Abstract

Abstract A process for fabricating volatile and nonvolatile field effect devices on a common semiconductor wafer, and a unique composite structure for a nonvolatile memory device fabricated according to the process. A distinct feature of the process is the elimination of nitride from beneath any poly I layers while selectively retaining sandwiched and coextensive segments of nitride and poly II layers for the memory devices. In one form, the method commences with a wafer treated according to the general localized oxidation of silicon process, followed by a blanket enhancement implant and selectively masked depletion implants. The succeeding contact etch step is followed by a deposition of a poly I layer, a resistor forming implant and a patterned etch of the poly I layer. Thereafter, a first isolation oxide is grown, selective implants are performed to center the memory window, the memory area is etched, and the memory area is covered by a regrowth of a very thin memory oxide. The wafer is then coated with nitride and poly II, before undergoing a patterned plasma etch which successively and coextensively removes poly II and nitride in unwanted areas. Consequently, any nitride which remains is in a sandwiched arrangement with an overlying layer of poly II. The process inherently retains no nitride under any poly I layer, and thereby enhances the reliability of the complete IC. The composite nonvolatile memory device includes a poly II nonvolatile memory capacitor, a poly II depletion IGFET, and a poly I depletion IGFET over a single continuum of channel. The structural arrangement provides for selective access to the nonvolatile memory capacitor through the poly I IGFET during the write mode.

Inventors

  • 👤 Vinod K. Dham
  • 👤 Edward H. Honnigford
  • 👤 John K. Stewart, Jr.
  • 👤 Robert F. Pfeifer
  • 👤 Murray L. Trudel

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-30 22:26
CPC Classifications
H; H10; H10B; H10B20/00; H10B20/27; H10B20/30; H10B20/38; H10B20/383; H10D; H10D84/00; H10D84/80; H10D84/82; H10D84/83; H10D64/00; H10D64/20; H10D64/27; H10D64/311; H10D64/411; H10D64/511; H10D64/514; H10D64/516

Claims Analysis

Total Claims: 10
Claim 1
Independent Claim 84 words
A process for fabricating volatile and nonvolatile field effect devices on a common semiconductor substrate, comprising the steps of: separating a silicon substrate into distinct active regions; doping selected areas in said active regions to adjust the respective threshold voltages; forming a patterned first layer of semiconductor material on the substrate; forming a first isolation dielectric layer; patterning said first isolation dielectric layer to position a memory element; forming a memory dielectric at the position of the memory element; forming a second dielectric layer;
Claim 2
Dependent Claim 84 words
A process for fabricating volatile and nonvolatile field effect devices on a common semiconductor substrate, comprising the steps of: separating a silicon substrate into distinct active regions; doping selected areas in said active regions to adjust the respective threshold voltages; forming a patterned first layer of semiconductor material on the substrate; forming a first isolation dielectric layer; patterning said first isolation dielectric layer to position a memory element; forming a memory dielectric at the position of the memory element; forming a second dielectric layer;
Claim 3
Dependent Claim 38 words
forming a second layer of semiconductor material; patterning said second layer of semiconductor material and said second dielectric layer; removing selected areas of said first isolation dielectric; and doping selected areas of said substrate and semiconductor material layers.
Claim 4
Dependent Claim 38 words
forming a second layer of semiconductor material; patterning said second layer of semiconductor material and said second dielectric layer; removing selected areas of said first isolation dielectric; and doping selected areas of said substrate and semiconductor material layers.
Claim 5
Dependent Claim 14 words
The process recited in claim 1, wherein said second dielectric layer contains silicon nitride.
Claim 6
Dependent Claim 79 words
The process recited in claim 2, wherein: said step of forming a patterned first layer of dopable material includes the doping of said first layer of dopable material sufficiently to form a resistive element; said pattern in said first layer of dopable material includes a segment suitable to form a resistive element; and said step of patterning said second layer of dopable material and said second dielectric layer retains coextensive layers over the memory element and the resistive element.
Claim 7
Dependent Claim 60 words
The process recited in claim 3, wherein: said step of doping selected areas in said active regions is comprised of a blanket enhancement implant followed by selected depletion implants; and the step of doping said substrate at the position of the memory element to center a memory window, is included after said step of forming a first isolation dielectric layer.
Claim 8
Dependent Claim 59 words
The process recited in claim 4, wherein: said step of patterning said first isolation dielectric layer to position the memory element comprises a selective etch through said first isolation dielectric layer to expose the underlying substrate surface; and said step of forming a memory dielectric comprises the thermal growth of a thin memory oxide on said exposed substrate surface.
Claim 9
Dependent Claim 35 words
The process recited in claims 1, 2, 3, 4 or 5, including the further step of: exposing selected poly-to-substrate contact areas of said substrate, after said step of doping selected areas in said active regions.
Claim 10
Dependent Claim 48 words
The processes recited in claim 6, wherein said processes are extended by the steps of: forming a second isolation dielectric layer; removing selected areas of said second isolation dielectric layer to expose areas of poly and substrate; annealing in a hydrogen environment; and depositing a patterned metallization layer.

References Cited (Backward Citations)

US4270262A Cited
US4249191A Cited
US4257832A Cited
US4229755A Cited
US4335505A Cited
US4306353A Cited
US4370798A Cited
US4342149A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1988-08-12 1989-02-11 1989-08-13 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1992-08-12 1993-02-11 1993-08-13 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1996-08-12 1997-02-11 1997-08-13 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag