divided silica particles, and a water content of at least 75 percent by weight; (c) charging water or aqueous alkali metal hydroxide solution to the cathode compartment; (d) applying a direct current across the cell to decompose alkali metal oxide at the anode into alkali metal ions and gaseous oxygen and to cause said alkali metal ions to migrate from the anode compartment through the membrane into the cathode compartment therein forming alkali metal hydroxide; (e) withdrawing aqueous alkali metal silicate solution from the anode compartment, said solution having a silica: alkali metal oxide weight ratio of about 3:1 to about 4.5:1 and a pH greater than 10, whereby to maintain the solution free of colloidal suspension or sol of finely divided silica particles; and (f) withdrawing alkali metal hydroxide from and adding make-up water to the cathode compartment.
Claim 2
Dependent Claim 231 words
A process for increasing the silica:alkali metal oxide weight ratio of aqueous alkali metal silicate solution comprising: (a) providing an electrolytic cell having a cathode compartment and an associated cathode and an anode compartment and an associated anode, said compartments separated by a cation selective permionic membrane; (b) charging aqueous alkali metal silicate solution to the anode compartment, said solution having a silica: alkali metal oxide weight ratio of up to about 2.5:1, a pH of at least 11, whereby to maintain the solution free of colloidal suspension or sol of finely divided silica particles, and a water content of at least 75 percent by weight; (c) charging water or aqueous alkali metal hydroxide solution to the cathode compartment; (d) applying a direct current across the cell to decompose alkali metal oxide at the anode into alkali metal ions and gaseous oxygen and to cause said alkali metal ions to migrate from the anode compartment through the membrane into the cathode compartment therein forming alkali metal hydroxide; (e) withdrawing aqueous alkali metal silicate solution from the anode compartment, said solution having a silica: alkali metal oxide weight ratio of about 3:1 to about 4.5:1 and a pH greater than 10, whereby to maintain the solution free of colloidal suspension or sol of finely divided silica particles; and (f) withdrawing alkali metal hydroxide from and adding make-up water to the cathode compartment.
Claim 3
Dependent Claim 37 words
The process of claim 1 wherein the aqueous alkali metal silicate solution charged to the anode compartment in aqueous sodium silicate solution and the alkali metal hydroxide solution charged to the cathode compartment is sodium hydroxide solution.
Claim 4
Dependent Claim 29 words
The process of claim 1 wherein the aqueous alkali metal silicate solution charged to the anode compartment has a water content of at least about 90 percent by weight.
Claim 5
Dependent Claim 31 words
The process of claim 1 wherein the aqueous alkali metal silicate solution charged to the anode compartment has a silica:alkali metal oxide weight ratio of from about 2:1 to about 2.5:1.

References Cited (Backward Citations)

US1557491A Cited
US1562940A Cited
US2223929A Cited
US3654105A Cited
US3645865A Cited
US3668088A Cited
US3712941A Cited
US3734842A Cited
US3723273A Cited
US4147605A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1984-11-30 1985-06-01 1985-12-01 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1988-11-30 1989-06-01 1989-12-01 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1992-11-30 1993-06-01 1993-12-01 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag