Patent US4396446A successfully refreshed from Google Patents.
← Back to Patent Explorer
US4396446A Expired / Lapsed US ⏱️ 0.0 years remaining

Method for producing an optical telecommunication element

Assignee: US Philips Corp
•
Filing: 1981-01-08
•
Granted: 1983-08-02
•
Expires: 2001-01-08
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract An optical communication element comprises an optical fiber bonded in a state of axial compression to a metal tape. The tape may be folded up into a tube and sealed by soldering. Such elements are strong and not sensitive to stress corrosion. Such an optical communication element may be produced by passing a metal tape and an optical fiber in contact around a drum with the optical fiber on the outside. An adhesive, which solidifies or cures during the passage around the drum is applied to the metal tape.

Inventors

  • 👤 Adrianus J. J. Franken

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-30 09:00
CPC Classifications
G; G02; G02B; G02B6/00; G02B6/44; G02B6/4479; G02B6/4401; G02B6/4403; G02B6/441; Y; Y10; Y10T; Y10T156/00; Y10T156/10; Y10T156/1002; Y10T156/1007; Y10T156/1008; Y10T156/1013; Y10T29/00; Y10T29/51; Y10T29/5185

Claims Analysis

Total Claims: 9
Claim 1
Independent Claim 156 words
A method of producing an optical communication element comprising at least one optical fiber bonded to a metal tape, said method comprising the steps of: providing a metal tape having first and second opposite sides; applying an uncured adhesive layer to the first side of the metal tape; contacting an optical fiber to the adhesive on the first side of the metal tape; passing the metal tape around a drum, the second side of the tape contacting the drum; and curing the adhesive during its passage around the drum; characterized in that the drum has a diameter, the metal tape has a thickness, and the optical fiber has a diameter, all of which are chosen so that the metal tape has a path length around the drum which is at least 0.5 parts per thousand shorter than the path length of the optical fiber around the drum, thus providing axial compression in the adhered optical fiber.
Claim 2
Independent Claim 156 words
A method of producing an optical communication element comprising at least one optical fiber bonded to a metal tape, said method comprising the steps of: providing a metal tape having first and second opposite sides; applying an uncured adhesive layer to the first side of the metal tape; contacting an optical fiber to the adhesive on the first side of the metal tape; passing the metal tape around a drum, the second side of the tape contacting the drum; and curing the adhesive during its passage around the drum; characterized in that the drum has a diameter, the metal tape has a thickness, and the optical fiber has a diameter, all of which are chosen so that the metal tape has a path length around the drum which is at least 0.5 parts per thousand shorter than the path length of the optical fiber around the drum, thus providing axial compression in the adhered optical fiber.
Claim 3
Dependent Claim 24 words
A method as claimed in claim 1, characterized in that the uncured adhesive is a molten hot melt adhesive which is cured by solidification.
Claim 4
Dependent Claim 66 words
A method as claimed in claim 2, characterized in that the drum does not rotate, the metal tape is fed onto the drum at a feeder portion of the drum, the metal tape leaves the drum at a discharge portion of the drum, and the method further comprises the steps of: heating the drum at the feeder portion; and cooling the drum at the discharge portion.
Claim 5
Dependent Claim 37 words
A method as claimed in claim 3, characterized in that after the adhesive is cured, the method further comprises the steps of: folding the metal tape to form a tube; and sealing the folded tape by soldering.
Claim 6
Dependent Claim 28 words
A method as claimed in claim 4, characterized in that the method further comprises the step of filling the tube formed by the metal tape with a foam.
Claim 7
Dependent Claim 28 words
A method as claimed in claim 4, characterized in that the method further comprises the step of filling the tube formed by the metal tape with a gel.
Claim 8
Dependent Claim 29 words
A method as claimed in claim 1, characterized in that the metal tape is an iron-nickel alloy with 36 weight % nickel, and the optical fiber is quartz glass.
Claim 9
Dependent Claim 46 words
A method as claimed in claim 1, characterized in that the metal tape is an iron-chromium alloy with 17 to 19 weight % chromium, and the optical fiber is made of a glass having a coefficient of thermal expansion of 9 to 11×10 -6 ° C.

References Cited (Backward Citations)

US3751623A Cited
US3813098A Cited
NL7507580A Cited
GB1518082A Cited
CA1065137A Cited
US4146302A Cited
DE2701650A1 Cited
US4289375A Cited
US4184860A Cited
US4138193A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1986-08-01 1987-01-31 1987-08-02 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1990-08-01 1991-01-31 1991-08-02 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1994-08-01 1995-01-31 1995-08-02 $7700.00 Window Closed / Lapsed