Abstract The oxynitride film according to the present invention contains Ga and/or Al and has O/N ratio of at least 0.15. This film is obtained by relying on, for example, chemical vapor deposition technique. The O/N ratio in the film may be varied by, for example, varying the distance between the substrate and the substance-supply source, or by varying the proportion of an oxidizing gas contained in a carrier gas. This film is used either as a surface passivation film of III-V compound semiconductors such as GaAs, or as an insulating film for active surface portions of IG-FET, or as an optical anti-reflective film. This is a division of application Ser. No. 215,442 filed Dec. 11, 1980, now Pat. 4,331,737, which in turn is a continuation of application Ser.No. 23,766, filed Mar. 26, 1979.
An oxynitride film formed of an oxynitride of one substance selected from the group consisting of gallium, aluminum and their mixture, said oxynitride having a finite and non-zero molar ratio of oxygen to nitrogen.
Claim 2
Dependent Claim
34 words
An oxynitride film formed of an oxynitride of one substance selected from the group consisting of gallium, aluminum and their mixture, said oxynitride having a finite and non-zero molar ratio of oxygen to nitrogen.
Claim 3
Dependent Claim
17 words
An oxynitride film according to claim 1, in which said oxygen-to-nitrogen molar ratio is at least 0.15.
Claim 4
Dependent Claim
54 words
An oxynitride film according to claim 1 having the formula GaO x N y , AlO x N y , or Ga x Al y O x N y where x is the atomic fraction of oxygen and y is the atomic fraction of nitrogen based on the total atoms of oxygen and nitrogen.
Claim 5
Dependent Claim
17 words
An oxynitride film according to claim 1, in which said film is formed on an underlying substrate.
Claim 6
Dependent Claim
20 words
An oxynitride film according to claim 4, in which said film serves as an underlying material for of another film.
Claim 7
Dependent Claim
21 words
An oxynitride film according to claim 4, in which said oxygen-to-nitrogen ratio varies in the direction of thickness of said film.
Claim 8
Dependent Claim
27 words
An oxynitride film according to claim 4 wherein the underlying substrate is formed of at least one substance selected from the group consisting of gallium and aluminum.
Claim 9
Dependent Claim
29 words
An oxynitride film according to claim 4 in which said underlying substrate is formed of at least one substance selected from the group consisting of gallium, aluminum and indium.
Claim 10
Dependent Claim
23 words
An oxynitride film according to claim 8, in which said one substance is gallium and said oxygen-to-nitrogen molar ratio is at least 0.15.