Lead frame for molded integrated circuit package
Assignee: Motors Liquidation Co
•
Filing: 1982-09-03
•
Granted: 1985-01-01
•
Expires: 2002-09-03
Abstract
Abstract A lead frame for a molded semiconductor device package. The lead frame has a pattern of finger leads with convergent free inner ends and dam bars between adjacent finger leads. The dam bars are partially severed from their contiguous finger leads due to cuts on their edges intended to face a body member molded over the finger lead inner ends. The partially severed dam bar edge is preferably positioned to be substantially at the periphery of the molded body member. The resultant molded body member can thus have a finished surface even between the finger leads as molded and dam bar cutting die wear reduced.
Inventors
- 👤 Charles T. Eytcheson
- 👤 Phillip A. Lutz
- 👤 Harold L. Fields
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-10-29 15:59
CPC Classifications
H; H10; H10W; H10W70/00; H10W70/40; H10W70/421; H10W70/01; H10W70/04; H10W70/048; H10W74/00; H10W74/01; Y; Y10; Y10T; Y10T29/00; Y10T29/49; Y10T29/49002; Y10T29/49117; Y10T29/49121
Claims Analysis
Total Claims: 4
Claim 1
Independent Claim
174 words
A method of making a semiconductor device package that includes molding a plastic body member over a semiconductor die affixed to inner free ends of a convergent pattern of finger leads of a sheet-like lead frame, the lead frame having integral dam bars transversely connecting finger leads, the improvement of providing a lead frame in which each dam bar has a cut made before the molding operation between each end and a contiguous finger lead extending from an inner facing edge of the dam bar toward but not reaching the opposite dam bar edge, positioning the lead frame in a mold having a package body molding cavity periphery adjacent the dam bar inner facing edge to minimize flash between finger leads during molding, clamping the dam bars between opposed faces on the mold, molding a package body within the cavity without producing a significant web between finger leads, and cutting the balance of each dam bar from each finger lead without encountering excessive cutting die wear due to contact with abrasive body molding material.
Claim 2
Independent Claim
174 words
A method of making a semiconductor device package that includes molding a plastic body member over a semiconductor die affixed to inner free ends of a convergent pattern of finger leads of a sheet-like lead frame, the lead frame having integral dam bars transversely connecting finger leads, the improvement of providing a lead frame in which each dam bar has a cut made before the molding operation between each end and a contiguous finger lead extending from an inner facing edge of the dam bar toward but not reaching the opposite dam bar edge, positioning the lead frame in a mold having a package body molding cavity periphery adjacent the dam bar inner facing edge to minimize flash between finger leads during molding, clamping the dam bars between opposed faces on the mold, molding a package body within the cavity without producing a significant web between finger leads, and cutting the balance of each dam bar from each finger lead without encountering excessive cutting die wear due to contact with abrasive body molding material.
Claim 3
Independent Claim
245 words
A method of making a semiconductor device package that includes molding a plastic body member around a semiconductor die and its connected inner free ends of a convergent finger lead pattern on a sheet-like lead frame, the lead frame having integral dam bars transversely connecting finger leads, the improvement of providing a lead frame in which each dam bar is partially severed before the molding operation from each of its contiguous finger leads starting from a mold cavity-facing edge on the dam bar for a distance at least about one-third the dam bar inner and opposite edge spacing, the dam bar inner edge is not more than about one-half the aforementioned dam bar edge spacing and is located to be substantially congruent with a mold cavity for molding the plastic body member, positioning the lead frame in a mold with the dam bar inner edges located substantially at the periphery of a body cavity, clamping lead frame dam bars between opposed faces of the mold, injecting a plastic molding composition into the body cavity effective to mold the body member without concurrently producing any significant plastic fin between the finger leads, and cutting the dam bars completely away from the finger leads without depositing fin molding composition into the cutting die assembly and causing excessive cutting die wear, effective to produce an as-molded body on the package that can be used without any special surface finishing selective to body surface areas between the finger leads.
Claim 4
Independent Claim
245 words
A method of making a semiconductor device package that includes molding a plastic body member around a semiconductor die and its connected inner free ends of a convergent finger lead pattern on a sheet-like lead frame, the lead frame having integral dam bars transversely connecting finger leads, the improvement of providing a lead frame in which each dam bar is partially severed before the molding operation from each of its contiguous finger leads starting from a mold cavity-facing edge on the dam bar for a distance at least about one-third the dam bar inner and opposite edge spacing, the dam bar inner edge is not more than about one-half the aforementioned dam bar edge spacing and is located to be substantially congruent with a mold cavity for molding the plastic body member, positioning the lead frame in a mold with the dam bar inner edges located substantially at the periphery of a body cavity, clamping lead frame dam bars between opposed faces of the mold, injecting a plastic molding composition into the body cavity effective to mold the body member without concurrently producing any significant plastic fin between the finger leads, and cutting the dam bars completely away from the finger leads without depositing fin molding composition into the cutting die assembly and causing excessive cutting die wear, effective to produce an as-molded body on the package that can be used without any special surface finishing selective to body surface areas between the finger leads.
References Cited (Backward Citations)
US3574815A
Cited
US3611061A
Cited
US4109096A
Cited
US4234666A
Cited
US4301464A
Cited
US4214364A
Cited
US4374080A
Cited
US4449690A
Cited
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1988-01-01 | 1988-07-02 | 1989-01-01 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 1992-01-01 | 1992-07-02 | 1993-01-01 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 1996-01-01 | 1996-07-02 | 1997-01-01 | $7700.00 | Window Closed / Lapsed |