Abstract

Abstract A high efficiency vertical cavity surface emitting laser with first and second mirror stacks and an active area sandwiched therebetween. The second mirror stack is formed into a mesa with exposed end surface and outer sidewalls and a centrally located light emission region. A portion of the mesa adjacent the exposed outer sidewalls has a reduced electrical conductance so as to spread operating current from the outer sidewalls into the centrally located light emission region. The electrical conductance of the portion is reduced by oxidizing or etching the outer sidewalls.

Inventors

  • 👤 Michael S. Lebby
  • 👤 Chan-Long Shieh
  • 👤 Hsing-Chung Lee

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-26 06:30
CPC Classifications
H; H01; H01S; H01S5/00; H01S5/10; H01S5/18; H01S5/183; H01S5/18308; H01S5/18311; H01S5/18313; H01S5/18316; H01S5/30; H01S5/32; H01S5/3211; H01S5/3215; Y; Y10; Y10S; Y10S438/00; Y10S438/911

Claims Analysis

Total Claims: 16
Claim 1
Independent Claim 111 words
A method of fabricating a high efficiency vertical cavity surface emitting laser comprising the steps of: forming first and second mirror stacks with an active area sandwiched therebetween; forming the second mirror stack into a mesa with exposed end surface and outer sidewalls and a centrally located light emission region; reducing the electrical conductance of a portion of the second mirror stack adjacent the exposed outer sidewalls to channel operating current from the outer sidewalls into the centrally located light emission region; and forming an electrical contact at least on the end surface of the mesa in overlying relationship to the portion of the second mirror stack with reduced electrical conductance.
Claim 2
Independent Claim 111 words
A method of fabricating a high efficiency vertical cavity surface emitting laser comprising the steps of: forming first and second mirror stacks with an active area sandwiched therebetween; forming the second mirror stack into a mesa with exposed end surface and outer sidewalls and a centrally located light emission region; reducing the electrical conductance of a portion of the second mirror stack adjacent the exposed outer sidewalls to channel operating current from the outer sidewalls into the centrally located light emission region; and forming an electrical contact at least on the end surface of the mesa in overlying relationship to the portion of the second mirror stack with reduced electrical conductance.
Claim 3
Dependent Claim 46 words
A method of fabricating a high efficiency vertical cavity surface emitting laser as claimed in claim 1 wherein the step of reducing the electrical conductance of a portion of the second mirror stack includes oxidizing selected layers of the second mirror stack adjacent the outer sidewalls.
Claim 4
Dependent Claim 64 words
A method of fabricating a high efficiency vertical cavity surface emitting laser as claimed in claim 2 wherein the step of forming the second mirror stack includes depositing alternate layers of high and low aluminum content AlGaAs in at least a portion of the second mirror stack and the step of oxidizing selected layers includes oxidizing at least the high aluminum content AlGaAs layers.
Claim 5
Dependent Claim 48 words
A method of fabricating a high efficiency vertical cavity surface emitting laser as claimed in claim 3 wherein the step of oxidizing the high aluminum content AlGaAs layers includes flowing nitrogen gas with added water moisture over the outer sidewalls at a temperature of approximately 400 degrees centigrade.
Claim 6
Dependent Claim 46 words
A method of fabricating a high efficiency vertical cavity surface emitting laser as claimed in claim 1 wherein the step of reducing the electrical conductance of a portion of the second mirror stack includes etching selected layers of the second mirror stack adjacent the outer sidewalls.
Claim 7
Dependent Claim 64 words
A method of fabricating a high efficiency vertical cavity surface emitting laser as claimed in claim 5 wherein the step of forming the second mirror stack includes depositing alternate layers of high and low aluminum content AlGaAs in at least a portion of the second mirror stack and the step of etching selected layers includes etching at least the high aluminum content AlGaAs layers.
Claim 8
Dependent Claim 37 words
A method of fabricating a high efficiency vertical cavity surface emitting laser as claimed in claim 6 wherein the step of etching the high aluminum content AlGaAs layers includes wet etching with dilute HF with DI water.
Claim 9
Dependent Claim 55 words
A method of fabricating a high efficiency vertical cavity surface emitting laser as claimed in claim 1 including in addition the step of increasing the conductance of a portion of the second mirror stack adjacent the end surface and between the portion of the second mirror stack with reduced electrical conductance and the electrical contact.
Claim 10
Dependent Claim 38 words
A method of fabricating a high efficiency vertical cavity surface emitting laser as claimed in claim 8 wherein the step of increasing the conductance of a portion of the second mirror stack includes relatively highly doping the portion.
Claim 11
Dependent Claim 105 words
A high efficiency vertical cavity surface emitting laser comprising: first and second mirror stacks with an active area sandwiched therebetween; the second mirror stack being formed into a mesa with exposed end surface and outer sidewalls and a centrally located light emission region; a portion of the second mirror stack adjacent the exposed outer sidewalls having a reduced electrical conductance so as to channel operating current from the outer sidewalls into the centrally located light emission region; and an electrical contact at least on the end surface of the mesa in overlying relationship to the portion of the second mirror stack with reduced electrical conductance.
Claim 12
Dependent Claim 105 words
A high efficiency vertical cavity surface emitting laser comprising: first and second mirror stacks with an active area sandwiched therebetween; the second mirror stack being formed into a mesa with exposed end surface and outer sidewalls and a centrally located light emission region; a portion of the second mirror stack adjacent the exposed outer sidewalls having a reduced electrical conductance so as to channel operating current from the outer sidewalls into the centrally located light emission region; and an electrical contact at least on the end surface of the mesa in overlying relationship to the portion of the second mirror stack with reduced electrical conductance.
Claim 13
Dependent Claim 47 words
A high efficiency vertical cavity surface emitting laser as claimed in claim 10 wherein the second mirror stack includes alternating layers of high and low aluminum content AlGaAs and the portion with reduced electrical conductance includes portions of the high aluminum content AlGaAs layers which are oxidized.
Claim 14
Dependent Claim 45 words
A high efficiency vertical cavity surface emitting laser as claimed in claim 10 wherein the second mirror stack includes alternating layers of high and low aluminum content AlGaAs and the portion with reduced electrical conductance includes removed portions of the high aluminum content AlGaAs layers.
Claim 15
Dependent Claim 49 words
A high efficiency vertical cavity surface emitting laser as claimed in claim 10 including in addition a portion of the second mirror stack, adjacent the end surface and between the portion of the second mirror stack with reduced electrical conductance and the electrical contact, having a relatively increased conductance.
Claim 16
Dependent Claim 70 words
A high efficiency vertical cavity surface emitting laser as claimed in claim 13 wherein the portion of the second mirror stack having a relatively increased conductance includes a first layer of AlGaAs, adjacent the end surface, at least 100 Å thick with at least a 10 19 doping and a second layer of AlGaAs, adjacent the first layer, at least 2000 Å thick and with at least 10 19 doping.

References Cited (Backward Citations)

US4943970A Cited
US4873696A Cited
US5245622A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1997-10-24 1998-04-25 1998-10-25 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 2001-10-24 2002-04-25 2002-10-25 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 2005-10-24 2006-04-25 2006-10-25 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag