← Back to Patent Explorer
US5912069A Expired / Lapsed US ⏱️ 0.0 years remaining

Metal nanolaminate composite

Assignee: NextTrip Inc
•
Filing: 1996-12-19
•
Granted: 1999-06-15
•
Expires: 2016-12-19
📄 Original PDF 🌐 Google Patents

Abstract

Abstract Metal-polymer nanolaminate products are fabricated from a bulk nanolaminate material composed of thousands of alternating metal and polymer layers. The nanolaminate material is produced by a prior art ultra high speed vacuum nanotechnology process that forms metal layers separated by radiation cross linked multifunctional acrylate polymer materials. The polymer to metal ratio in the nanolaminate composite can be successfully controlled. The polymer chemistry in the nanolaminate can be varied to incorporate a broad range of functional groups. The nanolaminate products are safe to handle and are environmentally and chemically stable at least up to 250° C. A change in polymer chemistry can be used to lower or enhance the thermal degradation point of the polymer material.

Inventors

  • 👤 Angelo Yializis
  • 👤 Richard E. Ellwanger

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-07 20:25
CPC Classifications
B; B32; B32B; B32B15/00; B32B15/04; B32B15/08; Y; Y10; Y10T; Y10T428/00; Y10T428/24; Y10T428/24942; Y10T428/2495; Y10T428/29; Y10T428/2982; Y10T428/31504; Y10T428/31678

Claims Analysis

Total Claims: 14
Claim 1
Independent Claim 86 words
A metal-polymer laminate wherein at least 50% of the weight comprises at least one metal component, said metal-polymer laminate having at least 1,000 alternating metal and polymer layers and produced in a vacuum environment by successive, sequential deposition of the metal and polymer layers, wherein each metal layer has a thickness of at least 20 nm, wherein each polymer layer has a thickness of at least 20 nm, and wherein the ratio of the metal layer thickness to the polymer layer thickness is at least 0.9.
Claim 2
Dependent Claim 86 words
A metal-polymer laminate wherein at least 50% of the weight comprises at least one metal component, said metal-polymer laminate having at least 1,000 alternating metal and polymer layers and produced in a vacuum environment by successive, sequential deposition of the metal and polymer layers, wherein each metal layer has a thickness of at least 20 nm, wherein each polymer layer has a thickness of at least 20 nm, and wherein the ratio of the metal layer thickness to the polymer layer thickness is at least 0.9.
Claim 3
Dependent Claim 16 words
The metal-polymer laminate of claim 1 wherein the bulk multilayer material is reduced to a powder.
Claim 4
Dependent Claim 43 words
The metal-polymer laminate of claim 1 wherein said at least one metal component is selected from the following group of metallic elements, all of which release heat upon combustion to the oxide: Al, B, Si, Ti, Li, Na, K, Fe, Mg, and Hf.
Claim 5
Dependent Claim 25 words
The metal-polymer laminate of claim 1 wherein the polymer includes at least one functional group, which is chosen to enhance combustion of the metal component.
Claim 6
Dependent Claim 31 words
The metal-polymer laminate of claim 4 wherein the polymer contains at least one of the following elements, all of which can enhance combustion of the metal component: O, F, Cl, N.
Claim 7
Dependent Claim 17 words
The metal-polymer laminate of claim 1 wherein the polymer is chosen to form bonds to propellant binders.
Claim 8
Dependent Claim 102 words
A metal-polymer-liquid laminate wherein at least 50% of the weight is comprised of one or more metal components, having at least 1000 alternating metal and polymer layers, having at least one liquid layer, and which is produced in a vacuum environment by successive, sequential deposition of the metal and polymer layers, wherein each metal layer has a thickness of least 20 nm, wherein each polymer layer has a thickness of at least 20 nm, each liquid layer has a thickness of less than 20 nm, and the ratio of the metal layer thickness to the polymer layer thickness is at least 0.9.
Claim 9
Dependent Claim 102 words
A metal-polymer-liquid laminate wherein at least 50% of the weight is comprised of one or more metal components, having at least 1000 alternating metal and polymer layers, having at least one liquid layer, and which is produced in a vacuum environment by successive, sequential deposition of the metal and polymer layers, wherein each metal layer has a thickness of least 20 nm, wherein each polymer layer has a thickness of at least 20 nm, each liquid layer has a thickness of less than 20 nm, and the ratio of the metal layer thickness to the polymer layer thickness is at least 0.9.
Claim 10
Dependent Claim 16 words
The metal-polymer laminate of claim 7 wherein the bulk multilayer material is reduced to a powder.
Claim 11
Dependent Claim 43 words
The metal-polymer laminate of claim 7 wherein said at least one metal component is selected from the following group of metallic elements, all of which release heat upon combustion to the oxide: Al, B, Si, Ti, Li, Na, K, Fe, Mg, and Hf.
Claim 12
Dependent Claim 35 words
The metal-polymer laminate of claim 7 wherein the polymer has at least one functional group and wherein either the polymer or the liquid layer or both are chosen to enhance combustion of the metal component.
Claim 13
Dependent Claim 31 words
The metal-polymer laminate of claim 10 wherein the polymer contains at least one of the following elements, all of which can enhance combustion of the metal component: O, F, Cl, N.
Claim 14
Dependent Claim 13 words
The metal-polymer laminate of claim 6 wherein said propellant binders comprise hydroxy-terminated polybutadiene.

References Cited (Backward Citations)

US4112849A Cited
US4842893A Cited
US5032461A Cited
US4954371A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 2002-06-14 2002-12-14 2003-06-15 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 2006-06-14 2006-12-14 2007-06-15 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 2010-06-14 2010-12-14 2011-06-15 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag