Method for the prevention of fouling and/or corrosion of structures in seawater, brackish water and/or fresh water

Assignee: MARINE ENVIRONMENTAL RESEARCH Inc 105 N 10TH ST MOREHEAD CITY NC 28557
•
Filing: 1991-02-21
•
Granted: 1994-09-13
•
Expires: 2011-02-21
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract A device and method for preventing fouling and/or corrosion of the exposed surfaces of a structure which is in contact with seawater, brackish water, fresh water, or a combination of these. The system includes using a structure having an exposed zinc-containing surface. At the exposed surface water interface a negative capacitive charge or an asymmetric alternating electrostatic is induced and maintained.

Inventors

  • 👤 William J. Riffe
  • 👤 Jack D. Carter

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-28 11:57
CPC Classifications
B; B63; B63B; B63B59/00; B63B59/04; B08; B08B; B08B17/00; B08B17/02; C; C23; C23F; C23F13/00; C23F15/00

Claims Analysis

Total Claims: 16
Claim 1
Independent Claim 268 words
A method for preventing the fouling or corrosion of a structure having a surface in contact with seawater, brackish water, fresh water, or a combination of these, said method comprising using a structure having a conductive zinc-containing surface, where said structure is made of zinc or of a zinc-containing alloy or said structure is made of a conductive or non-conductive material and is equipped with a zinc-containing surface layer or with a zinc-containing coating applied thereto, wherein said conductive zinc-containing surface layer and coating form an interfacial layer between said conductive structure and said water, said coating further containing a silicate, iron oxide, di-iron phosphide, or a mixture thereof, said method further comprising: (a) inducing and maintaining a negative capacitive charge on the surface of said structure in contact with said water sufficient to prevent said fouling or said corrosion; or (b) inducing and maintaining an asymmetric alternating electrostatic potential on said conductive zinc-containing coating sufficient to prevent said fouling or said corrosion; using as a means for inducing said negative capacitive charge or for inducing said asymmetric alternating electrostatic potential, a means comprising at least one condenser bank attached to said structure, wherein said at least one condenser bank is protected from contact by said water, wherein said means for inducing said negative capacitive charge or for inducing said asymmetric alternating electrostatic potential has a terminal of a first polarity conductively connected to said zinc-containing surface and a terminal of opposite polarity capacitively connected to said zinc-containing surface, wherein said terminal polarity capacitively connected to said zinc containing surface is protected from contact by said water environment.
Claim 2
Independent Claim 268 words
A method for preventing the fouling or corrosion of a structure having a surface in contact with seawater, brackish water, fresh water, or a combination of these, said method comprising using a structure having a conductive zinc-containing surface, where said structure is made of zinc or of a zinc-containing alloy or said structure is made of a conductive or non-conductive material and is equipped with a zinc-containing surface layer or with a zinc-containing coating applied thereto, wherein said conductive zinc-containing surface layer and coating form an interfacial layer between said conductive structure and said water, said coating further containing a silicate, iron oxide, di-iron phosphide, or a mixture thereof, said method further comprising: (a) inducing and maintaining a negative capacitive charge on the surface of said structure in contact with said water sufficient to prevent said fouling or said corrosion; or (b) inducing and maintaining an asymmetric alternating electrostatic potential on said conductive zinc-containing coating sufficient to prevent said fouling or said corrosion; using as a means for inducing said negative capacitive charge or for inducing said asymmetric alternating electrostatic potential, a means comprising at least one condenser bank attached to said structure, wherein said at least one condenser bank is protected from contact by said water, wherein said means for inducing said negative capacitive charge or for inducing said asymmetric alternating electrostatic potential has a terminal of a first polarity conductively connected to said zinc-containing surface and a terminal of opposite polarity capacitively connected to said zinc-containing surface, wherein said terminal polarity capacitively connected to said zinc containing surface is protected from contact by said water environment.
Claim 3
Dependent Claim 15 words
The method of claim 1, for preventing the fouling of said structure by zebra mussels.
Claim 4
Dependent Claim 13 words
The method of claim 1, comprising inducing and maintaining said negative capacitive charge.
Claim 5
Dependent Claim 12 words
The method of claim 1, comprising inducing said asymmetric alternating electrostatic potential.
Claim 6
Independent Claim 197 words
A method for preventing fouling or corrosion of an exterior surface or surfaces of a structure in contact with a water environment, said method comprising using a structure having an interior surface and a conductive zinc-containing exterior surface, wherein said structure is made of zinc or of a zinc-containing alloy, or said structure is made of a conductive or non-conductive material and is equipped with a zinc-containing surface layer or with a zinc-containing coating forming an interfacial layer between said exterior surface and said water, said coating further containing a silicate, iron oxide, di-iron phosphide, or a mixture of these, said method further comprising inducing and maintaining a negative capacitive charge on at least that part of said exterior surface in contact with said water, said negative capacitive charge being sufficient to prevent said fouling or said corrosion, wherein said negative capacitive charge is induced and maintained by a means comprising a power supply having a terminal of a first polarity conductively connected to said exterior surface and a terminal of opposite polarity capacitively connected to said exterior surface, wherein said power supply and said capacitive connection means are both protected from contact by said water environment.
Claim 7
Independent Claim 197 words
A method for preventing fouling or corrosion of an exterior surface or surfaces of a structure in contact with a water environment, said method comprising using a structure having an interior surface and a conductive zinc-containing exterior surface, wherein said structure is made of zinc or of a zinc-containing alloy, or said structure is made of a conductive or non-conductive material and is equipped with a zinc-containing surface layer or with a zinc-containing coating forming an interfacial layer between said exterior surface and said water, said coating further containing a silicate, iron oxide, di-iron phosphide, or a mixture of these, said method further comprising inducing and maintaining a negative capacitive charge on at least that part of said exterior surface in contact with said water, said negative capacitive charge being sufficient to prevent said fouling or said corrosion, wherein said negative capacitive charge is induced and maintained by a means comprising a power supply having a terminal of a first polarity conductively connected to said exterior surface and a terminal of opposite polarity capacitively connected to said exterior surface, wherein said power supply and said capacitive connection means are both protected from contact by said water environment.
Claim 8
Dependent Claim 15 words
The method of claim 5, for preventing the fouling of said structure by zebra mussels.
Claim 9
Dependent Claim 17 words
The method of claim 5, wherein said structure is a ship, a pipe, sheet or a bar.
Claim 10
Dependent Claim 16 words
The method of claim 7 wherein said sheet is a perforated sheet or an expanded sheet.
Claim 11
Dependent Claim 12 words
The method of claim 8, wherein said expanded sheet is a screen.
Claim 12
Dependent Claim 12 words
The method of claim 9, wherein said screen is an expanded mesh.
Claim 13
Dependent Claim 11 words
The method of claim 7, wherein said bar is a wire.
Claim 14
Independent Claim 196 words
A method for preventing fouling or corrosion of an exterior surface or surfaces of a structure in contact with a water environment, comprising using a structure having an interior surface and a conductive zinc-containing exterior surface, wherein said structure is made of zinc or of a zinc-containing alloy or said structure is made of a conductive or a non-conductive material and is equipped with a zinc-containing surface layer or with a zinc-containing coating forming an interfacial layer between said exterior surface and said water, said coating further containing a silicate, iron oxide, di-iron phosphide, or a mixture of these, said method further comprising inducing and maintaining a negative capacitive charge on at least the part of said exterior surface in contact with said water, said negative capacitive charge being sufficient to prevent said fouling or said corrosion, wherein said negative capacitive charge is induced and maintained by a means comprising a power supply having a terminal of a first polarity conductively connected to said exterior surface and a terminal of opposite polarity capacitively connected to said exterior surface, wherein said power supply and said capacitive connection means are both situated in the interior of said structure.
Claim 15
Independent Claim 196 words
A method for preventing fouling or corrosion of an exterior surface or surfaces of a structure in contact with a water environment, comprising using a structure having an interior surface and a conductive zinc-containing exterior surface, wherein said structure is made of zinc or of a zinc-containing alloy or said structure is made of a conductive or a non-conductive material and is equipped with a zinc-containing surface layer or with a zinc-containing coating forming an interfacial layer between said exterior surface and said water, said coating further containing a silicate, iron oxide, di-iron phosphide, or a mixture of these, said method further comprising inducing and maintaining a negative capacitive charge on at least the part of said exterior surface in contact with said water, said negative capacitive charge being sufficient to prevent said fouling or said corrosion, wherein said negative capacitive charge is induced and maintained by a means comprising a power supply having a terminal of a first polarity conductively connected to said exterior surface and a terminal of opposite polarity capacitively connected to said exterior surface, wherein said power supply and said capacitive connection means are both situated in the interior of said structure.
Claim 16
Dependent Claim 15 words
The method of claim 12, for preventing the fouling of said structure by zebra mussels.

References Cited (Backward Citations)

US872759A Cited
US3497434A Cited
US3620943A Cited
US3661742A Cited
US4196064A Cited
US4502936A Cited
US4767512A Cited
US4772344A Cited
US5009757A Cited
US5055165A Cited
US5088432A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1997-09-12 1998-03-14 1998-09-13 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 2001-09-12 2002-03-14 2002-09-13 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 2005-09-12 2006-03-14 2006-09-13 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag