Abstract
Abstract A method of manufacturing gradient index optical element comprises preparing a sol using silicon alkoxide and a metal alkoxide as a dopant source of index-modifying cations. The sol is treated to obtain a wet gel. Metal alkoxide from the wet gel is eluted by immersing the wet gel in a solvent to produce a concentration gradiation of the metal alkoxide in the wet gel, and the wet gel is then washed. The steps of eluting and washing are repeated so that a gradient index optical element is produced having a large difference in refractive index between the outer periphery portion and the center of the gel.
Inventors
- 👤 Minoru Inami
- 👤 Satoshi Noda
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-10-30 04:43
CPC Classifications
C; C03; C03C; C03C1/00; C03C1/006
Claims Analysis
Total Claims: 10
Claim 1
Independent Claim
107 words
A method of manufacturing a gradient index optical element utilizing a sol-gel process, comprising the steps of: (a) preparing a sol by adding a metal alkoxide as a source of refractive index-modifying dopant to silicon alkoxide; (b) subjecting said sol to a gelling treatment to obtain a wet gel; (c) immersing said wet gel in a solvent to elute some of said dopant from said gel to produce a concentration gradient of said dopant in said gel, and thereafter washing said gel; (d) repeating the above sep (c) at least once; and (e) drying said wet gel to obtain a dry gel and sintering said dry gel.
Claim 2
Independent Claim
107 words
A method of manufacturing a gradient index optical element utilizing a sol-gel process, comprising the steps of: (a) preparing a sol by adding a metal alkoxide as a source of refractive index-modifying dopant to silicon alkoxide; (b) subjecting said sol to a gelling treatment to obtain a wet gel; (c) immersing said wet gel in a solvent to elute some of said dopant from said gel to produce a concentration gradient of said dopant in said gel, and thereafter washing said gel; (d) repeating the above sep (c) at least once; and (e) drying said wet gel to obtain a dry gel and sintering said dry gel.
Claim 3
Dependent Claim
46 words
A method of manufacturing a gradient index optical element according to claim 1; wherein the duration of the immersing of the wet gel carried out in step (c) is greater than the duration in each repeated immersing of the wet gel carried out in step (d).
Claim 4
Dependent Claim
40 words
A method of manufacturing a gradient index optical element according to claim 1; wherein the immersing of the wet gel in step (c) is carried out for a duration sufficient to allow the solvent to reach the center of the
Claim 5
Dependent Claim
42 words
A method of manufacturing a gradient index optical element according to claim 1; wherein each repeated immersing of the wet gel in step (d) is carried out for a duration insufficient to allow the solvent to reach the center of the gel.
Claim 6
Dependent Claim
20 words
A method of manufacturing a gradient index optical element according to claim 1; wherein the silicon alkoxide is silicon tetramethoxide.
Claim 7
Dependent Claim
20 words
A method of manufacturing a gradient index optical element according to claim 5; wherein the metal alkoxide is titanium tetra-n-buthoxide.
Claim 8
Dependent Claim
20 words
A method of manufacturing a gradient index optical element according to claim 1; wherein the metal alkoxide is titanium tetra-n-buthoxide.
Claim 9
Dependent Claim
20 words
A method of manufacturing a gradient index optical element according to claim 1; wherein the repeating step is performed twice.
Claim 10
Dependent Claim
21 words
A method of manufacturing a gradient index optical element according to claim 1; wherein the repeating step is performed three times.
References Cited (Backward Citations)
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1996-08-23 | 1997-02-22 | 1997-08-24 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 2000-08-23 | 2001-02-22 | 2001-08-24 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 2004-08-23 | 2005-02-22 | 2005-08-24 | $7700.00 | Window Closed / Lapsed |