Claims Analysis
Total Claims: 14
Claim 1
Independent Claim
97 words
A method for improving the sulfur capture potential of lime in the fluidized bed combustion of coal and for improving the flow characteristics of the feed coal thereto comprising: (a) introducing the gas from fluidized bed combustion of coal which contains particles comprising calcium oxide into a filtering means whereby said particles are collected; (b) mixing said particles with wet coal at a temperature from about 200° F. to about 400° F., thereby drying said coal and hydrating said calcium oxide to form calcium hydroxide; (c) introducing the mixture from step (b) into said fluidized bed combustor.
Claim 2
Independent Claim
97 words
A method for improving the sulfur capture potential of lime in the fluidized bed combustion of coal and for improving the flow characteristics of the feed coal thereto comprising: (a) introducing the gas from fluidized bed combustion of coal which contains particles comprising calcium oxide into a filtering means whereby said particles are collected; (b) mixing said particles with wet coal at a temperature from about 200° F. to about 400° F., thereby drying said coal and hydrating said calcium oxide to form calcium hydroxide; (c) introducing the mixture from step (b) into said fluidized bed combustor.
Claim 3
Dependent Claim
30 words
A method according to claim 1 wherein an amount of water is added to said mixture from step (b) sufficient to complete the conversion of calcium oxide to calcium hydroxide.
Claim 4
Dependent Claim
17 words
A method according to claim 1 wherein said temperature is from about 200° F. to 250° F.
Claim 5
Independent Claim
115 words
A method for improving the sulfur capture potential of lime in the fluidized bed combustion of coal and for improving the flow characteristics of the coal feed therefor comprising: (a) contacting wet coal with gas from fluidized bed combustion of coal thereby drying said coal; (b) conducting the moisture-containing gas resulting from step (a) into a filtering means whereby particles in said gas comprising calcium oxide are collected; (c) exposing said collected particles to said moisture containing gas at a temperature from about 200° F. to 400° F., thereby hydrating said calcium oxide to form calcium hydroxide; (d) introducing the particles from step (c) and the coal from step (a) into said fluidized bed combustor.
Claim 6
Independent Claim
115 words
A method for improving the sulfur capture potential of lime in the fluidized bed combustion of coal and for improving the flow characteristics of the coal feed therefor comprising: (a) contacting wet coal with gas from fluidized bed combustion of coal thereby drying said coal; (b) conducting the moisture-containing gas resulting from step (a) into a filtering means whereby particles in said gas comprising calcium oxide are collected; (c) exposing said collected particles to said moisture containing gas at a temperature from about 200° F. to 400° F., thereby hydrating said calcium oxide to form calcium hydroxide; (d) introducing the particles from step (c) and the coal from step (a) into said fluidized bed combustor.
Claim 7
Dependent Claim
22 words
A method according to claim 4 wherein in step (d) said particles and coal are mixed prior to introduction into said combustor.
Claim 8
Dependent Claim
21 words
A method according to claim 4 wherein in step (d) said particles and said coal are separately introduced into said combustor.
Claim 9
Dependent Claim
19 words
A method according to claim 4 wherein in step (b) said filtering means comprises said coal in step (a).
Claim 10
Dependent Claim
17 words
A method according to claim 4 wherein in step (b) said filtering means comprises a fabric filter.
Claim 11
Dependent Claim
17 words
A method according to claim 8 wherein said temperature is from about 200° F. to 250° F.
Claim 12
Independent Claim
90 words
A method for improving the sulfur capture potential of lime in the fluidized bed combustion of coal comprising: (a) introducing moisture-containing gas from fluidized bed combustion of coal which contains particles comprising calcium oxide into a filtering means whereby said particles are collected; (b) retaining said collected particles on said filtering means at a temperature from about 200° F. to 400° F. for a period of time sufficient to substantially hydrate said calcium oxide to form calcium hydroxide; (c) introducing the product from step (b) into said fluidized bed combustor.
Claim 13
Independent Claim
90 words
A method for improving the sulfur capture potential of lime in the fluidized bed combustion of coal comprising: (a) introducing moisture-containing gas from fluidized bed combustion of coal which contains particles comprising calcium oxide into a filtering means whereby said particles are collected; (b) retaining said collected particles on said filtering means at a temperature from about 200° F. to 400° F. for a period of time sufficient to substantially hydrate said calcium oxide to form calcium hydroxide; (c) introducing the product from step (b) into said fluidized bed combustor.
Claim 14
Dependent Claim
23 words
A method according to claim 10 wherein said particles are retained on said filtering means in step (b) for longer than 30 minutes.