Abstract

Abstract Heavy Metals contained in industrial waste streams are removed therefrom by flocculation using a source of ferric ions and an alkaline material at a basic pH. Both the flocculated heavy metals and the coagulant chemicals are recovered by acidifying the floc to a pH of between 3.2 and 3.7. This liberates the heavy metals back into solution but does not destroy the floc particles. After separation and removal of the concentrated heavy metal solution, the floc is further acidified to completely dissolve it. This dissolved ferric ion containing solution may then be reused to treat succeeding portions of heavy metal containing waste streams. The concentrated heavy metals solution may also be recycled or the metals contained therein recovered for reuse or disposed of in an acceptable manner.

Inventors

  • 👤 James E. Etzel
  • 👤 Praveen Anand

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-08 20:48
CPC Classifications
C; C02; C02F; C02F9/00; C02F1/00; C02F1/52; C02F1/5236; C02F2101/00; C02F2101/10; C02F2101/20; Y; Y10; Y10S; Y10S210/00; Y10S210/902; Y10S210/911; Y10S210/912; Y10S210/913

Claims Analysis

Total Claims: 7
Claim 1
Independent Claim 194 words
A method of treating an industrial aqueous waste stream containing one or more ionized heavy metal compounds of the type releasable from a ferric hydroxide flocculant at a pH of about 3.2 to 3.7 to remove such ionized heavy metal compounds comprising the steps of: (a) adding a source of ferric ions and an alkaline material to said waste stream in amounts sufficient to raise the pH of the stream to about 10.2 or above and mixing to form a ferric hydroxide flocculent, whereby said flocculent binds said heavy metal compounds to yield a flocculated material containing said heavy metal compounds, (b) settling and separating the flocculated material from the stream, (c) acidifying said flocculated material by addition of an acid in an amount sufficient to lower the pH to about 3.2 to 3.7 and mixing whereby heavy metals bound by said flocculent are released into solution, (d) removing the heavy metal containing solution from said flocculent, (e) regenerating said flocculent by addition of an acid in an amount sufficient to lower the pH to about 3 or less and mixing to dissolve the flocculent and (f) recycling said dissolved flocculent to step (a).
Claim 2
Independent Claim 194 words
A method of treating an industrial aqueous waste stream containing one or more ionized heavy metal compounds of the type releasable from a ferric hydroxide flocculant at a pH of about 3.2 to 3.7 to remove such ionized heavy metal compounds comprising the steps of: (a) adding a source of ferric ions and an alkaline material to said waste stream in amounts sufficient to raise the pH of the stream to about 10.2 or above and mixing to form a ferric hydroxide flocculent, whereby said flocculent binds said heavy metal compounds to yield a flocculated material containing said heavy metal compounds, (b) settling and separating the flocculated material from the stream, (c) acidifying said flocculated material by addition of an acid in an amount sufficient to lower the pH to about 3.2 to 3.7 and mixing whereby heavy metals bound by said flocculent are released into solution, (d) removing the heavy metal containing solution from said flocculent, (e) regenerating said flocculent by addition of an acid in an amount sufficient to lower the pH to about 3 or less and mixing to dissolve the flocculent and (f) recycling said dissolved flocculent to step (a).
Claim 3
Dependent Claim 26 words
The method of claim 1 in which said source of ferric ions is selected from the group consisting of ferric chloride, ferric sulfate, and mixtures thereof.
Claim 4
Dependent Claim 28 words
The method of claim 2 in which said alkaline material is selected from the group consisting of sodium hydroxide, calcium hydroxide, sodium carbonate, calcium carbonate, and mixtures thereof.
Claim 5
Dependent Claim 19 words
The method of claim 1 including the step of recycling the stream from step (b) to an industrial process.
Claim 6
Dependent Claim 22 words
The method of claim 1 including the step of recovering the heavy metals from step (d) for reuse in an industrial process.
Claim 7
Dependent Claim 39 words
The method of claim 1 including the step of passing the removed heavy metals from step (d) through a packed bed of vermiculite particles having a cation-exchange capacity in order to capture said heavy metals on said vermiculite particles.

References Cited (Backward Citations)

US2128569A Cited
US3347786A Cited
US3494864A Cited
US3800024A Cited
US3725266A Cited
US4163716A Cited
JPS5162182A Cited
US4040955A Cited
JPS55107742A Cited
US4210530A Cited
US4222872A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1985-08-09 1986-02-08 1986-08-10 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1989-08-09 1990-02-08 1990-08-10 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1993-08-09 1994-02-08 1994-08-10 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag